Synthesis of nanosized composite powders via a wet chemical process for sintering high performance W-Y2O3 alloy

被引:66
作者
Dong, Zhi [1 ]
Liu, Nan [1 ]
Ma, Zongqing [1 ]
Liu, Chenxi [1 ]
Guo, Qianying [1 ]
Yamauchi, Yusuke [2 ,3 ]
Alamri, Hatem R. [4 ]
Alothman, Zeid A. [5 ]
Hossain, Md. Shahriar A. [2 ,3 ]
Liu, Yongchang [1 ]
机构
[1] Tianjin Univ, Sch Mat Sci & Engn, State Key Lab Hydraul Engn Simulat & Safety, Tianjin 300072, Peoples R China
[2] Natl Inst Mat Sci, Int Ctr Mat Nanoarchitecton MANA, 1-1 Namiki, Tsukuba, Ibaraki 3050044, Japan
[3] Univ Wollongong, Australian Inst Innovat Mat, North Wollongong, NSW 2500, Australia
[4] Umm Al Qura Univ, Jamoum Univ Coll, Phys Dept, Mecca 21955, Saudi Arabia
[5] King Saud Univ, Coll Sci, Chem Dept, Adv Mat Res Chair, Riyadh 11451, Saudi Arabia
基金
中国国家自然科学基金;
关键词
W-Y2O3; alloy; Wet chemical method; SPS; Ultrafine grain; PLASMA-FACING COMPONENTS; MECHANICAL-PROPERTIES; TUNGSTEN COMPOSITES; GRAIN-GROWTH; DENSIFICATION; SIZE;
D O I
10.1016/j.ijrmhm.2017.09.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
With the aim of preparing high performance oxide dispersion strengthened tungsten-based alloys by powder metallurgy, the W-Y2O3 composite nanopowders were prepared by an improved bottom-up wet chemical method. Ultrasonic treatment and anionic surfactant sodium dodecyl sulfate (SDS) addition were innovatively introduced into this wet chemical method in order to fabricate homogeneous, ultrafine W-Y2O3 composite nanopowders. As a result, the average tungsten grain size of 40-50 nm was obtained for this composite nano powders. For comparison, W-Y2O3 composite powders were also prepared by traditional mechanical milling. After that, spark plasma sintering (SPS) was employed to consolidate the powders prepared by either mechanical milling or wet chemical method to yield high density as well as suppress grain growth. It is found that the W-Y2O3 alloy prepared by wet chemical method and subsequent SPS possesses smaller grain size (0.76 +/- 0.17 mu m) and higher relative density (99.0%) than that prepared by mechanical milling and subsequent SPS. Moreover, the oxide nanoparticles (about 2-10 nm) are dispersed within tungsten grains and at grain boundaries more uniformly in W-Y2O3 alloy prepared by wet chemical method and subsequent SPS. Due to the ultrafine grains, high sintering density and homogeneously distributed oxide nanoparticles, the Vickers microhardness of yttria dispersion strengthened tungsten-based alloy prepared in our work reaches up to 598.7 +/- 7.3 HV0.2, higher than that reported in the previous studies. These results indicate that the improved bottom-up wet chemical method combined with ultrasonic treatment and anionic surfactant addition developed in our work is a promising way to fabricate high performance oxide dispersion strengthened tungsten-based alloys with ultrafine grain and high density.
引用
收藏
页码:266 / 272
页数:7
相关论文
共 50 条
  • [41] Microstructure and properties of La2O3 doped W composites prepared by a wet chemical process
    Li, Jianfeng
    Cheng, Jigui
    Wei, Bangzheng
    Zhang, Minglong
    Luo, Laima
    Wu, Yucheng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2017, 66 : 226 - 233
  • [42] Effects of high-energy ball milling of commercial Y2O3 powders on their densification using spark plasma sintering
    Park, Cheol Woo
    Lee, Jung Hun
    Kang, Suk Hyun
    Park, Jae Hwa
    Kim, Hyun Mi
    Kang, Hyo Sang
    Lee, Hee Ae
    Lee, Joo Hyung
    In, Jun Hyeong
    Shim, Kwang Bo
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2018, 19 (02): : 179 - 182
  • [43] Microstructure and transient laser thermal shock behavior of W-TiC-Y2O3 composites prepared by wet chemical method
    Xu, Meng-Yao
    Luo, Lai-Ma
    Lin, Jin-Shan
    Xu, Yue
    Zan, Xiang
    Xu, Qiu
    Tokunaga, Kazutoshi
    Zhu, Xiao-Yong
    Wu, Yu-Cheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 766 : 784 - 790
  • [44] Thermal shock behavior of W-0.5 wt% Y2O3 alloy prepared via a novel chemical method
    Zhao, Mei-Ling
    Luo, Lai-Ma
    Lin, Jing-Shan
    Zan, Xiang
    Zhu, Xiao-Yong
    Luo, Guang-Nan
    Wu, Yu-Cheng
    JOURNAL OF NUCLEAR MATERIALS, 2016, 479 : 616 - 622
  • [45] Green synthesis of nanocrystalline α-Al2O3 powders by both wet-chemical and mechanochemical methods
    Gao, Huiying
    Li, Zhiyong
    Zhao, Peng
    MODERN PHYSICS LETTERS B, 2018, 32 (08):
  • [46] Effect of the heating rate and Y2O3 coating on the microstructure of Wf/ Y2O3/W composites via field assisted sintering technology
    Shu, Rui
    Mao, Yiran
    Lau, Alexander
    Coenen, Jan W.
    Terra, Alexis
    Liu, Chao
    Riesch, Johann
    Linsmeier, Christian
    Broeckmann, Christoph
    NUCLEAR MATERIALS AND ENERGY, 2024, 38
  • [47] Microstructure and mechanical properties of a W-2wt.%Y2O3 composite produced by sintering and hot forging
    Battabyal, M.
    Schaeublin, R.
    Spaetig, P.
    Walter, M.
    Rieth, M.
    Baluc, N.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 442 (1-3) : S225 - S228
  • [48] Effect of source gases on CVD synthesis of CNTs@TiB2 composite powders using Ni/Y2O3 as the catalyst
    Lin, Jia
    Yang, Yihang
    Zhang, Houan
    Li, Fenqiang
    CERAMICS INTERNATIONAL, 2020, 46 (08) : 10704 - 10709
  • [49] High-performance B4C-LaB6 composite ceramics fabricated via hot-pressing sintering with La2O3 as sintering additive
    Yang, Mingsheng
    Zhuang, Yanxin
    Xing, Pengfei
    CERAMICS INTERNATIONAL, 2021, 47 (23) : 32675 - 32684
  • [50] Damage evolutions of completely recrystallized W-Y2O3 composite evaluated using the dual effects of electron beam thermal shock and helium ion irradiation
    Yao, Gang
    Zhao, Zhi-Hao
    Luo, Lai-Ma
    Cheng, Ji-Gui
    Zan, Xiang
    Xu, Qiu
    Wu, Yu-Cheng
    MATERIALS CHEMISTRY AND PHYSICS, 2021, 271