共 50 条
Adsorption characteristics of CN- species on the chalcopyrite surface and its response to flotation
被引:19
|作者:
Zhao, Qianfei
Yang, Hongying
Tong, Linlin
[1
]
机构:
[1] Northeastern Univ, Key Lab Ecol Met Multimetall Mineral, Minist Educ, Shenyang 110819, Liaoning, Peoples R China
基金:
国家重点研发计划;
关键词:
Chalcopyrite;
Cyanide adsorption;
Coverage thickness;
Inhibition;
ToF-SIMS;
LEACHING BEHAVIOR;
XPS SPECTRA;
TOF-SIMS;
CYANIDE;
MECHANISM;
COPPER;
SPHALERITE;
RECOVERY;
XANTHATE;
IONS;
D O I:
10.1016/j.seppur.2021.119322
中图分类号:
TQ [化学工业];
学科分类号:
0817 ;
摘要:
Among cyanide tailings, chalcopyrite is one of the main minerals. However, little study is available regarding the flotation behavior and mechanism of cyanide chalcopyrite, especially the influence of cyanide leaching time on the physical and chemical properties of chalcopyrite surface. In this work, the cyanide adsorption mechanism of the chalcopyrite surface over time and its response to flotation was probed for the first using contact angle, zeta potential, microflotation, X - ray photoelectron spectroscopy (XPS) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). The results of contact angle showed that the surface hydrophobicity of the chalcopyrite surface decreased with increasing cyanidation time, thus preventing the adsorption of xanthate, which was confirmed by zeta potential and microflotation. XPS analysis indicated that with the gradual progress of cyanidation, hydrophilic CN-, CNO-, SO42- and CuCN- were formed on the surface of chalcopyrite. ToF-SIMS investigated the distribution of anion species on the surface of chalcopyrite, showing that with the increasing cyanidation time, more cyanide species formed on the surface of mineral layer, and gradually diffuse from the mineral surface to the bulk phase, finally forming a film with depth of about 20 nm. Thus, the chalcopyrite hydrophobicity was depressed.