The Pr2O3/Si(001) interface

被引:32
|
作者
Schmeisser, D [1 ]
机构
[1] Brandenburg Tech Univ Cottbus, D-03013 Cottbus, Germany
关键词
electronic structure; high-k dielectric; resonant; photoelectron spectroscopy;
D O I
10.1016/S1369-8001(03)00072-6
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Praseodymium sequioxide (Pr2O3) is among the most promising hetero-oxides which are treated as candidates of choice to replace SiO2 as the gate dielectric material for sub-0.1mum CMOS technology. However, in order to enable the process integration the hetero-oxides require substantial characterization. In particular, the basic interaction mechanism at the interface to the silicon substrate is a key issue. A good knowledge of this mechanism is required to address the reliability issues. The challenges in material science are to understand the chemical bonding of the hetero-oxides to silicon in a microscopic scale. This report focuses on the studies of Pr2O3 ultra thin (<1 nm) epitaxial layers prepared in situ. Photoelectron spectroscopy (PES) is used for spectroscopic characterization of the interface elements as well as for a nondestructive depth profiling. We report on the atomic origin of the valence and conduction band states as revealed by resonant PES, on the valence band discontinuity, on the formation of interface dipole moment, and on the stability regime of a mixed silicate phase. Within the latter, the chemical state of Si atoms at the interface is identified and the chemical stability of the various oxide phases is discussed. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:59 / 70
页数:12
相关论文
共 50 条
  • [1] Pr2O3/Si(001) interface reactions and stability
    Schmeisser, D
    Dabrowski, J
    Müssig, HJ
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 109 (1-3): : 30 - 33
  • [2] Complex interface and growth analysis of single crystalline epi-Si(111)/Y2O3/Pr2O3/Si(111) heterostructures: Strain engineering by oxide buffer control
    Wilke, A.
    Yang, J. -M.
    Kim, J. W.
    Seifarth, O.
    Dietrich, B.
    Giussani, A.
    Zaumseil, P.
    Storck, P.
    Schroeder, T.
    SURFACE AND INTERFACE ANALYSIS, 2011, 43 (04) : 827 - 835
  • [3] Al-oxynitrides as a buffer layer for Pr2O3/SiC interfaces
    Sohal, Rakesh
    Torche, Mohamed
    Henkel, Karsten
    Hoffmann, Patrick
    Tallarida, Massimo
    Schmeisser, Dieter
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2006, 9 (06) : 945 - 948
  • [4] The interaction of Al, Ag, Au, and Ti to Pr2O3 thin film dielectrics
    Torche, M.
    Henkel, K.
    Schmeisser, D.
    MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2006, 26 (5-7): : 1127 - 1130
  • [5] Observation of Chemisorbed O2 Molecule at SiO2/Si(001) Interface During Si Dry Oxidation
    Tsuda, Yasutak
    Yoshigoe, Akitaka
    Ogawa, Shuich
    Sakamoto, Tetsuya
    Takakuwa, Yuji
    E-JOURNAL OF SURFACE SCIENCE AND NANOTECHNOLOGY, 2023, 21 (01) : 30 - 39
  • [6] Highly selective and stable nickel catalysts supported on ceria promoted with Sm2O3, Pr2O3 and MgO for the CO2 methanation reaction
    Siakavelas, G., I
    Charisiou, N. D.
    AlKhoori, S.
    AlKhoori, A. A.
    Sebastian, V
    Hinder, S. J.
    Baker, M. A.
    Yentekakis, I., V
    Polychronopoulou, K.
    Goula, M. A.
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2021, 282
  • [7] A density functional theory study of the Fe(001)/Fe3O4(001) interface
    Shikhman, I. A.
    Shelyapina, M. G.
    Kupriyanova, G. S.
    SOLID COMPOUNDS OF TRANSITION ELEMENTS II, 2013, 194 : 288 - +
  • [8] Band offsets at the epitaxial anatase TiO2/n-SrTiO3(001) interface
    Chambers, S. A.
    Ohsawa, T.
    Wang, C. M.
    Lyubinetsky, I.
    Jaffe, J. E.
    SURFACE SCIENCE, 2009, 603 (05) : 771 - 780
  • [9] Interfacial layer formation during the growth of Gd2O3 on Si(001) and its thermal stability
    Gribisch, Philipp
    Fissel, Andreas
    SEMICONDUCTOR SCIENCE AND TECHNOLOGY, 2021, 36 (11)
  • [10] Insight into interfacial structure and bonding nature of diamond(001)/Cr3C2(001) interface
    Gu, Kaixuan
    Pang, Mingjun
    Zhan, Yongzhong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 770 : 82 - 89