摘要
The fracture toughness of the electroless nickel phosphorus coatings have been measured using a notched tensile specimen made of the film, which was stripped along the interface between outer and inner layers of the coatings. The results showed that the average fracture toughness of as-deposited NiP amorphous coatings was K-IC=7.1 MPa m(1/2) and decreased with increasing heat treatment temperature. For example, K-IC = 5.2 MPa m(1/2) for a 300 degrees C treatment, K-IC=3.7 MPa m(1/2) for a 330 degrees C treatment and K-IC= 1.2 MPa m(1/2) for a 400 degrees C treatment corresponding to complete crystallization. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:349 / 351
页数:3
相关论文
共 50 条
  • [1] Indentation tests to determine the fracture toughness of nickel phosphorus coatings
    Roman, A
    Chicot, D
    Lesage, J
    SURFACE & COATINGS TECHNOLOGY, 2002, 155 (2-3) : 161 - 168
  • [2] Modeling of Fracture Toughness of Electroless Nickel (EN) Coatings
    K. Zangeneh
    S.M. Monir-vaghefi
    F. Ashrafizadeh
    材料热处理学报, 2004, (05) : 1088 - 1091
  • [3] Modeling of fracture toughness of electroless nickel (EN) coatings
    Zangeneh, K
    Monir-vaghefi, SM
    Ashrafizadeh, F
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 AND 2, PROCEEDINGS, 2004, : 1088 - 1091
  • [4] Fractography and Fracture Toughness Measurement
    Morrell, Roger
    FRACTOGRAPHY OF ADVANCED CERAMICS III, 2009, 409 : 17 - 27
  • [5] Fracture toughness measurement on TiN hard coatings using internal energy induced cracking
    Wang, An-Ni
    Yu, Ge-Ping
    Huang, Jia-Hong
    SURFACE & COATINGS TECHNOLOGY, 2014, 239 : 20 - 27
  • [6] Nanoscratching deformation and fracture toughness of electroless Ni-P coatings
    Shen, Y. F.
    Xue, W. Y.
    Liu, Z. Y.
    Zuo, L.
    SURFACE & COATINGS TECHNOLOGY, 2010, 205 (02) : 632 - 640
  • [7] Relationship between fracture toughness and temperature in epoxy coatings
    Zhao Bo
    Li Jing-wei
    Li Shu-guang
    Lu Yi-hui
    Hao Ju-tao
    POLIMERY, 2015, 60 (04) : 258 - 263
  • [8] Superlattice effect for enhanced fracture toughness of hard coatings
    Hahn, R.
    Bartosik, M.
    Soler, R.
    Kirchlechner, C.
    Dehm, G.
    Mayrhofer, P. H.
    SCRIPTA MATERIALIA, 2016, 124 : 67 - 70
  • [9] THE ANALYSIS OF DIFFERENT FRACTURE TOUGHNESS MODELS FOR PVD COATINGS
    Sowa, Sylwia
    Smolik, Jerzy
    Kacprzynska-Golacka, Joanna
    Piasek, Artur
    31ST INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, METAL 2022, 2022, : 555 - 560
  • [10] Fracture toughness of nanoscale hydroxapatite coatings on titanium substrates
    Roest, R
    Heness, G
    Latella, B
    Ben-Nissan, B
    FRACTURE AND STRENGTH OF SOLIDS VI, PTS 1 AND 2, 2006, 306-308 : 1307 - 1312