Mode I interlaminar fracture toughness of carbon-epoxy coupons with embedded ceramic sensors

被引:9
|
作者
Torres, Mauricio [1 ]
Tellez, Ricardo A. [2 ]
Hernandez, Hilario [3 ]
Camps, Thierry [4 ]
机构
[1] Natl Council Sci & Technol CONACYT, Ctr Engn & Ind Dev CIDESI, Queretaro, Mexico
[2] Cranfield Univ, Sch Aerosp, Cranfield, Beds, England
[3] Inst Politecn Nacl, ESIME UP Ticoman, Mexico City, DF, Mexico
[4] Univ Fed Toulouse Midi Pyrenees, LAAS, Toulouse, France
关键词
carbon fibers; delamination; fractography; fracture toughness; COMPOSITE STRUCTURES; MONITORING PATCH; PREDICTION; GROWTH; BEHAVIOR;
D O I
10.1002/adv.21905
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
This study analyses the mechanical and crack growth behavior of woven carbon fiber reinforced plastics (CPRF) with embedded ceramic sensors. The material studied here is 3K-70-P carbon fiber plain weave with EPOLAM 2015 (R) epoxy resin. The composite is manufactured with vacuum bagging procedure. Later on, the composite Mode I interlaminar fracture toughness (G(IC)) is calculated by means of double cantilever beam tests (DCB) for two layout configurations [0/90] and [+/- 45] with and without embedded sensors. Results give an initial approach of the fracture behavior of an instrumented composite facing an interlaminar crack. The interlaminar fracture toughness for the instrumented specimens is lower compared to the noninstrumented coupons. The presence of the sensor and its wire connection has a considerable impact on the damage tolerance of the woven composite, where the sensors surroundings seem to be the more likely region to be affected by an interlaminar fracture.
引用
收藏
页码:2294 / 2302
页数:9
相关论文
共 50 条
  • [1] Loading rate dependency on mode I interlaminar fracture toughness of unidirectional and woven carbon fibre epoxy composites
    Zabala, H.
    Aretxabaleta, L.
    Castillo, G.
    Aurrekoetxea, J.
    COMPOSITE STRUCTURES, 2015, 121 : 75 - 82
  • [2] Mode-II interlaminar fracture toughness of carbon/epoxy laminates
    Saidpour, H
    Barikani, M
    Sezen, M
    IRANIAN POLYMER JOURNAL, 2003, 12 (05) : 389 - 400
  • [3] Mode I fracture characterization of a hybrid cork and carbon-epoxy laminate
    Fernandes, R.
    de Moura, M. F. S. F.
    Silva, F. G. A.
    Dourado, N.
    COMPOSITE STRUCTURES, 2014, 112 : 248 - 253
  • [4] Mode-I interlaminar fracture toughness in unidirectional carbon-fibre/epoxy composites
    Barikani, M
    Saidpour, H
    Sezen, M
    IRANIAN POLYMER JOURNAL, 2002, 11 (06) : 413 - 423
  • [5] CNT-PAN hybrid nanofibrous mat interleaved carbon/epoxy laminates with improved Mode I interlaminar fracture toughness
    Eskizeybek, Volkan
    Yar, Adem
    Avci, Ahmet
    COMPOSITES SCIENCE AND TECHNOLOGY, 2018, 157 : 30 - 39
  • [6] Influence of femtosecond laser treated surfaces on the mode I fracture toughness of carbon-epoxy bonded joints
    Moreira, R. D. F.
    Oliveira, V.
    Silva, F. G. A.
    Vilar, R.
    de Moura, M. F. S. F.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2018, 82 : 108 - 113
  • [7] Mode I interlaminar fracture of carbon/epoxy multidirectional laminates
    Pereira, AB
    de Morais, AB
    COMPOSITES SCIENCE AND TECHNOLOGY, 2004, 64 (13-14) : 2261 - 2270
  • [8] Experimental characterization of the interlaminar fracture toughness of a woven and a unidirectional carbon/epoxy composite
    Fanteria, D.
    Lazzeri, L.
    Panettieri, E.
    Mariani, U.
    Rigamonti, M.
    COMPOSITES SCIENCE AND TECHNOLOGY, 2017, 142 : 20 - 29
  • [9] Dynamic mode II interlaminar fracture toughness of electrically modified carbon/epoxy composites
    Shamchi, Sahand P.
    de Moura, Marcelo F. S. F.
    Zhao, Zhongjie
    Yi, Xiaosu
    Moreira, Pedro M. G. P.
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2022, 159
  • [10] Mode I and mode II interlaminar fracture toughness of CFRP laminates toughened by carbon nanofiber interlayer
    Arai, Masahiro
    Noro, Yukihiro
    Sugimoto, Koh-Ichi
    Endo, Morinobu
    COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (02) : 516 - 525