Acoustic emission analysis of Vickers indentation fracture of cermet and ceramic coatings

被引:7
作者
Faisal, N. H. [1 ,2 ]
Ahmed, R. [1 ,2 ]
机构
[1] Heriot Watt Univ, Dept Mech Engn, Sch Engn & Phys Sci, Edinburgh EH14 4AS, Midlothian, Scotland
[2] Alfaisal Univ, Coll Engn, Riyadh 11533, Saudi Arabia
关键词
instrumentation; acoustic emission; Vickers indentation; open loop; thermal spray coatings; fracture toughness; RESIDUAL STRAIN-MEASUREMENTS; ALUMINA-ZIRCONIA COMPOSITES; BRITTLE MATERIALS; NEUTRON-DIFFRACTION; TOUGHNESS TEST; CRACKS;
D O I
10.1088/0957-0233/22/12/125704
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this work was to develop an instrumented experimental methodology of quantitative material evaluation based on the acoustic emission (AE) monitoring of a dead-weight Vickers indentation. This was to assess the degree of cracking and hence the toughness of thermally sprayed coatings. AE data were acquired during indentation tests on samples of coatings of nominal thickness 250-325 mu m at a variety of indentation loads ranging from 49 to 490 N. Measurements were carried out on five different carbide and ceramic coatings (HVOF as-sprayed WC-12% Co (JP5000 and JetKote), HIPed WC-12% Co (JetKote) and as-sprayed Al2O3 (APS/Metco and HVOF/theta-gun)). The raw AE signals recorded during indentation were analysed and the total surface crack length around the indent determined. The results showed that the total surface crack length measured gave fracture toughness (K-1c) values which were consistent with the published literature for similar coatings but evaluated using the classical approach (Palmqvist/half-penny model). Hence, the total surface crack length criteria can be applied to ceramic and cermet coatings which may or may not exhibit fracture via radial cracks. The values of K-1c measured were 3.4 +/- 0.1 MPa m(1/2) for high-velocity oxygen fuel (HVOF) (theta-gun) Al2O3, 4.6 +/- 0.3 MPa m(1/2) for as-sprayed HVOF (JetKote) WC-12% Co, 7.1 +/- 0.1 MPa m(1/2) for as-sprayed HVOF (JP5000) WC-12% Co and 7.4 +/- 0.2 MPa m(1/2) for HIPed HVOF (JetKote) WC-12% Co coatings. The crack lengths were then calibrated against the AE response and correlation coefficients evaluated. The values of K-1c measured using AE correlations were 3.3 MPa m(1/2) for HVOF (theta-gun) Al2O3, 2.6 MPa m(1/2) for APS (Metco) Al2O3, 2.5 MPa m(1/2) for as-sprayed HVOF (JetKote) WC-12% Co, 6.3 MPa m(1/2) for as-sprayed HVOF (JP5000) WC-12% Co and 8.6 MPa m(1/2) for HIPed HVOF (JetKote) WC-12% Co coatings. It is concluded that within each category of coating type, AE can be used as a suitable surrogate for crack length measurement for assessing coating quality. Hence, a full measure of crack prevalence which would require time-consuming fractal dimension analysis can be made redundant for a given coating type, offering a motivation for AE-based indentation testing as a measure of quality control. Similarly, for cases where surface crack length cannot be measured due to delamination/spallation of surface, AE-based fracture toughness provides a benchmark for coating quality assessment.
引用
收藏
页数:20
相关论文
共 50 条
[1]   Residual strain measurements in thermal spray cermet coatings via neutron diffraction [J].
Ahmed, R. ;
Yu, H. ;
Stewart, S. .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2007, 129 (02) :411-418
[2]   Residual Strain and Fracture Response of Al2O3 Coatings Deposited via APS and HVOF Techniques [J].
Ahmed, R. ;
Faisal, N. H. ;
Paradowska, A. M. ;
Fitzpatrick, M. E. .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2012, 21 (01) :23-40
[3]   Neutron diffraction residual strain measurements in alumina coatings deposited via APS and HVOF techniques [J].
Ahmed, R. ;
Faisal, N. H. ;
Reuben, R. L. ;
Paradowska, A. M. ;
Fitzpatrick, M. ;
Kitamura, J. ;
Osawa, S. .
INTERNATIONAL CONFERENCE ON NEUTRON SCATTERING 2009, 2010, 251
[4]   Neutron diffraction residual strain measurements in post-treated thermal spray cermet coatings [J].
Ahmed, R. ;
Yu, H. ;
Stoica, V. ;
Edwards, L. ;
Santisteban, J. R. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 498 (1-2) :191-202
[5]   The bending strength of brittle materials and the characteristics of the elastic wave signal by Vickers indentation [J].
Ahn, SH ;
Nam, KW ;
Ando, K .
ADVANCES IN FRACTURE AND FAILURE PREVENTION, PTS 1 AND 2, 2004, 261-263 :1635-1640
[6]   ACOUSTIC-EMISSION AND DEFORMATION MODE IN CERAMICS DURING INDENTATION [J].
AKBARI, J ;
SAITO, Y ;
HANAOIKA, T ;
ENOMOTO, S .
JSME INTERNATIONAL JOURNAL SERIES A-MECHANICS AND MATERIAL ENGINEERING, 1994, 37 (04) :488-494
[7]  
[Anonymous], 1920, The phenomena of Rupture and Flow in Solids
[8]  
[Anonymous], 1992, E9282 ASTM, P92
[9]  
[Anonymous], 1993, FRACTURE BRITTLE SOL, DOI DOI 10.1017/CBO9780511623127
[10]   Processing-structure-property correlation and decarburization phenomenon in detonation sprayed WC-12Co coatings [J].
Babu, P. Suresh ;
Basu, Bikramjit ;
Sundararajan, G. .
ACTA MATERIALIA, 2008, 56 (18) :5012-5026