Effect of the Different Printing Patterns of Graphene Nanoparticles in Conductive Ink on Electrical and Mechanical Performance

被引:0
作者
Saad, Adzni Md. [1 ,2 ]
Salim, Mohd Azli [1 ,2 ,3 ]
Al-Mola, Mohammed Hussin A. [4 ]
Ahmad, Fauzi [1 ]
Saad, Hartini [5 ]
Akop, Mohd Zaid
机构
[1] Univ Tekn Malaysia Melaka, Fak Kejuruteraan Mekanikal, Durian Tunggal 76100, Melaka, Malaysia
[2] Univ Tekn Malaysia Melaka, Adv Mfg Ctr, Durian Tungggal 76100, Melaka, Malaysia
[3] Intelligent Engn Technol Serv Sdn, Bhd 1 Jalan TU43 Taman Tasik Utama, Ayer Keroh 76450, Melaka, Malaysia
[4] Univ Mosul, Fac Petr & Min Engn Univ Mosul, Mosul, Iraq
[5] Sekolah Kejuruteraan dan Sains Kreatif, Jabatan Kejuruteraan, Jalan Kulai Kota Tinggi KM 16, Jalan Kulai 81000, Johor, Malaysia
来源
INTERNATIONAL JOURNAL OF NANOELECTRONICS AND MATERIALS | 2021年 / 14卷
关键词
Graphene nanoparticles; conductive ink; sheet resistivity; nanoindentation; morphology analysis; NANOINDENTATION;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The utilization of graphene in the formation of conductive ink has been positively accepted by the electronics industry especially with the emerging of printable and flexible electronics. Because of that, it motivates this study to investigate the electrical, mechanical, and morphological properties for different patterns of Graphene Nanoparticle (GNP) conductive ink The samples were prepared using the screen-printing technique with a low annealing temperature of 100 degrees C for 30 minutes. The investigated parameter for the electrical property was the sheet resistivity, which showed that the zigzag pattern recorded the highest value of 1.077 k Omega/sq at the 3 mm of ink thickness. For the mechanical properties, the highest of hardness for 2 mm thickness was the curve pattern and for 3 mm was the square pattern, with the values of 3.849 GPa and 4.913 GPa. Both maximum values showed a direct correlation with the behavior of the elastic modulus of the ink The maximum values of elastic modulus were recorded at the same ink pattern and thickness. For the morphological analysis, the surface roughness and qualitative analysis using SEM images were performed. The surface roughness showed that the increase of GNP in the composition increased the surface roughness because it decreased the homogeneity of the mixture. The recorded SEM images of the ink layer microstructure surface showed a direct correlation with the obtained sheet resistivity data. The samples that produced high sheet resistivity showed the presence of bumps, creases, and defects on the ink layer surface. Based on the obtained data, the correlation between electrical, mechanical, and morphological properties can be established for the GNP conductive ink with various patterns and thicknesses.
引用
收藏
页码:225 / 240
页数:16
相关论文
共 30 条
  • [1] Abdullah M., 2014, EFFECT PARTICLE SIZE
  • [2] Fabrication of Stretchable Circuits on Polydimethylsiloxane (PDMS) Pre-Stretched Substrates by Inkjet Printing Silver Nanoparticles
    Abu-Khalaf, Jumana M.
    Al-Ghussain, Loiy
    Al-Halhouli, Ala'aldeen
    [J]. MATERIALS, 2018, 11 (12)
  • [3] An elastic-plastic indentation model for different geometric indenters and its applications
    Chen, Hui
    Cai, Li-xun
    Li, Chuanxi
    [J]. MATERIALS TODAY COMMUNICATIONS, 2020, 25
  • [4] How is flexible electronics advancing neuroscience research?
    Chen, Yihang
    Rommelfanger, Nicholas J.
    Mahdi, Ali I.
    Wu, Xiang
    Keene, Scott T.
    Obaid, Abdulmalik
    Salleo, Alberto
    Wang, Huiliang
    Hong, Guosong
    [J]. BIOMATERIALS, 2021, 268
  • [5] Dai L, 2006, CARBON NANOTECHNOLOGY: RECENT DEVELOPMENTS IN CHEMISTRY, PHYSICS, MATERIALS SCIENCE AND DEVICE APPLICATIONS, P1
  • [6] Defects, a challenge for graphene in flexible electronics
    Giesbers, A. J. M.
    Bouten, P. C. P.
    Cillessen, J. F. M.
    van der Tempel, L.
    Klootwijk, J. H.
    Pesquera, A.
    Centeno, A.
    Zurutuza, A.
    Balkenende, A. R.
    [J]. SOLID STATE COMMUNICATIONS, 2016, 229 : 49 - 52
  • [7] Analysis of the nanoindentation load-displacement curves measured on high-purity fine-grained alumina
    Gong, JH
    Peng, ZJ
    Miao, HZ
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (05) : 649 - 654
  • [8] Ho-anh-duc Nguyen, 2011, 2011 8th International Conference on Ubiquitous Robots and Ambient Intelligence (URAI 2011), P685, DOI 10.1109/URAI.2011.6145908
  • [9] Optimization of graphene conductive ink using solvent exchange techniques for flexible electronics applications
    Htwe, Y. Z. N.
    Abdullah, M. K.
    Mariatti, M.
    [J]. SYNTHETIC METALS, 2021, 274
  • [10] Ismail N, 2020, INT J NANOELECTRON M, V13, P305