Effects of small-grit grinding and glazing on mechanical behaviors and ageing resistance of a super-translucent dental zirconia

被引:27
作者
Lai, Xuan [1 ]
Si, Wenjie [2 ]
Jiang, Danyu [3 ]
Sun, Ting [1 ]
Shao, Longquan [1 ]
Deng, Bin [4 ]
机构
[1] Southern Med Univ, Nanfang Hosp, Dept Stomatol, Guangzhou 510515, Guangdong, Peoples R China
[2] Tsinghua Univ, Sch Mat Sci & Engn, Beijing 100084, Peoples R China
[3] Shanghai Inst Ceram, State Key Lab High Performance Ceram & Superfine, Shanghai 200050, Peoples R China
[4] Gen Hosp Chinese PLA, Dept Prosthodont, Beijing 100853, Peoples R China
基金
中国国家自然科学基金;
关键词
Zirconia; Small-grit grinding; Glazing; Mechanical behaviors; Ageing resistance; LOW-TEMPERATURE DEGRADATION; DIFFERENT SURFACE TREATMENTS; Y-TZP CERAMICS; OF-THE-ART; FLEXURAL STRENGTH; PHASE-TRANSFORMATION; STABILIZED ZIRCONIA; HIGHLY-TRANSLUCENT; 3Y-TZP CERAMICS; RESTORATIONS;
D O I
10.1016/j.jdent.2017.09.003
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: The purpose of this study is to elucidate the effects of small-grit grinding on the mechanical behaviors and ageing resistance of a super-translucent dental zirconia and to investigate the necessity of glazing for the small-grit ground zirconia. Methods: Small-grit grinding was performed using two kinds of silicon carbide abrasive papers. The control group received no grinding. The unground surfaces and the ground surfaces were glazed by an experienced dental technician. Finally, the zirconia materials were thermally aged in water at 134 degrees C for 5 h. After aforementioned treatments, we observed the surface topography and the microstructures, and measured the extent of monoclinic phase, the nano-hardness and nano-modulus of the possible transformed zone and the flexural strength. Results: Small-grit grinding changed the surface topography. The zirconia microstructure did not change obviously after surface treatments and thermal ageing; however, the glaze in contact with zirconia showed cracks after thermal ageing. Small-grit grinding did not induce a phase transformation but improved the flexural strength and ageing resistance. Glazing prevented zirconia from thermal ageing but severely diminished the flexural strength. The nano-hardness and nano-modulus of the surface layer were increased by ultrafine grinding. Conclusions: The results suggest that small-grit grinding is beneficial to the strength and ageing resistance of the super-translucent dental zirconia; however, glazing is not necessary and even impairs the strength for the supertranslucent dental zirconia. Clinical significance: This study is helpful to the researches about dental grinding tools and maybe useful for dentists to choose reasonable zirconia surface treatments.
引用
收藏
页码:23 / 31
页数:9
相关论文
共 50 条
[1]   EFFECT OF SURFACE TREATMENT ON FLEXURAL STRENGTH OF ZIRCONIA BARS [J].
Aboushelib, Moustafa N. ;
Wang, Hang .
JOURNAL OF PROSTHETIC DENTISTRY, 2010, 104 (02) :98-104
[2]   Fatigue behavior of Y-TZP ceramic after surface treatments [J].
Amaral, Marina ;
Cesar, Paulo Francisco ;
Bottino, Marco Antonio ;
Lohbauer, Ulrich ;
Valandro, Luiz Felipe .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 57 :149-156
[3]   Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis [J].
Aurelio, Iana L. ;
Marchionatti, Ana Maria E. ;
Montagner, Anelise F. ;
May, Liliana G. ;
Soares, Fabio Z. M. .
DENTAL MATERIALS, 2016, 32 (06) :827-845
[4]  
Basilio MD, 2016, J PROSTHET DENT, V116, P277, DOI 10.1016/j.prosdent.2016.01.011
[5]   Grinding damage assessment on four high-strength ceramics [J].
Canneto, Jean-Jacques ;
Cattani-Lorente, Maria ;
Durual, Stephane ;
Wiskott, Anselm H. W. ;
Scherrer, Susanne S. .
DENTAL MATERIALS, 2016, 32 (02) :171-182
[6]   Effect of different surface treatments on the hydrothermal degradation of a 3Y-TZP ceramic for dental implants [J].
Cattani-Lorente, M. ;
Scherrer, S. S. ;
Durual, S. ;
Sanon, C. ;
Douillard, T. ;
Gremillard, L. ;
Chevalier, J. ;
Wiskott, A. .
DENTAL MATERIALS, 2014, 30 (10) :1136-1146
[7]   Low temperature degradation of a Y-TZP dental ceramic [J].
Cattani-Lorente, Maria ;
Scherrer, Susanne S. ;
Ammann, Patrick ;
Jobin, Marc ;
Wiskott, H. W. Anselm .
ACTA BIOMATERIALIA, 2011, 7 (02) :858-865
[8]   Five-year clinical outcome of posterior zirconia ceramic inlay-retained FDPs with a modified design [J].
Chaar, M. Sad ;
Kern, Matthias .
JOURNAL OF DENTISTRY, 2015, 43 (12) :1411-1415
[9]   Low-temperature degradation of Zirconia and implications for biomedical implants [J].
Chevalier, Jerome ;
Gremillard, Laurent ;
Deville, Sylvain .
ANNUAL REVIEW OF MATERIALS RESEARCH, 2007, 37 (1-32) :1-32
[10]   The Tetragonal-Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends [J].
Chevalier, Jerome ;
Gremillard, Laurent ;
Virkar, Anil V. ;
Clarke, David R. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2009, 92 (09) :1901-1920