CoMoCrSi coatings prepared by high-velocity oxygen fuel spraying: microstructure and mechanical properties at elevated temperatures up to 800 °C

被引:12
|
作者
Guo, Hongjian [1 ,2 ,3 ]
Wang, Yijing [2 ]
Hao, Enkang [2 ]
Li, Bo [4 ]
An, Yulong [2 ]
Chen, Jianmin [2 ]
Zhou, Huidi [2 ]
Yan, Pengxun [1 ]
Wu, Zhiguo [1 ]
机构
[1] Gansu Acad Sci, Inst Nanomat Applicat Technol, Lanzhou 730000, Peoples R China
[2] Chinese Acad Sci, Lanzhou Inst Chem Phys, State Key Lab Solid Lubricat, Lanzhou 730000, Peoples R China
[3] Lanzhou City Univ, Sch Bailie Mech Engn, Lanzhou 730070, Peoples R China
[4] Xi An Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
high-velocity oxygen fuel spraying; CoMoCrSi coating; microstructure; tribological performance; wear mechanism; WC-CO; HEAT-TREATMENT; TRIBOLOGICAL PROPERTIES; OXIDATION BEHAVIOR; WEAR-RESISTANCE; ALLOY; PERFORMANCE; FABRICATION; DEPOSITION; OXIDE;
D O I
10.1088/2053-1591/ab6374
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructures, mechanical properties, and tribological behaviors from room temperature (RT) to 800 degrees C of HOVF-sprayed CoMoCrSi coatings were investigated in detail. The as-sprayed CoMoCrSi coatings were found to be predominantly composed of intermetallic Laves phases, i.e., Co7Mo6, Co3Mo2Si, Cr3Si, and some amorphous phases. The as-sprayed coatings possessed a compact and typical lamellar microstructure and balanced mechanical property; their Vickers hardness decreased from 855.9 +/- 16 HV5.0 at RT to 583.9 +/- 10 HV5.0 at 800 degrees C due to a normal soft phenomenon of material in hot environment. Further, between room temperature and 400 degrees C, the as-sprayed coatings suffered serious mechanical wear without any lubricant tribolayer forming on the worn surface, indicating that they would not function as good anti-wear materials at low temperatures. In particular, the coatings exhibited a brittle fracture coupled with abrasive wear at RT, obvious abrasive wear at 200 degrees C, and severe adhesive wear at 400 degrees C that with the highest friction coefficient of 0.65 and wear rate of 35.79 x 10(-6) mm(3)/(N.m). As the test temperature increased to 600 and 800 degrees C, the friction coefficient of the coating decreased to 0.45 and 0.26, respectively, and the corresponding wear rates reached 0.135 x 10(-6) mm(3)/(N.m) and 0.288 x 10(-6) mm(3)/(N.m), with a difference of approximately two orders of magnitude between the low- and high-temperature wear rate. This result further confirmed that the as-sprayed coatings are a better choice of abrasion-resistant materials for high-temperature applications. After sliding tests at 800 degrees C, numerous metallic oxides i.e., Co3O4, MoO3, and bimetallic oxides such as CoMoO4 and Co2CrO4 of nanometer size (50-100 nm) were identified in the continuous protective layer formed on the worn surface. These oxides played an important role of lubrication and reduced direct contact between the coating and its counterpart during the sliding process, leading to a decrease in the friction coefficient and material loss. The main wear mechanisms of the coatings at this temperature range are slight adhesive wear coupled with abrasive wear.
引用
收藏
页数:18
相关论文
共 50 条
  • [21] Microstructure and properties of high velocity arc spraying coatings
    Liang, Xiubing
    Xu, Binshi
    Ma, Shining
    Jixie Gongcheng Xuebao/Chinese Journal of Mechanical Engineering, 2003, 39 (02): : 119 - 122
  • [22] Microstructure and tribological properties of CrB2-enhanced NiCrBSi composite coatings prepared by high-velocity oxygen-fuel under different kerosene flow rates
    Chang, Cheng
    Liu, Xia
    Zhang, Shihong
    Ren, Yi
    Yang, Kang
    Yang, Yang
    SURFACE & COATINGS TECHNOLOGY, 2025, 496
  • [23] Oxidation Behavior of NiCoCrAlY Coatings Deposited by Vacuum Plasma Spraying and High-Velocity Oxygen Fuel Processes
    Kim, Junseong
    Pyeon, Janghyeok
    Kim, Bong-Gu
    Khadaa, Tserendorj
    Choi, Hyeryang
    Zhe, Lu
    Dube, Tejesh
    Zhang, Jing
    Yang, Byung-il
    Jung, Yeon-gil
    Yang, SeungCheol
    COATINGS, 2023, 13 (02)
  • [24] Tribochemical behavior of alumina coatings deposited by high-velocity oxy fuel spraying
    Khosravifard, A.
    Salahinejad, E.
    Yaghtin, A. H.
    Araghi, A.
    Akhbarizadeh, A.
    CERAMICS INTERNATIONAL, 2015, 41 (04) : 5713 - 5720
  • [25] Fabrication and characterization of nanostructured hydroxyapatite coating on Mg-based alloy by high-velocity oxygen fuel spraying
    Mardali, Marzieh
    Salimijazi, Hamidreza
    Karimzadeh, Fathallah
    Luthringer-Feyerabend, Berengere J. C.
    Blawert, Carsten
    Labbaf, Sheyda
    CERAMICS INTERNATIONAL, 2018, 44 (12) : 14667 - 14676
  • [26] Microstructure and properties of high velocity oxygen fuel sprayed (WC-Co)-Ni coatings
    Fu, Wei
    Chen, Qing-Yu
    Yang, Chao
    Yi, Deng-Liang
    Yao, Hai-Long
    Wang, Hong-Tao
    Ji, Gang-Chang
    Wang, Fang
    CERAMICS INTERNATIONAL, 2020, 46 (10) : 14940 - 14948
  • [27] Particle melting behavior during high-velocity oxygen fuel thermal spraying
    He J.
    Ice M.
    Lavernia E.
    Journal of Thermal Spray Technology, 2001, 10 (01) : 83 - 93
  • [28] The Surface Properties of WC-Co-Cr Based Coatings Deposited by High Velocity Oxygen Fuel Spraying
    Ozbek, Y. Y.
    Canikoglu, N.
    Ipek, M.
    ACTA PHYSICA POLONICA A, 2017, 131 (01) : 186 - 189
  • [29] Molybdenum based amorphous and nanocrystalline coatings prepared by high velocity oxy-fuel spraying
    Fan Zishuan
    Yu Hongying
    Wang Xudong
    RARE METALS, 2012, 31 (04) : 355 - 361
  • [30] The effect of high-velocity oxy-fuel spraying parameters on microstructure, corrosion and wear resistance of Fe-based metallic glass coatings
    Zhang, Han
    Hu, Yong
    Hou, Guoliang
    An, Yulong
    Liu, Guang
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2014, 406 : 37 - 44