Synthesis and Immobilization of MnO2 Nanoparticles on Bio-silica for the Efficient Degradation of an Azo Dye in the Aqueous Solution

被引:0
作者
Khataee, Alireza [1 ]
Bozorg, Soghra [1 ]
Vahid, Behrouz [2 ]
Trung-Dung Dang [3 ]
Hanifehpour, Younes [4 ]
Joo, Sang Woo [4 ]
机构
[1] Univ Tabriz, Fac Chem, Dept Appl Chem, Res Lab Adv Water & Wastewater Treatment Proc, Tabriz 5166614766, Iran
[2] Islamic Azad Univ, Tabriz Branch, Coll Engn, Dept Chem Engn, Tabriz, Iran
[3] Hanoi Univ Sci & Technol, Sch Chem Engn, Hanoi, Vietnam
[4] Yeungnam Univ, Sch Mech Engn, Kyongsan 712749, South Korea
基金
新加坡国家研究基金会;
关键词
Acid Orange 7; Degradation; Manganese oxide; MnO2 coated bio-silica; Nanocatalyst; PHOTOELECTRO-FENTON PROCESS; OPERATIONAL PARAMETERS; CARBON NANOTUBES; WASTE-WATER; ADSORPTION; REMOVAL; CATHODE;
D O I
10.2174/1573413710666140917211140
中图分类号
Q81 [生物工程学(生物技术)]; Q93 [微生物学];
学科分类号
071005 ; 0836 ; 090102 ; 100705 ;
摘要
In this study, MnO2 nanoparticles were synthesized on bio-silica by a simple one-step procedure using permanganate in the acidic medium. The synthesized catalyst was characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and Fourier transform infrared spectroscopy (FT-IR). The obtained results confirmed the nanostructure of MnO2 and its stabilization on the bio-silica as the support. The removal efficiency of acid orange 7 (AO7), using bare bio-silica and MnO2 coated bio-silica, was found to be 5 and 95%, respectively. The effect of operational parameters including AO7 concentration, catalyst dosage and process time of treatment process was also studied on the basis of efficiency. The results demonstrated that the color removal efficiency was decreased by increasing AO7 concentration, and increased by the enhancement of the process time. The optimal dosage of 0.8 g/L was chosen for the catalyst amount. Hydroxyl radicals played a significant role in the process based on the proposed mechanism. The spectral changes of AO7 during the process in UV-Vis region showed not only the efficient decolorization, but also the degradation of the dye after 50 min of the treatment.
引用
收藏
页码:129 / 134
页数:6
相关论文
共 27 条
  • [11] Preparation of MnO2/WMNT composite and MnO2/AB composite by redox deposition method and its comparative study as supercapacitive materials
    Chu, Hong-Yan
    Lai, Qiong-Yu
    Wang, Ling
    Lu, Jian-Fang
    Zhao, Yan
    [J]. IONICS, 2010, 16 (03) : 233 - 238
  • [12] Photocatalytic degradation of azo dye acid red 14 in water: investigation of the effect of operational parameters
    Daneshvar, N
    Salari, D
    Khataee, AR
    [J]. JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2003, 157 (01) : 111 - 116
  • [13] Bio-silica coated with amorphous manganese oxide as an efficient catalyst for rapid degradation of organic pollutant
    Dang, T. D.
    Banerjee, A. N.
    Cheney, M. A.
    Qian, S.
    Joo, S. W.
    Min, B. K.
    [J]. COLLOIDS AND SURFACES B-BIOINTERFACES, 2013, 106 : 151 - 157
  • [14] Goyal AK, 2011, CURR NANOSCI, V7, P640
  • [15] Synthesis, Characterization and Photocatalytic Properties of Nanostructured Sm-doped CdSe
    Khataee, A. R.
    Fathinia, S.
    Fathinia, M.
    Hanifehpour, Y.
    Joo, S. W.
    Soltani, B.
    [J]. CURRENT NANOSCIENCE, 2013, 9 (06) : 780 - 786
  • [16] Treatment of a dye solution using photoelectro-fenton process on the cathode containing carbon nanotubes under recirculation mode: Investigation of operational parameters and artificial neural network modeling
    Khataee, A. R.
    Vahid, B.
    Behjati, B.
    Safarpour, M.
    [J]. ENVIRONMENTAL PROGRESS & SUSTAINABLE ENERGY, 2013, 32 (03) : 557 - 563
  • [17] Simultaneous monitoring of photocatalysis of three pharmaceuticals by immobilized TiO2 nanoparticles: Chemometric assessment, intermediates identification and ecotoxicological evaluation
    Khataee, A. R.
    Fathinia, M.
    Joo, S. W.
    [J]. SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY, 2013, 112 : 33 - 45
  • [18] Decolorization of CI Acid Blue 9 solution by UV/Nano-TiO2, Fenton, Fenton-like, electro-Fenton and electrocoagulation processes: A comparative study
    Khataee, A. R.
    Vatanpour, V.
    Ghadim, A. R. Amani
    [J]. JOURNAL OF HAZARDOUS MATERIALS, 2009, 161 (2-3) : 1225 - 1233
  • [19] Treatment of an Azo Dye by Citrate Catalyzed Photoelectro-Fenton Process Under Visible Light using Carbon Nanotube-polytetrafluoroethylene Cathode
    Khataee, Alireza
    Marandizadeh, Hadi
    Zarei, Mahmoud
    Aber, Soheil
    Vahid, Behrouz
    Hanifehpour, Younes
    Joo, Sang W.
    [J]. CURRENT NANOSCIENCE, 2013, 9 (03) : 387 - 393
  • [20] Effect of OH and silanol groups in the removal of dyes from aqueous solution using diatomite
    Khraisheh, MAM
    Al-Ghouti, MA
    Allen, SJ
    Ahmad, MN
    [J]. WATER RESEARCH, 2005, 39 (05) : 922 - 932