Electrochemical performances of Mm0.7MgxNi2.58Co0.5Mn0.3Al0.12 (x=0, 0.3) hydrogen storage alloys in the temperature range from 238 to 303 K

被引:13
|
作者
Ni, Chengyuan [1 ]
Zhou, Huaiying [1 ,2 ]
Shi, Nianlei [2 ]
Wang, Zhongmin [2 ]
机构
[1] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Guilin Univ Elect Technol, Sch Mat Sci & Engn, Guilin 541004, Guangxi, Peoples R China
关键词
Hydrogen storage alloy; Low temperature property; Self-discharge; Electrochemical kinetics; METAL HYDRIDE ELECTRODE; IMPEDANCE SPECTROSCOPY; INTERMETALLIC HYDRIDES; ANNEALING TREATMENT; NI/MH BATTERIES; NI; MICROSTRUCTURE; LA; CO; SUBSTITUTION;
D O I
10.1016/j.electacta.2011.10.063
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
A series of experiments have been performed to investigate electrochemical properties of Mm(0.7)Mg(x)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) (x = 0, 0.3) alloy at various temperatures (238 K, 273 K and 303 K). The results indicate that both alloy electrodes exhibit high dischargeabilities after elemental substitution, above 320 mAh g(-1) even at 238 K. The capacity degradation of the two alloys are primarily ascribed to serious pulverization, other than the oxidation of active components at the initial stage. Moreover, the electrochemical performances of Mm(0.7)Mg(x)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) (x = 0, 0.3) alloy electrodes depend on the alloy type and testing temperature. Mm(0.7)Mg(0.3)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) alloy, consisting of LaNi5-phase and La2Ni7-phase, shows better properties of discharge capacity, cyclic stability, self-discharge and pulverization resistance at the three temperatures than those of single LaNi5-phase Mm(0.7)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) alloy. The electrochemical kinetics studies indicate that the activation energy of hydrogen diffusion and exchange current density (I-0) of Mm(0.7)Mg(0.3)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) alloy are lower than those of Mm(0.7)Ni(2.58)Co(0.5)Mn(0.3)Al(0.12) alloy. When the temperature increases from 238 to 303 K, the capacity loss, high-rate dischargeability, exchange current density I-0 and hydrogen diffusion coefficient (D/a(2)) of the two alloys increases, while capacity retention decreases. Further analysis of kinetics suggests that bulk hydrogen diffusion is the rate-determining step of the battery reaction at low temperature 238 K, and charge-transfer reaction on alloy surface is the rate-determining step when tested at 273 K and 303 K for both alloys. The perfect low temperature discharge capacities of the two alloys can mainly attribute to the decrease of activation energy for hydrogen diffusion after elemental substitution. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:237 / 244
页数:8
相关论文
共 45 条
  • [21] Microstructures and electrochemical properties of La0.7Ce0.3Ni3.7Co0.7-xAl0.2Mn0.4(Fe0.43B0.57)x (x=0-0.4) hydrogen storage alloys
    Zhou Yu
    Fan Yanping
    Peng Xianyun
    Liu Baozhong
    PROGRESS IN RENEWABLE AND SUSTAINABLE ENERGY, PTS 1 AND 2, 2013, 608-609 : 917 - +
  • [22] A study on hydrogen storage and electrochemical properties of La0.55Pr0.05Nd0.15Mg0.25Ni3.5 (Co0.5Al0.5)x (x=0.0, 0.1, 0.3, 0.5) alloys
    Qin Ming
    Lan Zhiqiang
    Ding Yang
    Xiong Kai
    Liu Yixin
    Guo Jin
    JOURNAL OF RARE EARTHS, 2012, 30 (03) : 222 - 227
  • [23] Microstructure and electrochemical characteristics of La0.7Ce0.3Ni3.75Mn0.35Al0.15Cu0.75-x(V0.81Fe0.19)x hydrogen storage alloys
    Liu Baozhong
    Hu Mengjuan
    Li Anming
    Ji Liqiang
    Zhang Baoqing
    Zhu Xilin
    JOURNAL OF RARE EARTHS, 2012, 30 (08) : 769 - 774
  • [24] Microstructures and electrochemical hydrogen storage characteristics of La0.7Ce0.3Ni4.2Mn0.9-xCu0.37(Fe0.43B0.57)x (x=0-0.20) alloys
    Peng, Xianyun
    Liu, Baozhong
    Fan, Yanping
    Zhu, Xilin
    Peng, Qiuming
    Zhang, Zhi
    JOURNAL OF POWER SOURCES, 2013, 240 : 178 - 183
  • [25] Phase structures of RENi4.3-xCoxMn0.4Al0.3 (x=0.5 ∼ 1.3)hydrogen storage alloys and their electrochemical performance at high temperature
    Li, SQ
    Chen, LX
    Guo, R
    Zhang, SK
    Ying, T
    Lei, YQ
    RARE METAL MATERIALS AND ENGINEERING, 2003, 32 (03) : 228 - 231
  • [26] Phase structure and electrochemical properties of La0.7Ce0.3Ni3.75Mn0.35Al0.15Cu0.75-x(Fe0.43B0.57)x hydrogen storage alloys
    Liu, Baozhong
    Hu, Mengjuan
    Ji, Liqiang
    Fan, Yanpin
    Wang, Yongguang
    Zhang, Zhi
    Li, Anming
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 516 : 53 - 57
  • [27] Structure and electrochemical properties of La0.7Mg0.3Ni2.45-xCo0.75Mn0.1Al0.2Wx (x=0-0.15) hydrogen storage alloys
    Pan, HG
    Wu, XF
    Gao, MX
    Chen, N
    Yue, YJ
    Lei, YQ
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (04) : 517 - 523
  • [28] Effects of annealing temperature on structure and the electrochemical properties of La0.7Mg0.3Ni2.45Co0.75Mn0.1Al0.2 hydrogen storage alloy
    Pan, HG
    Chen, N
    Gao, MX
    Li, R
    Lei, YQ
    Wang, QD
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 397 (1-2) : 306 - 312
  • [29] Effects of Mo0.46Fe0.54 Alloy on Microstructure and Electrochemical Hydrogen Storage Performances of La0.75Ce0.25Ni4.2Mn0.9-xCu0.3(Mo0.46Fe0.54)x (x=0-0.20) Alloys
    Cao, Jianliang
    Xie, Huanjian
    Wen, Zhihui
    Cao, Guohua
    Ji, Liqiang
    Fan, Yanping
    Liu, Baozhong
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (07): : 5854 - 5866
  • [30] A study on the structural and electrochemical properties of La0.7-xNdxMg0.3Ni2.45Co0.75Mn0.1Al0.2 (x=0.0-3.0) hydrogen storage alloys
    Ma, Shuai
    Gao, Mingxia
    Li, Rui
    Pan, Hongge
    Lei, Yongquan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 457 (1-2) : 457 - 464