Aging hardening and precipitate behavior of a solution-treated Mg-6Zn-4Sn-1Mn (wt.%) wrought Mg alloy

被引:10
作者
Hou, Caihong [1 ]
Hu, Fan [1 ]
Qi, Fugang [1 ,2 ]
Zhao, Nie [1 ,2 ]
Zhang, Dechuang [1 ]
Ouyang, Xiaoping [1 ]
Zhang, Dingfei [3 ]
机构
[1] Xiangtan Univ, Sch Mat Sci & Engn, Xiangtan 411105, Peoples R China
[2] Xiangtan Univ, Foshan Green Intelligent Mfg Res Inst, Foshan 528311, Peoples R China
[3] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
基金
中国国家自然科学基金;
关键词
Mg-Zn-Sn-Mn alloy; Aging hardening; Precipitate behavior; Precipitation sequence; HETEROGENEOUS NUCLEATION THEORY; MECHANICAL-PROPERTIES; ZN; MICROSTRUCTURE; MAGNESIUM; PHASES;
D O I
10.1016/j.jallcom.2021.161640
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Mg-Zn-Sn-Mn alloy is a new type of age hardening wrought Mg alloy. However, the precipitation behavior of the alloy is still not well understood. A solution-treated Mg-6Zn-4Sn-1Mn alloy is selected as the ex-perimental alloy in this paper. The hardening behavior, precipitate microstructure and precipitation se-quence of the solution-treated alloy during single aging and double aging at 180 degrees C are systematically studied by means of XRD, OM, SEM, TEM, EDS and microhardness. The results show that four types of precipitated phases are successively precipitated in the experimental alloy during the aging treatment, namely, G.P. zone parallel to the (0001)alpha base plane, rod-like 1 (MgZn2) phase perpendicular to the (0001)alpha base plane, disc-like 2 (MgZn2) phase parallel to the (0001)alpha base plane, and irregular beta' (Mg2Sn or Mg3Sn) phase. The habitual plane of most beta' phases is the (0001)alpha basal plane, and a small part of the beta' phase forms a certain angle with the (0001)alpha basal plane. A large number of finely dispersed G.P. zones can provide the heterogeneous nucleation sites for the 1 phase during the pre-aging stage, which promotes the nucleation of the precipitates during the second aging, so the peak aging hardness (87HV) of the double -aged alloy is much higher than that of the single-aged alloy (74HV), and the peak aging time (6 h) during second aging of the double aging is shorter than that (12 h) of single aging. The possible precipitation sequence of Mg-6Zn-4Sn-1Mn alloy during the isothermal aging treatment can be obtained, that is, alpha-Mn -> 1 (MgZn2)->beta (MgZn) in the Mn-rich zone, and SSSS -> G.P. zones -> 1 (MgZn2)-> 2 (MgZn2)->beta' (Mg2Sn or Mg3Sn)->(beta (MgZn) and beta (Mg2Sn)) in Zn-rich and Sn-rich zone. (c) 2021 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] High cycle fatigue behavior of extruded and double-aged Mg-6Zn-1Mn alloy
    Yu, Daliang
    Zhang, Dingfei
    Sun, Jing
    Luo, Yuanxin
    Xu, Junyao
    Zhang, Hongju
    Pan, Fusheng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 662 : 1 - 8
  • [42] Dealloying corrosion of anodic and nanometric Mg41Nd5 in solid solution-treated Mg-3Nd-1Li-0.2Zn alloy
    Gao, Gui-Jia
    Zeng, Mei-Qi
    Zhang, En-Liang
    Zeng, Rong-Chang
    Cui, Lan-Yue
    Xu, Dao-kui
    Wang, Feng-Qin
    Kannan, M. Bobby
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 83 : 161 - 178
  • [43] Effects of substitution of Nd in a sand-cast Mg-2.5Nd-0.6Zn-0.5Zr alloy with x wt.% Sm (x=2.5, 4, and 6)
    Zhang, Deping
    Yang, Qiang
    Zhang, Dongdong
    Guan, Kai
    Bu, Fanqiang
    Zhou, Hong
    Meng, Jian
    JOURNAL OF RARE EARTHS, 2017, 35 (12) : 1261 - 1267
  • [44] Investigation on corrosion behaviors of Mg-Zn-Al-Sn-Mn alloy treated by solution and artificial aging固溶时效处理Mg-Zn-Al-Sn-Mn合金的微观组织演变及腐蚀行为研究
    Jian-wei Tang
    Liang Chen
    Yi-hao Bao
    Zhi-gang Li
    Biao-hua Que
    Journal of Central South University, 2023, 30 : 3197 - 3210
  • [45] Homogenization-induced age-hardening behavior and room temperature mechanical properties of Mg-4Zn-0.5Ca-0.16Mn (wt%) alloy
    Duley, Partha
    Sanyal, Souriddha
    Bandyopadhyay, T. K.
    Mandal, Sumantra
    MATERIALS & DESIGN, 2019, 164
  • [46] High temperature mechanical behaviour of Mg-6Zn-1Y alloy with 1 wt.% calcium addition: Reinforcing effect due to I-(Mg3Zn6Y1) and Mg6Zn3Ca2 phases
    Medina, J.
    Garces, G.
    Perez, P.
    Stark, A.
    Schell, N.
    Adeva, P.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2020, 8 (04) : 1047 - 1060
  • [47] Hot compression deformation behavior of Mg-5Zn-3.5Sn-1Mn-0.5Ca-0.5Cu alloy
    Wang, Cong
    Liu, Yunteng
    Lin, Tao
    Luo, Tianjiao
    Zhao, Yuhong
    Hou, Hua
    Yang, Yuansheng
    MATERIALS CHARACTERIZATION, 2019, 157
  • [48] Tensile creep behavior of a die-cast Mg-6Al-0.2Mn-2Ca-0.3Si (wt.%) alloy
    Sakai, Takahiro
    Nakata, Taiki
    Miyamoto, Takeaki
    Kamado, Shigeharu
    Liao, Jinsun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 774 (774):
  • [49] Nanoscale precipitates with quasicrystal domains enhanced strength-ductility synergy in a Mg-6Zn-4Al-1Sn-0.5Mn alloy
    Shao, X. H.
    Yang, H. J.
    Jin, Q. Q.
    Song, Y. Y.
    Wang, J.
    Zhang, B.
    Ma, X. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 848
  • [50] In vitro corrosion of Mg-6Zn-1Mn-4Sn-1.5Nd/0.5Y alloys
    Zeng, Rong-Chang
    Wang, Lei
    Zhang, Ding-Fei
    Cui, Hong-Zhi
    Han, En-Hou
    FRONTIERS OF MATERIALS SCIENCE, 2014, 8 (03) : 230 - 243