Oxidation behaviour of the nickel-based superalloy DZ125 hot-dipped with Al coatings doped by Si

被引:40
作者
Zang, Junjie [1 ]
Song, Peng [1 ]
Feng, Jing [1 ]
Xiong, Xiping [1 ]
Chen, Rong [1 ]
Liu, Guangliang [1 ]
Lu, Jiansheng [1 ]
机构
[1] Kunming Univ Sci & Technol, Fac Mat Sci & Engn, Kunming 650093, Peoples R China
基金
中国国家自然科学基金;
关键词
Metal coatings; Superalloys; SEM; XRD; Oxidation; SINGLE-CRYSTAL SUPERALLOY; CYCLIC OXIDATION; PACK CEMENTATION; STAINLESS-STEEL; MICROSTRUCTURE; RESISTANCE; ALLOY; CODEPOSITION; SILICON;
D O I
10.1016/j.corsci.2016.07.020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A pure Al coating and Al-Si coating were prepared on the surface of the DZ125 superalloy by hot-dipping. The Al-Si coating provides better thermal oxidation resistance than that of the pure Al coating due to the formation of a more compact Al2O3 layer. The microstructure of the Al-Si coating shows a silicon aluminium-based layer with Ta5Si3 and AIHfSi phase forms after heat treatment in argon at 850 degrees C. This layer is a barrier to the diffusion of oxygen and other metal elements during cyclic oxidation, which has a significant effect on the formation of the compact Al2O3 layer. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:170 / 179
页数:10
相关论文
共 33 条
  • [1] The morphology of coating/substrate interface in hot-dip-aluminized steels
    Awan, Gul Hameed
    Ul Hasan, Faiz
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 472 (1-2): : 157 - 165
  • [2] Effect of nickel pre-plating on high-temperature oxidation behavior of hot-dipped aluminide mild steel
    Cheng, Wei-Jen
    Liao, Yi-Jhang
    Wang, Chaur-Jeng
    [J]. MATERIALS CHARACTERIZATION, 2013, 82 : 58 - 65
  • [3] Mechanisms of oxidation and its role in microstructural evolution of metallic thermal spray coatings - Case study for Ni-Al
    Deshpande, S
    Sampath, S
    Zhang, H
    [J]. SURFACE & COATINGS TECHNOLOGY, 2006, 200 (18-19) : 5395 - 5406
  • [4] Development of hard intermetallic coatings on austenitic stainless steel by hot dipping in an Al-Si alloy
    Frutos, E.
    Gonzalez-Carrasco, J. L.
    Capdevila, C.
    Jimenez, J. A.
    Houbaert, Y.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2009, 203 (19) : 2916 - 2920
  • [5] Microstructure and oxidation behavior of Al plus Si co-deposited coatings on nickel-based superalloys
    Fu, C.
    Kong, W. K.
    Cao, G. H.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 258 : 347 - 352
  • [6] Microstructure and hot corrosion behavior of Co-Si modified aluminide coating on nickel based superalloys
    He, Haiyan
    Liu, Zongjie
    Wang, Wan
    Zhou, Chungen
    [J]. CORROSION SCIENCE, 2015, 100 : 466 - 473
  • [7] Hong M.Z., 1995, J JILIN I CHEM TECHN, V2, P51
  • [8] Microstructure and corrosion resistance of rare earth NiCrMoY alloy coatings
    Hu, C. L.
    Hou, S. L.
    [J]. MATERIALS RESEARCH INNOVATIONS, 2015, 19 : 190 - 193
  • [9] The microstructure of aluminized type 310 stainless steel
    Hu, T. L.
    Huang, H. L.
    Gan, D.
    Lee, T. Y.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2006, 201 (06) : 3502 - 3509
  • [10] Effects of targeted γ-Ni plus γ′-Ni3Al-based coating compositions on oxidation behavior
    Izumi, T.
    Mu, N.
    Zhang, L.
    Gleeson, B.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2007, 202 (4-7) : 628 - 631