Development of hydrolysed protein-based plywood adhesive from slaughterhouse waste: effect of chemical modification of hydrolysed protein on moisture resistance of formulated adhesives

被引:15
作者
Adhikari, Birendra B. [1 ]
Kislitsin, Vadim [2 ]
Appadu, Pooran [1 ]
Chae, Michael [1 ]
Choi, Phillip [2 ]
Bressler, David C. [1 ]
机构
[1] Univ Alberta, Fac Agr Life & Environm Sci, Dept Agr Food & Nutr Sci, Edmonton, AB T6G 2P5, Canada
[2] Univ Alberta, Fac Engn, Dept Chem & Mat Engn, Edmonton, AB T6G 1H9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
SOY PROTEIN; WOOD; STRENGTH; PERFORMANCE; COMPOSITES; BIOMASS;
D O I
10.1039/c7ra09952e
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Specified risk materials (SRM) constitute the proteinaceous waste of slaughterhouses and are currently being disposed off either by incineration or by land filling. Over the last few years, our efforts have focused on developing technology platforms for deployment of this renewable resource for various value-added industrial applications. This report describes a technology for utilization of SRM for the development of an environmentally friendly plywood adhesive with an improved water resistance property. The feedstock (SRM) was first thermally hydrolysed according to a standard protocol, and the hydrolysed protein fragments (peptides) were recovered from the hydrolysate. The recovered peptides were chemically modified through esterification reaction using ethanol, and then chemically crosslinked with polyamideamine-epichlorohydrin (PAE) resin to develop a wood adhesive system. Plywood specimens were then developed using the peptides-PAE resin-based adhesive. The effects of crosslinking time, solid content of the adhesive formulation, ratio of peptides and crosslinking agent in the formulation, and curing conditions of specimen preparation on lap shear strength of resulting plywood specimens were systematically evaluated. Despite the hydrophilic nature of hydrolysed protein fragments, the peptides-PAE resin formulations exhibited remarkable water resistance property after curing. Capping of polar carboxyl groups of peptides by converting them to esters further improved the water resistance property of this adhesive system. Under the optimum conditions of adhesive preparation and curing, the ethyl ester derivative of peptides and PAE resin-based formulations resulted in plywood specimens having comparable dry as well as soaked shear strengths to those of commercial phenol formaldehyde resin.
引用
收藏
页码:2996 / 3008
页数:13
相关论文
共 42 条
[1]  
Adhikari BB, 2017, Bio-based Wood adhesives, P1
[2]   Enhancing the Adhesive Strength of a Plywood Adhesive Developed from Hydrolyzed Specified Risk Materials [J].
Adhikari, Birendra B. ;
Appadu, Pooran ;
Kislitsin, Vadim ;
Chae, Michael ;
Choi, Phillip ;
Bressler, David C. .
POLYMERS, 2016, 8 (08)
[3]   Structure and Physical Properties of Starch/Poly Vinyl Alcohol/Sodium Montmorillonite Nanocomposite Films [J].
Ali, Samer S. ;
Tang, Xiaozhi ;
Alavi, Sajid ;
Faubion, Jon .
JOURNAL OF AGRICULTURAL AND FOOD CHEMISTRY, 2011, 59 (23) :12384-12395
[4]  
[Anonymous], EC ENV ASS EL SPEC R
[5]  
[Anonymous], 1995, COMP AIR POLL EM FAC, pAP
[6]  
ASTM International, 2012, STAND SPEC UR FORM R
[7]   Effects of wood-surface roughness, adhesive viscosity and processing pressure on adhesion strength of protein adhesive [J].
Cheng, Enzhi ;
Sun, Xiuzhi .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2006, 20 (09) :997-1017
[8]  
ESPY HH, 1995, TAPPI J, V78, P90
[9]  
FRAENKEICONRAT H, 1945, J BIOL CHEM, V161, P259
[10]   Treatment alternatives of slaughterhouse wastes, and their effect on the inactivation of different pathogens: A review [J].
Franke-Whittle, Ingrid H. ;
Insam, Heribert .
CRITICAL REVIEWS IN MICROBIOLOGY, 2013, 39 (02) :139-151