Experimental study on characteristics of laser metal deposited Al-Si-Sn-Cu/Ti-6Al-4V composite coatings

被引:10
|
作者
Obiegbu, M. C. [1 ]
Fatoba, O. S. [1 ]
Akinlabi, E. T. [1 ,3 ]
Akinlabi, S. A. [2 ]
机构
[1] Univ Johannesburg, Dept Mech Engn Sci, Johannesburg, South Africa
[2] Univ Johannesburg, Dept Mech & Ind Engn Technol, Johannesburg, South Africa
[3] Covenant Univ, Dept Mech Engn, Ota, Ogun State, Nigeria
来源
MATERIALS RESEARCH EXPRESS | 2019年 / 6卷 / 04期
基金
新加坡国家研究基金会;
关键词
Ti-6Al-4V alloy; hardness; coefficient of friction; microstructure; Al-Si-Sn-Cu coating; laser metal deposition; characterization; AL-SN COATINGS; MECHANICAL-PROPERTIES; CORROSION BEHAVIOR; SURFACE-ANALYSES; HARDNESS VALUES; TITANIUM-ALLOYS; TI COATINGS; MICROSTRUCTURE; POROSITY; SPEED;
D O I
10.1088/2053-1591/aafe4d
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The development of laser based advanced coatings are continually implemented in order to meet the desired demands and performances of materials in industries. Many engineering materials used in industrial conditions are subjected to corrosion, wear and fatigue attack leading to rapid degradation of the material. This research is aimed at fabricating Al-Si-Sn-Cu quaternary coatings on Ti-6Al-4V alloy. A 3-kW continuous wave ytterbium laser system (YLS) attached to a KUKA robot which controls the movement of the cladding process was used for the laser cladding process. The appropriate selection of laser processing parameter produced desirable result and properties. Enhanced surface hardness and tribological properties were achieved as a result of well optimized laser process parameters and appropriate selection of reinforced powders. The results of the microhardness revealed an improvement as the hardness measured for the cladded Al-Si-Sn-Cu layer was 602 HV0.1. While the micro-hardness of the Ti-6Al-4V substrate was 302 HV0.1. Also, the COF of Al- Si-Sn-Cu quaternary coatings are lower than that of the Ti-6Al-4V substrate, which was attributed to strengthening effect and higher load bearing aptitude of Ti3Al, CuTi2, AlSi3Ti2, SiTi, AlTi0.6V0.4, and Al0.25Sn0.75V3 hard phases present in the coatings. The protective intermetallic phases result to a reduction in coefficient of friction and therefore demonstrated superior wear resistance performance.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Biomimetic Coatings on Fiber Laser Modified Ti-6Al-4V Surfaces
    Hong, T. F.
    Fu, L. M.
    Wu, B. S.
    Lin, K. Y.
    Lin, H. K.
    Kuo, T. Y.
    JOURNAL OF LASER MICRO NANOENGINEERING, 2016, 11 (02): : 147 - 152
  • [32] Microstructure, composition and hardness of laser-assisted hydroxyapatite and Ti-6Al-4V composite coatings
    Mansur, Muhammad Rakib
    Wang, James
    Berndt, Christopher C.
    SURFACE & COATINGS TECHNOLOGY, 2013, 232 : 482 - 488
  • [33] Elimination of defects in laser metal deposited TiCp/Ti6Al4V composite by synchronous ultrasonic impact treatment
    Xu, De
    Wang, Jiandong
    Wang, Zhen
    Sun, Qianfei
    Guo, Chunhuan
    Jiang, Fengchun
    Tong, Yunxiang
    MATERIALS LETTERS, 2023, 347
  • [34] Laser Metal Deposition of Ti6Al4V-A Brief Review
    Zhong, Chongliang
    Liu, Jianing
    Zhao, Tong
    Schopphoven, Thomas
    Fu, Jinbao
    Gasser, Andres
    Schleifenbaum, Johannes Henrich
    APPLIED SCIENCES-BASEL, 2020, 10 (03):
  • [35] Determination of α to β phase transformation kinetics in laser-powder bed fused Ti-6Al-2Sn-4Zr-2Mo-0.08Si and Ti-6Al-4V alloys
    Kaushik, Harish Chandra
    Korayem, Mahdi Habibnejad
    Hadadzadeh, Amir
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 860
  • [36] Effect of Bonding Temperature on the Joining of Ti-6Al-4V Alloy Using Cu Coatings and Sn Interlayers
    AlHazaa, Abdulaziz N.
    AlGharbi, Sultan H.
    Nishikawa, Hiroshi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (01) : 407 - 417
  • [37] Effect of Elevated Temperatures on the Mechanical Properties of a Direct Laser Deposited Ti-6Al-4V
    Ivanov, Sergei
    Gushchina, Marina
    Artinov, Antoni
    Khomutov, Maxim
    Zemlyakov, Evgenii
    MATERIALS, 2021, 14 (21)
  • [38] Microstructure and Properties of Ti-6Al-4V Titanium Alloy by Laser Deposited with Ultrasonic Vibration
    Li C.
    Du J.
    Qin L.
    Yang G.
    Wang W.
    Xiyou Jinshu/Chinese Journal of Rare Metals, 2024, 48 (05): : 632 - 639
  • [39] Study on Wear Resistance of Ti-6Al-4V Alloy Composite Coating Prepared by Laser Alloying
    Chen, Quan
    Zhang, Jiajia
    Huang, Anguo
    Wei, Pengyu
    APPLIED SCIENCES-BASEL, 2021, 11 (01): : 1 - 17
  • [40] Electron backscatter diffraction characterization of fatigue crack growth in laser metal wire deposited Ti-6Al-4V
    Akerfeldt, Pia
    Colliander, Magnus Hornqvist
    Pederson, Robert
    Antti, Marta-Lena
    MATERIALS CHARACTERIZATION, 2018, 135 : 245 - 256