Initial oxidation of Ni-based superalloy and its dynamic microscopic mechanisms: The interface junction initiated outwards oxidation

被引:61
作者
Zhai, Yadi [1 ]
Chen, Yanhui [1 ]
Zhao, Yunsong [2 ]
Long, Haibo [1 ]
Li, Xueqiao [1 ]
Deng, Qingsong [1 ]
Lu, Hui [1 ]
Yang, Xiaomeng [1 ]
Yang, Guo [1 ]
Li, Wei [1 ]
Yang, Luyan [1 ]
Mao, Shengcheng [1 ]
Zhang, Ze [3 ]
Li, Ang [1 ]
Han, Xiaodong [1 ]
机构
[1] Beijing Univ Technol, Inst Microstruct & Property Adv Mat, Beijing 100124, Peoples R China
[2] Beijing Inst Aeronaut Mat, Sci & Technol Adv High Temp Struct Mat Lab, Beijing 100095, Peoples R China
[3] Zhejiang Univ, Sch Mat Sci & Engn, Hangzhou 310007, Peoples R China
基金
北京市自然科学基金;
关键词
Nickel-based superalloy; Oxidation; Interface; Junction; Dynamic mechanism; HIGH-TEMPERATURE OXIDATION; LATTICE MISFIT; RESISTANCE; PROFILES; ALLOY; RATIO;
D O I
10.1016/j.actamat.2021.116991
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Understanding the high-temperature initial oxidation mechanism and its dynamic processes is generally important because a small amount of initial oxidation can induce rapid corrosion and cause catastrophic failure. We reveal the mechanism of initial oxidation in a third-generation Ni-based superalloy by in situ visualizations and investigations of the nano- and atomic-scale dynamic processes from room temperature to 900 degrees C with a Cs-corrected environmental transmission electron microscope. The initial oxidation starts from the gamma/gamma' interface at low temperatures. The high-temperature oxidation process with deficient oxygen prefers oxidation sites at the cross-junctions of the gamma/gamma' interfaces. The growth rate of the oxide nanoparticles depends on the oxidation temperatures, with a low rate below 600 degrees C and a rapid-growth speed at temperatures higher than 700 degrees C. Mass transfer from the gamma' and gamma phases to the gamma/gamma' interface, particularly at the cross-junctions of these interfaces, is observed to cause oxide accumulation. This study provides a direct observation of the interphase, interface-junction-initiated outward oxidization including Al and Cr elements. These results shed light on the initial oxidation mechanisms of materials containing a second phase with interphase interfaces and the materials at deficient oxygen conditions as well as those with protection coating layers. (C) 2021 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Competitive oxidation behavior of Ni-based superalloy GH4738 at extreme temperature
    Xu, Hui
    Yang, Shufeng
    Wang, Enhui
    Liu, Yunsong
    Guo, Chunyu
    Hou, Xinmei
    Zhang, Yanling
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2024, 31 (01) : 138 - 145
  • [22] Oxidation-fatigue damage mechanisms in a directionally solidified Ni-based superalloy at 850oC
    Rai, R. K.
    Chandra, S.
    Singh, A. P.
    Paulose, N.
    Srivastava, C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 922
  • [23] High temperature oxidation behavior of Ni-based superalloy Nimonic95 and the effect of pre-oxidation treatment
    Li, Danhong
    Chen, Junxiu
    Etim, Iniobong P.
    Liu, Ya
    Wu, Changjun
    Wang, Jianhua
    Su, Xuping
    VACUUM, 2021, 194
  • [24] Thickness Effects on Oxidation Behavior and Consequent γ' Degradation of a High-Al Ni-Based Single Crystal Superalloy
    Zhao, Haigen
    Guo, Wenqi
    Zhao, Wenyue
    Ru, Yi
    Wang, Junwu
    Pei, Yanling
    Gong, Shengkai
    Li, Shusuo
    CRYSTALS, 2023, 13 (02)
  • [25] Oxidation micromechanics and contribution during the low-cycle fatigue failure of a Ni-based single crystal superalloy
    Li, Y. M.
    Guo, H. Y.
    Wang, X. G.
    Tan, Z. H.
    Yang, Y. H.
    Du, Y. L.
    Liu, J. L.
    Liu, J. D.
    Zhou, Y. Z.
    Sun, X. F.
    INTERNATIONAL JOURNAL OF FATIGUE, 2025, 190
  • [26] The effect of Gd addition on the cyclic oxidation behavior and creep life of alumina-forming Ni-based superalloy
    Yun, Dae Won
    Seo, Seong Moon
    Jeong, Hi Won
    Yoo, Young Soo
    CORROSION SCIENCE, 2020, 170 (170)
  • [27] The Effect of Surface Machining on the High-Temperature Oxidation of a Single Crystal Ni-Based Superalloy
    Sun, Nairong
    Zhang, Lanting
    Li, Zhigang
    Sun, Feng
    Dong, Xianping
    Shan, Aidang
    MATERIALS TRANSACTIONS, 2014, 55 (10) : 1540 - 1546
  • [28] Surface Integrity and Oxidation of a Powder Metallurgy Ni-Based Superalloy Treated by Laser Shock Peening
    Tan, Qing
    Yan, Zhiran
    Huang, Hua
    Li, Shilei
    Wang, Yandong
    Feng, Yefei
    Zhou, Xin
    Li, Yinghong
    Ren, Yang
    Antonov, Stoichko
    JOM, 2020, 72 (05) : 1803 - 1810
  • [29] The Effect of Nb, Ta, and Ti on the Oxidation of a New Polycrystalline Ni-Based Superalloy
    J. W. X. Wo
    M. C. Hardy
    H. J. Stone
    High Temperature Corrosion of Materials, 2024, 101 : 485 - 509
  • [30] The effect of amorphous coating on high temperature oxidation resistance of Ni-based single crystal superalloy
    Wang, Mingming
    Cheng, Xiaopeng
    Jiang, Wenxiang
    Cao, Tianci
    Liu, Xianqiang
    Lu, Junxia
    Zhang, Yuefei
    Zhang, Ze
    CORROSION SCIENCE, 2023, 213