Effects of External Stress on High-Temperature Corrosion Behavior of T92 Ferrite Steel with Na2SO4-K2SO4 Molten Salts

被引:8
作者
Liu, Zhuhan [1 ]
Ning, Zhiyuan [1 ]
Zhou, Qulan [1 ]
Li, Na [1 ]
Liu, Taisheng [2 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Multiphase Flow Power Engn, Xian 710049, Peoples R China
[2] Key Lab Clean Combust & Flue Gas Purificat Sichua, Chengdu 610036, Peoples R China
来源
OXIDATION OF METALS | 2022年 / 97卷 / 1-2期
关键词
High-temperature corrosion; External stress; Decomposition of sulfates; Dissolution of oxides; SEM&XRD; HOT CORROSION; ALLOYS; OXIDATION; DEPOSITS; CHLORIDE; NI-20CR; METALS; CR;
D O I
10.1007/s11085-021-10084-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper reports an experimental study of the oxidation-sulfidation behavior of T92 steel in a complex environment consisting of a combination of high temperature (700 degrees C), SO2, molten sulfate salts, and applied stresses. The corrosion products, morphologies, and element distributions of corrosion scales were investigated in detail by SEM and XRD. Results indicate that the formation of sulfides in the deep layer where the p(O-2) is low-level prevents the reformation of a protective layer after the damage of the Cr2O3 layer. It is also noted that based on the data of maximum corrosion depth, when stresses are applied, the extent of corrosion had been alleviated, which is ascribed to that the applied stress also accelerated the fast formation of Cr2O3. However, the applied stress is also thought to accelerate the damage of the protective layer by inducing more boundaries of products and increasing the possibility of exfoliation of a corrosion scale. Thus, in the limited exposure duration to the corrosive environment in this study, there should be a "critical stress" under which the specimens present the best corrosion resistance.
引用
收藏
页码:141 / 155
页数:15
相关论文
共 50 条
  • [31] High Temperature Corrosion Behaviour of 20MnMoNi55 and AISI 304 Bare Steel in 75wt.%Na2SO4+25wt.%K2SO4 Molten Salt Environment at 900°C
    Kumar, Vijay
    Arora, Navneet
    INTERNATIONAL CONFERENCE ON ADVANCES IN MANUFACTURING AND MATERIALS ENGINEERING (ICAMME 2014), 2014, 5 : 76 - 85
  • [32] Hot Corrosion Behavior of Inconel 625 in Na2SO4 and V2O5 Molten Salt System
    Li, Liang
    Li, Lanfeng
    Zhang, Guofeng
    Xue, Hongdi
    Cui, Maomao
    Wang, Wenxu
    Liu, Dexue
    METALS, 2023, 13 (06)
  • [33] Na2SO4 Induced Hot Corrosion of Aluminized Low Carbon Steel at 700 °C
    Badaruddin, Mohammad
    ADVANCES IN APPLIED MECHANICS AND MATERIALS, 2014, 493 : 761 - 766
  • [34] Corrosion of steel alloys in molten NaCl + Na2SO4 at 700 °C for thermal energy storage
    Sarvghad, Madjid
    Will, Geoffrey
    Steinberg, Theodore A.
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2018, 179 : 207 - 216
  • [35] Corrosion behavior of HDA (hot-dip aluminized) carbon steel C45 half immersed in molten salts (NaCl, Na2SO4) isothermally at 973 K
    Muhammed, Hawkar J.
    Koncz-Horvath, Daniel
    Torok, Tamas, I
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2023, 37 (20) : 2807 - 2827
  • [36] EFFECTS OF SO3, SO2 AND O2 GASSES ON HOT CORROSION OF NI AND NI-CR ALLOYS IN MOLTEN NA2SO4
    HARA, M
    HISAICHI, T
    ITOH, K
    SHINATA, Y
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1991, 55 (11) : 1207 - 1215
  • [37] Effect of Minor Nb on Isothermal-Oxidation and Hot Corrosion Behavior of Two Nickel-Based Superalloys Under Na2SO4/Na2SO4-NaCl
    Zhou, Yuebo
    Wang, Hong
    Mo, Chenggang
    Zhang, Lina
    CORROSION, 2021, 77 (09) : 949 - 960
  • [38] High Temperature Corrosion Behavior of Cold Deformed 2.25 Cr-1 Mo Steel in SO2+O2 Atmosphere
    Ghosh, D.
    Mitra, S. K.
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2015, 34 (02) : 107 - 114
  • [39] CORROSION BEHAVIOR OF NICKEL BASE ALLOY FGH95 IN MOLTEN NaCl-Na2SO4
    Lue Jiaxin
    Zheng Lei
    Zhang Maicang
    Dong Jianxin
    ACTA METALLURGICA SINICA, 2009, 45 (02) : 204 - 210
  • [40] Hot corrosion behaviour of barium-strontium aluminosilicates in a molten Na2SO4 environment
    Jiang, Fengrui
    Cheng, Laifei
    Wang, Yiguang
    Huang, Xuanxuan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (02) : 823 - 832