Oxide growth mechanism and oxidation resistance in mechanically alloyed Ni-20Cr-20Fe-5Nb-1Y2O3 alloy

被引:1
|
作者
Kim, IH [1 ]
Kwun, SI [1 ]
机构
[1] Korea Univ, Div Engn & Mat Sci, Seoul 136701, South Korea
关键词
ultra-fine grain; oxidation; ODS alloy; mechanical alloying;
D O I
10.4028/www.scientific.net/MSF.475-479.4231
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The oxidation characteristics of a Ni-20Cr-20Fe-5Nb-IY2O3 alloy and a Ni-20Cr-20Fe-5Nb alloy both with ultra-fine grains were compared with those of commercial Inconel 718 and PM 1000 alloys. The oxidation resistance of the Ni-20Cr-20Fe-5Nb-1Y(2)O(3) alloy was superior to that of both the Ni-20Cr-2OFe-5Nb and commercial Inconel 718 alloys. This was attributed to the suppression of successive oxidation via the oxide formed during the oxidation of the ODS (oxide dispersion strengthening) alloy. It was confirmed that the prior powder boundary is the site where the oxide grows continuously during ODS alloy oxidation.
引用
收藏
页码:4231 / 4234
页数:4
相关论文
共 50 条
  • [1] Mechanical properties of nano grained Ni20Cr20Fe5Nb1Y2O3 composite and Ni20Cr20Fe5Nb2Al alloy
    Kim, IH
    Kim, YH
    Kim, CS
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 250 - 256
  • [2] Increased high temperature oxidation resistance of Ni20Cr20Fe5Nb1Y2O3alloy with nano-sized grains
    Kim, IH
    Kwun, SI
    ECO-MATERIALS PROCESSING & DESIGN VI, 2005, 486-487 : 109 - 112
  • [3] Formation of Ni3Nb and influence of Y2O3 on mechanical properties of nano-grained Ni20Cr20Fe5Nb1Y2O3 alloy
    Kim, IH
    Kim, YH
    FRACTURE AND STRENGTH OF SOLIDS VI, PTS 1 AND 2, 2006, 306-308 : 929 - 933
  • [4] OXIDATION AND SULFIDATION BEHAVIOR OF FE-20CR-16NI-4AL-1Y2O3 OXIDE-DISPERSION-STRENGTHENED ALLOY
    MALIK, AU
    NATESAN, K
    OXIDATION OF METALS, 1990, 34 (5-6): : 497 - 528
  • [5] The Oxide Scale Growth Mechanism on Fe20Cr5Al+RE Alloy in SO2+O2
    Jedlinski, J.
    Zurek, Z.
    Homa, M.
    Smola, G.
    Camra, J.
    DIFFUSION IN MATERIALS - DIMAT2008, 2009, 289-292 : 541 - +
  • [6] Oxidation behaviour of micro-crystalline Ni-20Cr-Y2O3ODS alloy coatings
    He, Y
    Huang, Z
    Qi, H
    Wang, D
    Li, Z
    Gao, W
    MATERIALS LETTERS, 2000, 45 (02) : 79 - 85
  • [8] Oxidation behaviour of Ni-20Cr-Y2O3 ODS microcrystalline coatings
    Pang, H.
    Qi, H.
    He, Y.
    Wang, D.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2001, 11 (02): : 187 - 192
  • [9] Effect of Y2O3 contents on oxidation resistance at 1150 °C and mechanical properties at room temperature of ODS Ni-20Cr-5Al alloy
    Sun, Duanjun
    Liang, Chunyuan
    Shang, Jinlong
    Yin, Jihui
    Song, Yaru
    Li, Weizhou
    Liang, Tianquan
    Zhang, Xiuhai
    APPLIED SURFACE SCIENCE, 2016, 385 : 587 - 596
  • [10] Oxidation of a quaternary three-phase Cu-20Ni-20Cr-5Fe alloy at 700-900°C in 1 atm of pure O2
    Cao, Z. Q.
    Shen, Y.
    Wang, C. J.
    Liu, W. H.
    CORROSION SCIENCE, 2007, 49 (06) : 2450 - 2460