Microstructural refinement by the formation of acicular ferrite on Ti-Mg oxide inclusion in low-carbon steel

被引:29
|
作者
Liu, Fangce [1 ]
Li, Jiawang [1 ]
Wang, Qi [1 ]
Liu, Yandong [1 ]
Bai, Yang [2 ]
He, Tong [3 ]
Yuan, Guo [4 ]
机构
[1] Northeastern Univ, Minist Educ, Key Lab Anisotropy & Texture Mat, Shenyang 110819, Liaoning, Peoples R China
[2] Liaoning Tech Univ, Sch Mat Sci & Engn, Shenyang 110819, Liaoning, Peoples R China
[3] Northeastern Univ, Res Acad, Shenyang 110819, Liaoning, Peoples R China
[4] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Liaoning, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2021年 / 824卷
关键词
Acicular ferrite; Ti-Mg oxide Inclusion; Mn-depleted zone; Lattice disregistry; Impact toughness; AUSTENITE GRAIN-SIZE; INTRAGRANULAR NUCLEATION; TRANSFORMATION; BEHAVIOR; GROWTH;
D O I
10.1016/j.msea.2021.141795
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, the mechanical properties and microstructure of hot-rolled low carbon steel containing Ti-Mg oxide inclusions as well as the effect of austenite grain size on acicular ferrite (AF) nucleation and the nucleation mechanism of AF were studied. The results indicated that the dominant inclusions in Ti-Mg deoxidized steel comprised Ti-Mg-Mn-O center dot MnS, which effectively promoted the nucleation of AF; thus, the microstructure after hot rolling consisted of fine AF and bainite (B). The variety of tensile property of Ti-Mg deoxidized steel was not obvious but the low-temperature impact toughness was significantly improved from 4 J to 126 J at -40 degrees C compared with Al deoxidized steel. Increasing the austenitizing temperature contributed to the nucleation of AF, and large amounts of fine AF formed in Ti-Mg deoxidized steel when the austenitizing temperature was 1250 degrees C with an average austenite grain size of similar to 92 mu m. Two kinds of nucleation mechanisms of AF were elucidated: a Nishiyama-Wasserman (N-W) orientation relationship of (100)(ferrite)parallel to(110)(oxide), [011](ferrite)parallel to[-111](oxide) between AF and Ti-Mg-Mn-O oxide, which caused low lattice disregistry, and a Mn-depleted zone (MDZ) around Ti-Mg-Mn-O center dot MnS inclusions. In order to investigate the reason for the formation of the MDZ, focused ion beam (FIB) was used to prepare the transmission electron microscope (TEM) sample containing a Ti-Mg-Mn-O center dot MnS inclusion, the specific orientation relationship of (-11-1)(MnS)parallel to(11-1)(oxide), [-112](MnS)parallel to[011](oxide) between MnS and the Ti-Mg-Mn-O oxide was examined, and the atomic image of the Ti-Mg-Mn-O oxide was observed. The precipitation of MnS on the surface of Ti-Mg-Mn-O oxide followed by the absorption of Mn atoms by Ti-Mg-Mn-O oxide resulted in the formation of a MDZ around Ti-Mg-Mn-O center dot MnS inclusions.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Lattice misfit between inclusion and acicular ferrite in weld metal of low carbon low alloy steel
    Graduate school of Engineering, Osaka University, Japan
    不详
    Yosetsu Gakkai Ronbunshu, 2009, 2 (114s-117s): : 114s - 117s
  • [32] Microstructural characteristic and toughening of an ultralow carbon acicular ferrite pipeline steel
    Zhao, MC
    Xiao, FR
    Shan, YY
    Li, YH
    Yang, K
    ACTA METALLURGICA SINICA, 2002, 38 (03) : 283 - 287
  • [33] ACICULAR FERRITE IN WELD METAL OF LOW CARBON STEEL
    Prokic-Cvetkovic, Radica
    Milosavljevic, Andelka
    Popovic, Olivera
    Kovacevic, Katarina
    STRUCTURAL INTEGRITY AND LIFE-INTEGRITET I VEK KONSTRUKCIJA, 2005, 5 (01): : 31 - 43
  • [34] The nanohardness of acicular ferrite and bainitic ferrite in low carbon microalloying steel
    Shang, C. J.
    Liang, X.
    Wang, X. M.
    He, X. L.
    Liu, H.
    PRICM 6: SIXTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-3, 2007, 561-565 : 65 - 68
  • [35] Non-metallic inclusions and acicular ferrite in low carbon steel
    Oh, YJ
    Lee, SY
    Byun, JS
    Shim, JH
    Cho, YW
    MATERIALS TRANSACTIONS JIM, 2000, 41 (12): : 1663 - 1669
  • [36] Mechanism of Acicular Ferrite Formation in Low Carbon Steel Ti-B Weld Metals with Different Oxygen Levels
    Yamada, Tomonori
    Terasaki, Hidenori
    Komizo, Yu-ichi
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2010, 96 (10): : 608 - 613
  • [37] Effect of aluminium content on acicular ferrite formation in low carbon steel weld metals
    Takada, A.
    Terasaki, H.
    Komizo, Y.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2013, 18 (02) : 91 - 97
  • [38] Inclusion characteristics and acicular ferrite formation in 1.8%Ni low carbon Al-killed steel with MgO nanoparticles addition
    Meng Sun
    Yang Li
    Zhou-hua Jiang
    Shuai Ma
    Yong-shuai Ji
    Yun-qie Mao
    Chang-yong Chen
    Yu-cheng Wang
    Rui Yang
    Journal of Iron and Steel Research International, 2024, 31 (12) : 3007 - 3021
  • [39] Inclusion Characteristics and Acicular Ferrite Nucleation in Ti-Containing Weld Metals of X70 Pipeline Steel
    Wang, Bingxin
    Liu, Xianghua
    Wang, Guodong
    STEEL RESEARCH INTERNATIONAL, 2018, 89 (02)
  • [40] In situ observation of growth behaviour of acicular ferrite in low-carbon steel containing 13 ppm magnesium
    Lin, Chi-Kang
    Pan, Yan-Chi
    Hwang, Weng-Sing
    Fang, Ying-Chien
    Su, Yen-Hao
    Lin, Guan-Ru
    Wu, Yun-Fang
    IRONMAKING & STEELMAKING, 2019, 46 (02) : 176 - 183