Aging hardening and precipitate behavior of a solution-treated Mg-6Zn-4Sn-1Mn (wt.%) wrought Mg alloy

被引:10
作者
Hou, Caihong [1 ]
Hu, Fan [1 ]
Qi, Fugang [1 ,2 ]
Zhao, Nie [1 ,2 ]
Zhang, Dechuang [1 ]
Ouyang, Xiaoping [1 ]
Zhang, Dingfei [3 ]
机构
[1] Xiangtan Univ, Sch Mat Sci & Engn, Xiangtan 411105, Peoples R China
[2] Xiangtan Univ, Foshan Green Intelligent Mfg Res Inst, Foshan 528311, Peoples R China
[3] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
基金
中国国家自然科学基金;
关键词
Mg-Zn-Sn-Mn alloy; Aging hardening; Precipitate behavior; Precipitation sequence; HETEROGENEOUS NUCLEATION THEORY; MECHANICAL-PROPERTIES; ZN; MICROSTRUCTURE; MAGNESIUM; PHASES;
D O I
10.1016/j.jallcom.2021.161640
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Mg-Zn-Sn-Mn alloy is a new type of age hardening wrought Mg alloy. However, the precipitation behavior of the alloy is still not well understood. A solution-treated Mg-6Zn-4Sn-1Mn alloy is selected as the ex-perimental alloy in this paper. The hardening behavior, precipitate microstructure and precipitation se-quence of the solution-treated alloy during single aging and double aging at 180 degrees C are systematically studied by means of XRD, OM, SEM, TEM, EDS and microhardness. The results show that four types of precipitated phases are successively precipitated in the experimental alloy during the aging treatment, namely, G.P. zone parallel to the (0001)alpha base plane, rod-like 1 (MgZn2) phase perpendicular to the (0001)alpha base plane, disc-like 2 (MgZn2) phase parallel to the (0001)alpha base plane, and irregular beta' (Mg2Sn or Mg3Sn) phase. The habitual plane of most beta' phases is the (0001)alpha basal plane, and a small part of the beta' phase forms a certain angle with the (0001)alpha basal plane. A large number of finely dispersed G.P. zones can provide the heterogeneous nucleation sites for the 1 phase during the pre-aging stage, which promotes the nucleation of the precipitates during the second aging, so the peak aging hardness (87HV) of the double -aged alloy is much higher than that of the single-aged alloy (74HV), and the peak aging time (6 h) during second aging of the double aging is shorter than that (12 h) of single aging. The possible precipitation sequence of Mg-6Zn-4Sn-1Mn alloy during the isothermal aging treatment can be obtained, that is, alpha-Mn -> 1 (MgZn2)->beta (MgZn) in the Mn-rich zone, and SSSS -> G.P. zones -> 1 (MgZn2)-> 2 (MgZn2)->beta' (Mg2Sn or Mg3Sn)->(beta (MgZn) and beta (Mg2Sn)) in Zn-rich and Sn-rich zone. (c) 2021 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Microstructure and Mechanical Properties of Extruded Mg-7Sn-5Zn-xAl (x = 0, 1, 2 and 3 wt.%) Alloy
    Jing Jiang
    Tingqu Li
    Guang-Li Bi
    Feng-Yun Yan
    Chi Cao
    Yuan-Dong Li
    Ying Ma
    Journal of Materials Engineering and Performance, 2019, 28 : 2672 - 2680
  • [32] Microstructure and Mechanical Properties of Extruded Mg-7Sn-5Zn-xAl (x=0, 1, 2 and 3 wt.%) Alloy
    Jiang, Jing
    Li, Tingqu
    Bi, Guang-Li
    Yan, Feng-Yun
    Cao, Chi
    Li, Yuan-Dong
    Ma, Ying
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (05) : 2672 - 2680
  • [33] Microstructure modification and precipitation strengthening for Mg-6Zn-1Mn-4Sn-0.5Ca through extrusion and aging treatment
    Chen, Xia
    Zhang, Ding-fei
    Zhao, Yang
    Feng, Jing-kai
    Jiang, Bin
    Pan, Fu-sheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2020, 30 (10) : 2650 - 2657
  • [34] Effects of different hot extrusion processes on corrosion behavior of Mg-6Gd-1Zn-0.5Zr alloy in 3.5 wt% sodium chloride solution
    Gao, Tianhao
    Xiang, Hongfu
    Cai, Chenglong
    Xiong, Zhaoxiang
    He, Xuancheng
    Guo, Yuhang
    Tang, Wenyu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [35] Precipitate behavior and mechanical properties of enhanced solution treated Al-Zn-Mg-Cu alloy during non-isothermal ageing
    Peng, Xiaoyan
    Li, Yao
    Liang, Xiaopeng
    Guo, Qi
    Xu, Guofu
    Peng, Yongyi
    Yin, Zhimin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 735 : 964 - 974
  • [36] EFFECT OF COOLING RATE ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF SOLUTION-TREATED Mg-9Gd-4Y-2Zn-0.5Zr ALLOY
    Wang, Zixuan
    Jia, Leichen
    Zheng, Jie
    Zhang, Zhimin
    Yu, Jianmin
    Zhao, Xi
    Xue, Yong
    MATERIALI IN TEHNOLOGIJE, 2022, 56 (02): : 201 - 208
  • [37] Development of extruded Mg-6Er-3Y-1.5Zn-0.4Mn(wt.%) alloy with high strength at elevated temperature
    Mingquan Zhang
    Yan Feng
    Jinghuai Zhang
    Shujuan Liu
    Qiang Yang
    Zhuang Liu
    Rongguang Li
    Jian Meng
    Ruizhi Wu
    Journal of Materials Science & Technology, 2019, 35 (10) : 2365 - 2374
  • [38] Effect of Sn Content on the Microstructure, Mechanical Properties and Corrosion Behavior of Biodegradable Mg-x ( 1, 3 and 5 wt.%) Sn-1Zn-0.5Ca Alloys
    Zhao, Zheng-Xue
    Hua, Zhen-Ming
    Li, Da-Wei
    Wei, Dong-Song
    Liu, Yan
    Wang, Jin-Guo
    Luo, Dan
    Wang, Hui-Yuan
    MATERIALS, 2018, 11 (12)
  • [39] Effects of Minor Zr and Sr on As-Cast Microstructure and Mechanical Properties of Mg-4Y-1.2Mn-1Zn (wt.%) Magnesium Alloy
    Yang, Mingbo
    Pan, Fusheng
    Shen, Jia
    Zhou, Tao
    Qin, Caiyuan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (01) : 47 - 54
  • [40] Effects of minor Ca addition on as-cast microstructure and mechanical properties of Mg-4Y-1.2Mn-1Zn (wt.%) magnesium alloy
    Yang, Mingbo
    Duan, Chengyu
    Li, Hongliang
    Guo, Tingzhang
    Zhang, Jia
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 574 : 165 - 173