Recovery of vanadium from stone coal acid leaching solution by coprecipitation, alkaline roasting and water leaching

被引:53
|
作者
Ye, Puhong [1 ]
Wang, Xuewen [1 ]
Wang, Mingyu [1 ]
Fan, Yeye [1 ]
Xiang, Xiaoyan [1 ]
机构
[1] Cent S Univ, Sch Met Sci & Engn, Changsha 410083, Peoples R China
关键词
Stone coal; Acid leaching; Coprecipitation; Alkaline roasting; Water leaching; EXTRACTING VANADIUM; TECHNOLOGY;
D O I
10.1016/j.hydromet.2012.02.013
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The recovery of vanadium from stone coal acid leaching solution by coprecipitation, alkaline roasting and water leaching was studied. A method used to recover vanadium from stone coal acid leaching solution was developed, and it primarily included vanadium coprecipitation with iron in the solution, vanadium extraction by alkaline leaching from the precipitate, and vanadium pentoxide preparation with the alkaline leaching solution. Experiments found that the vanadium in stone coal acid leaching solution can be effectively enriched in the precipitate obtained by adding 3.64 g NaClO3 per liter solution with initial pH 1.73 under stirring for 0.5 h at 95 degrees C. By roasting the mixture of 25 g of the precipitate with 22.5 g NaOH at 170 degrees C for 1.0 h. and then water leaching the roasted mixture at 98 degrees C for 1.0 h under stirring with L/S ratio of 3.3:1 mL/g, 97.0% of vanadium was extracted from the precipitate. After purifying with MgCl2, the vanadium pentoxide with purity 99.3% was obtained by adding NH4Cl to precipitate ammonium vanadate from the solution at pH about 2.0, and then roasting the ammonium vanadate at 520 degrees C for 2.0 h. The essential components of the coprecipitate are KFe3(SO4)(2)(OH)(6) and HNaV6O16 center dot 4H(2)O. (C) 2012 Elsevier By. All rights reserved.
引用
收藏
页码:108 / 115
页数:8
相关论文
共 50 条
  • [21] Phase Transformation and Dissolution Behavior of Pyrite in the Roasting-Sulfuric Acid Leaching Process of Vanadium-Bearing Stone Coal
    Wang, Xingjie
    Zhang, Yimin
    Liu, Tao
    Yuan, Yizhong
    MINERALS, 2020, 10 (06) : 1 - 10
  • [22] Calcified roasting-acid leaching process of vanadium from low-grade vanadium-containing stone coal
    Wang T.
    Xu L.
    Liu C.
    Zhang Z.
    Chinese Journal of Geochemistry, 2014, 33 (2): : 163 - 167
  • [23] Leaching vanadium by high concentration sulfuric acid from stone coal
    陈向阳
    兰新哲
    张秋利
    马红周
    周军
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20(S1) (S1) : 123 - 126
  • [24] Highly selective separation of vanadium over iron from stone coal by oxalic acid leaching
    Hu, Pengcheng
    Zhang, Yimin
    Liu, Tao
    Huang, Jing
    Yuan, Yizhong
    Zheng, Qiushi
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2017, 45 : 241 - 247
  • [25] Leaching vanadium by high concentration sulfuric acid from stone coal
    Chen Xiang-yang
    Lan Xin-zhe
    Zhang Qiu-li
    Ma Hong-Zhou
    Zhou Jun
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S123 - S126
  • [26] Calcified roasting-acid leaching process of vanadium from low-grade vanadium-containing stone coal
    WANG Taiying
    XU Longjun
    LIU Chenlun
    ZHANG Zhaodi
    Acta Geochimica, 2014, 33 (02) : 163 - 167
  • [27] Study on leaching vanadium from roasted residue of stone coal
    He, D.
    Feng, Q.
    Zhang, G.
    Luo, W.
    Ou, L.
    MINERALS & METALLURGICAL PROCESSING, 2008, 25 (04) : 181 - 184
  • [28] Study on leaching vanadium from roasted residue of stone coal
    D. He
    Q. Feng
    G. Zhang
    W. Luo
    L. Ou
    Mining, Metallurgy & Exploration, 2008, 25 : 181 - 184
  • [29] Study on leaching vanadium from roasted residue of stone coal
    School of Resources Processing and Bioengineering, Central South University, Changsha, China
    Miner Metall Process, 2008, 4 (181-184): : 181 - 184
  • [30] A kinetics study of multi-stage counter-current circulation acid leaching of vanadium from stone coal
    Zhu, Xiaobo
    Zhang, Yimin
    Huang, Jing
    Liu, Tao
    Wang, Yi
    INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2012, 114 : 1 - 6