Sub-surface oxidation at the aluminum-sapphire interface during low-temperature annealing

被引:8
作者
Dutta, Sreya [1 ]
Chan, Helen M. [1 ]
Vinci, Richard P. [1 ]
机构
[1] Lehigh Univ, Dept Mat Sci & Engn, Ctr Adv Mat & Nanotechnol, Bethlehem, PA 18015 USA
关键词
D O I
10.1111/j.1551-2916.2007.01714.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A study of the solid-state oxidation of evaporated aluminum (Al) films on c-plane sapphire was undertaken. The thickness of the films ranged from 100 to 1000 nm, and the samples were subjected to isothermal annealing in air, at temperatures from 350 degrees to 650 degrees C. For heat-treated samples, the removal of remnant metallic Al using a 45% KOH etch revealed the formation of novel, sub-surface oxidation features at the Al-sapphire interface. These features were associated with the hillocking of the Al film, and consisted of hollow, truncated pyramidal structures. Low ridge-like walls were observed around the periphery of the bases of these structures. The ridges exhibited a crystallographic relationship with the sapphire substrate; a corresponding relationship with the overlying Al film, due to its highly textured nature, was inferred. Transmission electron microscopy of sections through the ridges revealed that they consisted of alumina. It is believed that during heat treatment, voids develop in the Al in order to relieve the strain energy due to compressive stresses, and that faceting of the voids subsequently takes place due to surface energy considerations. The walls of the pyramidal structures are thought to have formed by the oxidation of the surfaces of the mentioned facetted voids.
引用
收藏
页码:2571 / 2575
页数:5
相关论文
共 31 条
  • [11] Analysis of local strain in aluminium interconnects by energy filtered CBED
    Krämer, S
    Mayer, J
    Witt, C
    Weickenmeier, A
    Rühle, M
    [J]. ULTRAMICROSCOPY, 2000, 81 (3-4) : 245 - 262
  • [12] STRESS RELIEF AND HILLOCK FORMATION IN THIN LEAD FILMS
    LAHIRI, SK
    [J]. JOURNAL OF APPLIED PHYSICS, 1970, 41 (07) : 3172 - &
  • [13] The influence of interfacial wetting and adhesion on the formation of voids at metal-ceramic interfaces
    Levi, G
    Kaplan, WD
    [J]. JOURNAL OF MATERIALS SCIENCE, 2006, 41 (03) : 817 - 821
  • [14] Aluminium-alumina interface morphology and thermodynamics from dewetting experiments
    Levi, G
    Kaplan, WD
    [J]. ACTA MATERIALIA, 2003, 51 (10) : 2793 - 2802
  • [15] Levin I, 1998, J AM CERAM SOC, V81, P1995, DOI 10.1111/j.1151-2916.1998.tb02581.x
  • [16] Comparative studies on oxygen diffusion coefficients for amorphous and γ-Al2O3 films using 18O isotope
    Nabatame, T
    Yasuda, T
    Nishizawa, M
    Ikeda, M
    Horikawa, T
    Toriumi, A
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2003, 42 (12): : 7205 - 7208
  • [17] InGaN-based laser diodes
    Nakamura, S
    [J]. ANNUAL REVIEW OF MATERIALS SCIENCE, 1998, 28 : 125 - 152
  • [18] Nakamura S., 2000, INTRO NITRIDE SEMICO
  • [19] Group III nitride semiconductors for short wavelength light-emitting devices
    Orton, JW
    Foxon, CT
    [J]. REPORTS ON PROGRESS IN PHYSICS, 1998, 61 (01) : 1 - +
  • [20] Patterning of sapphire substrates via a solid state conversion process
    Park, H
    Chan, HM
    Vinci, RP
    [J]. JOURNAL OF MATERIALS RESEARCH, 2005, 20 (02) : 417 - 423