Study on the Grooved Morphology of CMC-SiCf/SiC by Dual-Beam Coupling Nanosecond Laser

被引:4
作者
Chen, Tao [1 ,2 ]
Chen, Xiaoxiao [2 ,3 ]
Zhang, Xuanhua [1 ,2 ]
Zhang, Huihui [2 ,4 ]
Zhang, Wenwu [2 ,3 ]
Liu, Ganhua [1 ]
机构
[1] Jiangxi Univ Sci & Technol, Sch Mech & Elect Engn, Ganzhou 341000, Peoples R China
[2] Chinese Acad Sci, Ningbo Inst Mat Technol & Engn, Zhejiang Prov Key Lab Aero Engine Extreme Mfg Tec, Ningbo 315201, Peoples R China
[3] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
[4] Ningbo Univ, Sch Mech Engn & Mech, Ningbo 315211, Peoples R China
关键词
ceramic matrix composite; dual-beam coupling; nanosecond laser; grooved morphology; high-temperature oxidation; THERMAL-CONDUCTIVITY; COMPOSITES; BEHAVIOR; ENERGY;
D O I
10.3390/ma15196630
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Due to the excellent properties of high hardness, oxidation resistance, and high-temperature resistance, silicon carbide fiber reinforced silicon carbide ceramic matrix composite (CMC-SiCf/SiC) is a typical difficult-to-process material. In this paper, according to the relationship between the spatial posture of dual beams and the direction of the machining path, two kinds of scanning methods were set up. The CMC-SiCf/SiC grooving experiments were carried out along different feeding directions (transverse scanning and longitudinal scanning) by using a novel dual-beam coupling nanosecond laser, and the characteristics of grooving morphology were observed by Laser Confocal Microscope, Scanning Electron Microscopy (SEM), and Energy Dispersive Spectrometer (EDS). The results show that the transverse scanning grooving section morphology is V shape, and the longitudinal scanning groove section morphology is W shape. The grooving surface depth and width of transverse scanning are larger and smaller than that of longitudinal scanning when the laser parameters are the same. The depth of the transverse grooving is greater than that of the longitudinal grooving when the laser beam is transverse and longitudinal scanning, the maximum grooving depth is approximately 145.39 mu m when the laser energy density is 76.73 J/cm(2), and the minimum grooving depth is approximately 83.76 mu m when the laser energy density is about 29.59 J/cm(2). The thermal conductivity of fiber has a significant effect on the local characteristics of the grooved morphology when using a medium energy density grooving. The obvious recasting layer is produced after the laser is applied to CMC-SiCf/SiC when using a high energy density laser grooving, which directly affects the grooved morphology.
引用
收藏
页数:17
相关论文
共 29 条
[1]   Oxidation behaviour of SiC/SiC ceramic matrix composites in air [J].
Al Nasiri, Nasrin ;
Patra, Niranjan ;
Ni, Na ;
Jayaseelan, Daniel D. ;
Lee, William E. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (14) :3293-3302
[2]   Research on the ablation mechanism and ablation threshold of CMC-SiCf/SiC by using dual-beam coupling nanosecond laser [J].
Chen, Tao ;
Chen, Xiaoxiao ;
Liu, Ganhua ;
Zhang, Xuanhua ;
Zhang, Wenwu .
CERAMICS INTERNATIONAL, 2022, 48 (17) :24822-24839
[3]  
Chen X., 2021, PROC SPIE, V11907
[4]   The new challenges of machining Ceramic Matrix Composites (CMCs): Review of surface integrity [J].
Diaz, Oriol Gavalda ;
Luna, Gonzalo Garcia ;
Liao, Zhirong ;
Axinte, Dragos .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2019, 139 :24-36
[5]   Ultra-high temperature ablation behaviour of 2.5D SiC/SiC under an oxy-acetylene torch [J].
Du, Jinkang ;
Yu, Guoqiang ;
Jia, Yunfa ;
Ni, Zheng ;
Gao, Xiguang ;
Song, Yingdong ;
Wang, Fang .
CORROSION SCIENCE, 2022, 201
[6]   Investigations on the thermal effect caused by laser cutting with respect to static strength of CFRP [J].
Herzog, Dirk ;
Jaeschke, Peter ;
Meier, Oliver ;
Haferkamp, Heinz .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2008, 48 (12-13) :1464-1473
[7]  
Jiang W., 2019, INFRARED LASER ENG, V49, P300
[8]  
Jiao HW, 2021, INT J ADV MANUF TECH, V112, P3017, DOI 10.1007/s00170-020-06499-w
[9]  
Lawal S. S., 2019, Journal of Physics: Conference Series, V1378, DOI 10.1088/1742-6596/1378/3/032103
[10]   Fatigue Damage and Lifetime of SiC/SiC Ceramic-Matrix Composite under Cyclic Loading at Elevated Temperatures [J].
Li, Longbiao .
MATERIALS, 2017, 10 (04)