Thermal expansion coefficient tailoring of LAS glass-ceramic for anodic bondable low temperature co-fired ceramic application

被引:22
|
作者
Wei, Anqing [1 ,2 ]
Liu, Zhifu [1 ,2 ]
Zhang, Faqiang [1 ]
Ma, Mingsheng [1 ]
Chen, Guanyu [1 ,2 ]
Li, Yongxiang [3 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, CAS Key Lab Inorgan Funct Mat & Devices, Shanghai 200050, Peoples R China
[2] Univ Chinese Acad Sci, Ctr Mat Sci & Optoelect Engn, Beijing 100049, Peoples R China
[3] RMIT Univ, Sch Engn, Melbourne, Vic 3000, Australia
基金
中国国家自然科学基金;
关键词
Anodic bonding; Thermal expansion; Spodumene; Glass-ceramic; X-RAY-DIFFRACTION; LI2O-AL2O3-SIO2; GLASS; ALUMINOSILICATE GLASS; NUCLEATING-AGENT; CRYSTALLIZATION; ZRO2; SPODUMENE; LITHIUM; DESIGN; TIO2;
D O I
10.1016/j.ceramint.2019.10.209
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Li-Al-Si glass-ceramics were prepared by conventional glass-ceramic fabrication method. The influences of Na2O content on the sintering property, microstructure, and coefficient of thermal expansion were investigated. The results show that the coefficient of thermal expansion of LAS glass-ceramics can be tailored to match that of silicon by the addition of Na2O content. Na2O has a remarkable influence on the crystallinity of Li-Al-Si glass-ceramic. The coefficient of thermal expansion of Li-Al-Si glass-ceramic is thus tunable between that of glass phase and crystal phase. The Si-O bond length change in stretch vibration modes introduced by Na2O also contributes to the variation of coefficient of thermal expansion of the Li-Al-Si glass-ceramics. The coefficient of thermal expansion of the Li-Al-Si glass-ceramic with 1.5 wt% Na2O addition is about + 3.34 ppm/degrees C at 350 degrees C and shows a good compatibility to that of silicon in a wide temperature range, which makes it a promising candidate for anodic bondable low temperature co-fired ceramic substrate applications.
引用
收藏
页码:4771 / 4777
页数:7
相关论文
共 50 条
  • [31] Super Compact Low-Temperature Co-Fired Ceramic Bandpass Filters Using the Hybrid Resonator
    Yang, Tao
    Tamura, Masaya
    Itoh, Tatsuo
    IEEE TRANSACTIONS ON MICROWAVE THEORY AND TECHNIQUES, 2010, 58 (11) : 2896 - 2907
  • [32] A Low Temperature Co-Fired Ceramic-Based Dielectrophoretic Device for Manipulating Micro and Nanostructure Materials
    Seon, Ji-Yun
    Yoon, Young Joon
    Choi, Jaekyoung
    Kim, Hyo Tae
    Kim, Chang-Yeoul
    Kim, Jong-Hee
    Baik, Hong Koo
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2013, 13 (11) : 7540 - 7545
  • [33] Current Research Status of Low Temperature Sintering Glass-ceramic
    KANG Jing-rui
    ZHAO Ya-bin
    ZHAO Ying-na
    科技视界, 2015, (26) : 203 - 203
  • [34] Glass-Ceramic Materials Synthesized By Low-Temperature Plasma
    Vlasov, V. A.
    Skripnikova, N. K.
    Volokitin, G. G.
    Ushkov, V. A.
    Bruyako, M. G.
    Zorin, D. A.
    RUSSIAN PHYSICS JOURNAL, 2023, 66 (02) : 159 - 165
  • [35] Glass-Ceramic Materials Synthesized By Low-Temperature Plasma
    V. A. Vlasov
    N. K. Skripnikova
    G. G. Volokitin
    V. A. Ushkov
    M. G. Bruyako
    D. A. Zorin
    Russian Physics Journal, 2023, 66 : 159 - 165
  • [36] Densification and microwave properties of low-temperature co-fired CaO-B2O3-SiO2 glass-ceramic with La-B-Si additions
    Zhou, Xiaohua
    Li, Enzhu
    Yang, Shilin
    Li, Bo
    Tang, Bin
    Yuan, Ying
    Zhang, Shuren
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2013, 104 (06) : 606 - 608
  • [37] Fabrication and performance evaluation of a high temperature co-fired ceramic vaporizing liquid microthruster
    Cheah, Kean How
    Low, Kay-Soon
    JOURNAL OF MICROMECHANICS AND MICROENGINEERING, 2015, 25 (01)
  • [38] Formation of glass-ceramic materials based on pyroxene solid solution-fluorapatite phases and their thermal expansion properties
    Salama, SN
    Saad, EA
    Darwish, H
    Abo-Mosallm, HA
    CERAMICS INTERNATIONAL, 2005, 31 (04) : 559 - 566
  • [39] Concurrent Crystallization Mechanism Leading to Low Temperature Percolation of LAGP Glass-Ceramic Electrolyte
    Bertrand, Marc
    Rousselot, Steeve
    Rioux, Maxime
    Ayme-Perrot, David
    Dolle, Mickael
    ACS APPLIED MATERIALS & INTERFACES, 2024, 16 (22) : 28818 - 28828
  • [40] Thermal shock resistance of SiC/MAS-LAS multilayer joint of carbon/carbon composites to LAS glass-ceramic
    Peng Han
    Fu Qian-Gang
    Jia Bing-Lin
    Li He-Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 607 - 611