Effects of External Stress on High-Temperature Corrosion Behavior of T92 Ferrite Steel with Na2SO4-K2SO4 Molten Salts

被引:8
|
作者
Liu, Zhuhan [1 ]
Ning, Zhiyuan [1 ]
Zhou, Qulan [1 ]
Li, Na [1 ]
Liu, Taisheng [2 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Multiphase Flow Power Engn, Xian 710049, Peoples R China
[2] Key Lab Clean Combust & Flue Gas Purificat Sichua, Chengdu 610036, Peoples R China
来源
OXIDATION OF METALS | 2022年 / 97卷 / 1-2期
关键词
High-temperature corrosion; External stress; Decomposition of sulfates; Dissolution of oxides; SEM&XRD; HOT CORROSION; ALLOYS; OXIDATION; DEPOSITS; CHLORIDE; NI-20CR; METALS; CR;
D O I
10.1007/s11085-021-10084-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper reports an experimental study of the oxidation-sulfidation behavior of T92 steel in a complex environment consisting of a combination of high temperature (700 degrees C), SO2, molten sulfate salts, and applied stresses. The corrosion products, morphologies, and element distributions of corrosion scales were investigated in detail by SEM and XRD. Results indicate that the formation of sulfides in the deep layer where the p(O-2) is low-level prevents the reformation of a protective layer after the damage of the Cr2O3 layer. It is also noted that based on the data of maximum corrosion depth, when stresses are applied, the extent of corrosion had been alleviated, which is ascribed to that the applied stress also accelerated the fast formation of Cr2O3. However, the applied stress is also thought to accelerate the damage of the protective layer by inducing more boundaries of products and increasing the possibility of exfoliation of a corrosion scale. Thus, in the limited exposure duration to the corrosive environment in this study, there should be a "critical stress" under which the specimens present the best corrosion resistance.
引用
收藏
页码:141 / 155
页数:15
相关论文
共 50 条
  • [11] Hot corrosion behavior of a centimeter Fe-based amorphous composite coating prepared by laser cladding in molten Na2SO4 + K2SO4 salts
    Liu, Wenyi
    Hou, Yong
    Liu, Chao
    Wang, Yongtian
    Jiang, Runsen
    Xu, Gang
    SURFACE & COATINGS TECHNOLOGY, 2015, 270 : 33 - 38
  • [12] High-temperature corrosion of aluminized-AISI 1020 steel with NaCl and Na2SO4 deposits
    Badaruddin, M.
    Sugiyanto
    Asmi, D.
    BULLETIN OF MATERIALS SCIENCE, 2019, 43 (01)
  • [13] STUDY ON THE EFFECTS OF EXTERNAL STRESS ON HOT CORROSION BEHAVIOR OF STEEL T91 IN THE OXIDIZING ATMOSPHERE CONTAINING SO2
    Liu, Zhuhan
    Li, Na
    Zhou, Qulan
    Liu, Taisheng
    PROCEEDINGS OF THE ASME POWER CONFERENCE JOINT WITH ICOPE-17, 2017, VOL 1, 2017,
  • [14] Hot Corrosion Behavior of ZrB2-SiC-Graphite Composite in NaCl and Na2SO4 Molten Salts
    Liu, X.
    Wang, G.
    Liu, L.
    Wang, Z.
    Wu, Z.
    Liu, M.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2018, 9 (03): : 309 - 317
  • [15] High-Temperature Corrosion of Ni-Cr-Mo Cladding Layers with Different Si Contents in NaCl-KCl-Na2SO4-K2SO4 Mixed Salt Medium
    Chen, Shanshan
    Liu, Zongde
    Shen, Yue
    Liu, Simin
    MATERIALS, 2022, 15 (09)
  • [16] Corrosion behavior of the NiCrAlY and NiSiAlY alloys with salt mixtures of NaCl/Na2SO4
    Zheng, Haiyang
    Cui, Tiancheng
    Zhu, Bing
    Yu, Xiaopeng
    Yu, Miao
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2024, 42 (02):
  • [17] Hot corrosion behavior and mechanism of FGH96 P/M superalloy in molten NaCl-Na2SO4 salts
    Jiang, He
    Dong, Jian-Xin
    Zhang, Mai-Cang
    Zheng, Lei
    Yao, Zhi-Hao
    RARE METALS, 2019, 38 (02) : 173 - 180
  • [18] High-Temperature Corrosion Characteristics of Ni-20Cr-xSi Alloy Laser Cladding Layer in NaCl-KCl-Na2SO4-K2SO4 Mixed Salt Environment
    Chen, Shanshan
    Liu, Zongde
    Liu, Fulai
    COATINGS, 2023, 13 (08)
  • [19] High-Temperature Na2SO4 Deposit-Assisted Corrosion of Silicon Carbide - I: Temperature and Time Dependence
    Hagan, Joseph M.
    Opila, Elizabeth J.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2015, 98 (04) : 1275 - 1284
  • [20] The Effects of KCl, K2SO4 and K2CO3 on the High Temperature Corrosion of a 304-Type Austenitic Stainless Steel
    Pettersson, Jesper
    Folkeson, Nicklas
    Johansson, Lars-Gunnar
    Svensson, Jan-Erik
    OXIDATION OF METALS, 2011, 76 (1-2): : 93 - 109