The influence of process parameters on vertical surface roughness of the AlSi10Mg parts fabricated by selective laser melting

被引:159
作者
Yang, Tao [1 ]
Liu, Tingting [1 ]
Liao, Wenhe [1 ]
MacDonald, Eric [2 ]
Wei, Huiliang [1 ]
Chen, Xiangyuan [1 ]
Jiang, Liyi [1 ]
机构
[1] Nanjing Univ Sci & Technol, Sch Mech Engn, Nanjing 210094, Jiangsu, Peoples R China
[2] Youngstown State Univ, 1 Univ Plaza, Youngstown, OH 44455 USA
关键词
AlSi10Mg alloy; Selective laser melting; Linear energy density; Single deposited tracks; Vertical surface roughness; Surface morphologies; METALLIC COMPONENTS; TENSILE PROPERTIES; MICROSTRUCTURE; BEHAVIOR; FATIGUE;
D O I
10.1016/j.jmatprotec.2018.10.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In recent years, the aluminum alloys parts produced by Selective Laser Melting (SLM) are increasingly used instead of casting aluminum alloys parts in the automotive, aerospace and other fields. However, the high surface roughness of the vertical surfaces is a major issue influencing the application of SLM for aluminum. Moreover, most of the methods to reduce the surface roughness, such as polishing, bead blasting or machining, will increase the production delays and costs. The present study aims at evaluating the effect of linear energy density on the surface roughness of the vertical planes. Both deposited tracks and volumetric specimens were produced and the morphologies and the surface roughnesses were measured. The obtained results indicate that the surface roughness of the vertical planes was reduced to 4 pm from 15 pm when deposited a suitable linear energy density, reducing the surface roughness by more than 70%. The surface morphologies and the height change rate of the deposited tracks had a significant influence on the surface roughness. Furthermore, for experiments with the same linear energy density, the surface roughness was improved with higher laser power.
引用
收藏
页码:26 / 36
页数:11
相关论文
共 27 条
[1]  
Aboulkhair N. T., 2014, Addit. Manuf, V14, P77, DOI [DOI 10.1016/J.ADDMA.2014.08.001, 10.1016/j.addma.2014.08.001]
[2]   Roughness modeling of AlSi10Mg parts fabricated by selective laser melting [J].
Boschetto, Alberto ;
Bottini, Luana ;
Veniali, Francesco .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2017, 241 :154-163
[3]   Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting [J].
Buchbinder, Damien ;
Meiners, Wilhelm ;
Pirch, Norbert ;
Wissenbach, Konrad ;
Schrage, Johannes .
JOURNAL OF LASER APPLICATIONS, 2014, 26 (01)
[4]   THE DEFORMATION AND FRACTURE-BEHAVIOR OF AN AL-SI-MG CASTING ALLOY [J].
CACERES, CH ;
DAVIDSON, CJ ;
GRIFFITHS, JR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 197 (02) :171-179
[5]   Influence of process parameters on surface roughness of aluminum parts produced by DMLS [J].
Calignano, F. ;
Manfredi, D. ;
Ambrosio, E. P. ;
Iuliano, L. ;
Fino, P. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2013, 67 (9-12) :2743-2751
[6]   Experimental investigation on selective laser melting behaviour and processing windows of in situ reacted Al/Fe2O3 powder mixture [J].
Dadbakhsh, S. ;
Hao, L. ;
Jerrard, P. G. E. ;
Zhang, D. Z. .
POWDER TECHNOLOGY, 2012, 231 :112-121
[7]   Additive manufacturing of metallic components - Process, structure and properties [J].
DebRoy, T. ;
Wei, H. L. ;
Zuback, J. S. ;
Mukherjee, T. ;
Elmer, J. W. ;
Milewski, J. O. ;
Beese, A. M. ;
Wilson-Heid, A. ;
De, A. ;
Zhang, W. .
PROGRESS IN MATERIALS SCIENCE, 2018, 92 :112-224
[8]   PRECISE DEPOSITION OF MOLTEN MICRODROPS - THE PHYSICS OF DIGITAL MICROFABRICATION [J].
GAO, FQ ;
SONIN, AA .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1994, 444 (1922) :533-554
[9]   Laser additive manufacturing of metallic components: materials, processes and mechanisms [J].
Gu, D. D. ;
Meiners, W. ;
Wissenbach, K. ;
Poprawe, R. .
INTERNATIONAL MATERIALS REVIEWS, 2012, 57 (03) :133-164
[10]   On the effect of internal channels and surface roughness on the high-cycle fatigue performance of Ti-6Al-4V processed by SLM [J].
Guenther, Johannes ;
Leuders, Stefan ;
Koppa, Peter ;
Troester, Thomas ;
Henkel, Sebastian ;
Biermann, Horst ;
Niendorf, Thomas .
MATERIALS & DESIGN, 2018, 143 :1-11