Effect of Phosphorus Content on Hydrogen Embrittlement for High Strength Steel Treated with Electroless Ni-P Plating

被引:1
作者
Hino, Makoto [1 ]
Doi, Yuho [1 ]
Kuwano, Ryoichi [1 ]
Oda, Yukinori [2 ]
Horikawa, Keitaro [3 ]
机构
[1] Hiroshima Inst Technol, Grad Sch Engn, Dept Mech Syst, Hiroshima 7315193, Japan
[2] C Uyemura & Co Ltd, Hirakata, Osaka 5730065, Japan
[3] Osaka Univ, Grad Sch Engn Sci, Dept Mech Sci & Bioengn, Toyonaka, Osaka 5608531, Japan
关键词
hydrogen embrittlement; high strength steel; three-point bending test; electroless Ni-P plating; hydrogen permeability;
D O I
10.2320/jinstmet.JB201906
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Hydrogen embrittlement of SK85 high-strength steel sheets was evaluated through a three-point bending test. The effects of electroless Ni-P plating and Ni electroplating on hydrogen embrittlement were examined with respect to the hydrogen permeability of the plated films. On the morrow of the plating, electroless Ni-P plating indicates a high degree of hydrogen embrittlement, irrespective of the phosphorus content in the film. However, hydrogen embrittlement of Ni electroplating is further suppressed than that of electroless Ni-P plating, which can be attributed to the excellent hydrogen diffusing ability of Ni electroplating. These results demonstrate that the hydrogen permeability of a plated film is an important factor for hydrogen embrittlement. Hydrogen present on the plated film surface was visualized by employing the hydrogen microprint technique, and the corresponding results reveal that the hydrogen permeability of the plated film is dependent on the film crystal structure. Furthermore, the pits in the film can become a route for hydrogen emission.
引用
收藏
页码:80 / 86
页数:7
相关论文
共 17 条
[1]  
[Anonymous], 2011, GEND MEKK, P300
[2]  
Frohmberg R.P., 1955, Trans. ASM, V47, P892
[3]   Evaluation of Hydrogen Embrittlement for High Strength Steel by Three-Point Bending Test and Application to Zinc Electroplating [J].
Hino, Makoto ;
Asashita, Hideaki ;
Yasui, Naoyuki ;
Takago, Shigeki ;
Hiramatsu, Minoru ;
Kanadani, Teruto .
JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2016, 80 (12) :731-735
[4]  
Hino Y., 2019, J. Surf. Finish. Soc. Jpn., V70, P110
[5]  
Hiramatsu M., 1988, KINZOKU HYOMEN GIJUT, V39, P404
[6]  
Hiramatsu M., 1996, Corrosion Engineering, V45, P47
[7]  
Masumoto K., 1984, AMORPHOUS ALLOY, P324
[8]  
Matsuoka M., 1990, J SURF FINISH SOC JP, V41, P706
[9]   Effect of Surface Structure and Hydrogen on the Fatigue Strength of Electroless Nickel-Phosphorus Plated Al-1.2%Si Alloy [J].
Nagata, Norihito ;
Kanadani, Teruto ;
Nakagawa, Keiyu ;
Fukuhara, Minoru ;
Horikawa, Keitaro ;
Murakami, Kouji ;
Hino, Makoto .
JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2015, 79 (03) :151-155
[10]   Hydrogen related failure of steels - a new aspect [J].