Effects of Different Silane Coupling Agent Monomers on Flexural Strength of an Experimental Filled Resin Composite

被引:17
作者
Matinlinna, Jukka P. [1 ]
Vallittu, Pekka K. [2 ]
Lassila, Lippo V. [2 ]
机构
[1] Univ Hong Kong, Fac Dent, Hong Kong, Hong Kong, Peoples R China
[2] Univ Turku, Inst Dent, Turku, Finland
关键词
Silanization; silane coupling agent; biomechanical properties; filled resin; resin composite; ADHESION; CONVERSION; SURFACE; METALS; CEMENT;
D O I
10.1163/016942410X503302
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The hydrolytic stability of various silane combinations and their effects on biomechanical properties and water sorption of an experimental dental composite made of bis-GMA and TEGDMA and silane-treated fillers were evaluated. Four silane coupling agents and their blends with a cross-linker silane were used as coupling agents for the 0.7-mu m BaSiO3 fillers. The silanization was carried out in toluene containing 1% (v/v) of one of the four following organofunctional silane coupling agents: 3-acryloxypropyltrimethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-styrylethyltrimethoxysilane and 3-isocyanatopropyltriethoxysilane. Blends of these functional silanes with 1% (v/v) of a cross-linker silane, 1,2-bis-(triethoxysilyl) ethane were also used for silanization. Composites were prepared by mixing 5.00 g Ba-glass filler with 2.00 g of a resin mixture consisting of bis-GMA (58.8 wt%) and TEGDMA (39.2 wt%) in a high-speed mixer. Three-point bending test specimens (2.0 mm x 2.0 mm x 25.0 mm) were fabricated (n = 8) in a mould and photo-polymerized. The degree of conversion was measured with FT-IR. Biomechanical testing was carried out according to the ISO 10477 standard. Specimens were tested (flexural strength) after 30 days of water storage (37 degrees C, distilled water). Water sorption and solubility (in wt%) were also measured on 1, 2, 3, 5, 7, 14, 21 and 30 days in water storage. Statistical analysis with ANOVA showed that the highest flexural strength was obtained when 3-acryloxypropyltrimethoxysilane + 1,2-bis-(triethoxysilyl) ethane (100.5 MPa; SD, 25.7 MPa) was used in the silanization step, and the lowest was obtained when 3-isocyanatopropyltriethoxysilane + 1,2-bis-(triethoxysilyl) ethane (28.9 MPa; SD, 8.8 MPa) was used. The three-point bending strength was significantly affected by the functionality of the main silane tested (p < 0.05), but not by the addition of the cross-linker silane (p > 0.05). The composite that had been silanized with 3-isocyanatopropyltriethoxysilane had the greatest amount of water uptake (1.75%), and the composite silanized with 3-methacryloxypropyltrimethoxysilane + 1,2-bis-(triethoxysilyl) ethane had the least (1.08%). In conclusion, selection of the functional silane monomer can be a significant factor in developing filled resin composites in dentistry. (C) Koninklijke Brill NV, Leiden, 2011
引用
收藏
页码:179 / 192
页数:14
相关论文
共 50 条
[41]   Interfacial adhesive strength of a silane coupling agent with metals: A first principles study [J].
Uetsuji, Yasutomo ;
Yagi, Takahiro ;
Nakamura, Yoshinobu .
MATERIALS TODAY COMMUNICATIONS, 2020, 25
[42]   Immediate and Tate Repair of Microhybrid Resin Composites: Effect of Silane Coupling Agent, Universal Adhesives and Photo Polymerization [J].
Ugurlu, Muhittin ;
Husain, Nadin Al-Haj ;
Ozcan, Mutlu .
EUROPEAN JOURNAL OF PROSTHODONTICS AND RESTORATIVE DENTISTRY, 2023, 31 (02) :116-125
[43]   Effect of water glass treatment for zirconia and silane coupling on bond strength of resin cement [J].
Ushijima, Kei ;
Hiraishi, Noriko ;
Ikeda, Masaomi ;
Tsuji, Yukiko ;
Tsuchida, Yumi ;
Shimada, Yasushi .
CLINICAL ORAL INVESTIGATIONS, 2024, 28 (06)
[44]   Effectiveness of surface treatments on fatigue and static flexural bond strength of a CAD-CAM resin composite [J].
Pilecco, Rafaela Oliveira ;
da Rosa, Lucas Saldanha ;
Soares, Pablo Machado ;
Rippe, Marilia Pivetta ;
Valandro, Luiz Felipe ;
Tribst, Joao Paulo Mendes ;
dal Piva, Amanda Maria de Oliveira ;
Kleverlaan, Cornelis Johannes ;
Pereira, Gabriel Kalil Rocha .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 140
[45]   Flexural properties of experimental nanofiber reinforced composite are affected by resin composition and nanofiber/resin ratio [J].
Vidotti, Hugo A. ;
Manso, Adriana P. ;
Leung, Victor ;
do Valle, Accacio L. ;
Ko, Frank ;
Carualho, Ricardo M. .
DENTAL MATERIALS, 2015, 31 (09) :1132-1141
[46]   Bond strength of a resin composite to a polyacid-modified resin composite under different conditions [J].
Benderli, YG ;
Koray, F ;
Turan, N .
QUINTESSENCE INTERNATIONAL, 2002, 33 (10) :770-775
[47]   Dielectric behaviour of silica filled vinyl solution-SBR in the presence of silane coupling agent [J].
Ward, A. A. ;
Bishai, A. M. ;
Hanna, F. F. ;
Yehia, A. A. ;
Stoll, B. ;
von Soden, W. ;
Herminghaus, S. ;
Mansour, A. A. .
KGK-KAUTSCHUK GUMMI KUNSTSTOFFE, 2006, 59 (12) :654-658
[48]   Effects of silane coupling agents and solutions of different polarity on PMMA bonding to alumina [J].
Chaijareenont, Pisaisit ;
Takahashi, Hidekazu ;
Nishiyama, Norihiro ;
Arksornnukit, Mansuang .
DENTAL MATERIALS JOURNAL, 2012, 31 (04) :610-616
[49]   The effects of a compatibilizer and a silane coupling agent on the mechanical properties of white rice husk ash filled polypropylene/natural rubber blend [J].
Ismail, H ;
Mega, L .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2001, 40 (04) :463-478
[50]   Effects of Silane Coupling Agent treatment on Properties of PMN/EP Composites [J].
Shi, Minxian ;
Zhang, Ming ;
Huang, Zhixiong ;
Qin, Yan .
MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, PTS 1-3, 2011, 160-162 :359-363