The effect of precipitation-hardening conditions on wear behaviours at 2024 alurninium wrought alloy

被引:51
作者
Kacar, H [1 ]
Atik, E [1 ]
Meric, C [1 ]
机构
[1] Celal Bayer Univ, Fac Engn, Dept Mech Engn, TR-45140 Manisa, Turkey
关键词
2024 aluminium wrought alloy; abrasive wear; precipitation hardening;
D O I
10.1016/S0924-0136(03)00642-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, wear behaviours of 2024 aluminium wrought alloy were investigated in different tribological conditions based on its ageing conditions. For this purpose, the alloy aged in five different temperatures and periods (at room temperature for I week, at 120 degreesC for 24 h, at 150 degreesC for 18 h, at 160 degreesC for 16 It, at 200 degreesC for 2 h) was worn in pin-on disc model wear test apparatus using different abrasive grit size (5, 11, 18 and 30 mum SiC papers). Furthermore, the effects of different sliding speeds (0.078, 0.156, 0.208 and 0.338 in s(-1)) and loads (6.45, 9, 9.3 and I I N) on wear resistance were also examined. It was measured amounts of mass loss and examined worn surfaces. The mass loss of the specimens increased with load and the abrasive grit size. (C) 2003 Published by Elsevier B.V.
引用
收藏
页码:762 / 766
页数:5
相关论文
共 11 条
[1]   Mechanical properties and wear strengths in aluminium-alumina composites [J].
Atik, E .
MATERIALS AND STRUCTURES, 1998, 31 (210) :418-422
[2]   Precipitation in a heat-treatable aluminum alloy cooled at different rates [J].
Cavazos, JL ;
Colás, R .
MATERIALS CHARACTERIZATION, 2001, 47 (3-4) :175-179
[3]   Effect of hardness on three very different forms of wear [J].
Gore, GJ ;
Gates, JD .
WEAR, 1997, 203 :544-563
[4]   Precipitation and strengthening in aluminium alloys [J].
Lendvai, J .
ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 :43-56
[5]  
Martin P.L., 1984, J MATER SCI, V19, P3835
[6]   An investigation on the elastic modulus and density of vacuum casted aluminum alloy 2024 containing lithium additions [J].
Meric, C .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2000, 9 (03) :266-271
[7]   Physical and mechanical properties of cast under vacuum aluminum alloy 2024 containing lithium additions [J].
Meriç, C .
MATERIALS RESEARCH BULLETIN, 2000, 35 (09) :1479-1494
[8]   Two-body abrasion of a cast Al-Cu (2014 Al) alloy-Al2O3 particle composite:: influence of heat treatment and abrasion test parameters [J].
Modi, OP .
WEAR, 2001, 248 (1-2) :100-111
[9]   A comparison of the reciprocating and continuous two-body abrasive wear behavior of solution-treated and age-hardened 2014 Al alloy [J].
Odabas, D ;
Su, S .
WEAR, 1997, 208 (1-2) :25-35
[10]   THE EFFECT OF THERMAL AGING ON THE ABRASIVE WEAR BEHAVIOR OF AGE-HARDENING 2014-A1/SIC AND 6061-A1/SIC COMPOSITES [J].
SONG, WO ;
KRAUKLIS, P ;
MOURITZ, AP ;
BANDYOPADHYAY, S .
WEAR, 1995, 185 (1-2) :125-130