Friction and Wear Properties of Ni3Si Alloy with Ti Addition at High Temperatures

被引:2
|
作者
Wu, Changyin [1 ]
Niu, Muye [1 ,2 ]
Bao, Shuai [1 ]
Sun, Yuhang [1 ]
Zhang, Xinghua [1 ,2 ]
机构
[1] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
[2] Jiangsu Univ Sci & Technol, Natl Demonstrat Ctr Expt Mat Sci & Engn Educ, Zhenjiang 212003, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
tribological properties; Ni3Si alloy; wear mechanisms; high temperatures; SLIDING WEAR; TRIBOLOGICAL PROPERTIES; NI-17.5SI-29.3CR ALLOY; CORROSION BEHAVIOR; MICROSTRUCTURE; OXIDATION; CR; NI-3(SI; TI); RESISTANCE; GLASSES;
D O I
10.3390/ma13040982
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The tribological properties of Ni3Si alloy were studied at high temperatures. The effect of the addition of Ti was also analyzed. The surface composition was analyzed by Raman spectroscopy. The results showed that the friction coefficient decreased with the increasing temperature, and the wear rate changed slightly from 25 to 400 degrees C. However, the wear resistance of the alloys decreased sharply at 600 degrees C, and this was due to the decrease of the high-temperature strength and the severe oxidation of the alloys. Although the oxidation resistance of Ni3Si alloy decreased with Ti addition, the tribological property was improved by the addition of Ti. The Ni3Si alloy with 5% Ti addition had the best wear resistance at high temperatures as compared to pure Ni3Si alloy and with 10% Ti addition, and the wear rates of the alloys were in the order of magnitude of 10(-5) mm(3)/Nm. With the increase of temperature, the wear mechanism of pure Ni3Si alloy transformed from abrasive wear to oxidation wear. As the Ti content increased, the wear mechanisms of the alloys changed from abrasive wear to fatigue wear at low temperature, and oxidation wear and fatigue wear at high temperature.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Friction and wear properties of Ni3Si alloy under different vacuum conditions
    Niu, Muye
    Zhang, Xinghua
    Chen, Jiajun
    Yang, Xiaoyuan
    VACUUM, 2019, 161 : 443 - 449
  • [2] STRENGTHENING AND DUCTILIZATION OF NI3SI BY THE ADDITION OF TI ELEMENTS
    TAKASUGI, T
    NAGASHIMA, M
    IZUMI, O
    ACTA METALLURGICA ET MATERIALIA, 1990, 38 (05): : 747 - 755
  • [3] Effect of ti addition on microstructural evolution of Ni3Si
    Yu, Qing
    Sun, Yaoning
    Sun, Wenlei
    Key Engineering Materials, 2012, 522 : 123 - 126
  • [4] Mechanical and chemical properties of Ni3Si and Ni3(Si,Ti) alloys multiphased by chromium addition
    Takasugi, T
    Kawai, H
    Kaneno, Y
    MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (06) : 671 - 680
  • [5] Microstructure and room temperature mechanical properties of Ni3Si based alloy with titanium addition
    Wang, S. K.
    Fu, C. C.
    Cai, Z. W.
    Jian, S. R.
    Jang, J. S. C.
    Zhang, H. Z.
    Hsu, H. C.
    MATERIALS TECHNOLOGY, 2012, 27 (01) : 139 - 141
  • [6] Intermetallic alloys Ni3Si and Ni3(Si,Ti):: Microstructures and properties
    Fan, Ding
    Sun, Yao-Ning
    Zheng, Min
    Zhang, Jian-bin
    Zheng, Yu-Feng
    HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 : 1143 - 1145
  • [7] Growth morphology of Ni3Si in high undercooled Ni-Si eutectic alloy
    惠增哲
    杨根仓
    周尧和
    Progress in Natural Science, 1997, (05) : 114 - 121
  • [8] Growth morphology of Ni3Si in high undercooled Ni-Si eutectic alloy
    Xi, Zengzhe
    Yang, Gencang
    Zhou, Yaohe
    Progress in Natural Science, 1997, 7 (05): : 630 - 631
  • [9] Growth morphology of Ni3Si in high undercooked Ni-Si eutectic alloy
    Xi, ZZ
    Yang, GC
    Zhou, YH
    PROGRESS IN NATURAL SCIENCE, 1997, 7 (05) : 624 - 631
  • [10] The effect of Cr addition on mechanical and chemical properties of Ni3Si alloys
    Takasugi, T
    Kawai, H
    Kaneno, Y
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 329 : 446 - 454