Deformation and fracture behavior of an Al2O3/YAG composite from room temperature to 2023 K

被引:92
作者
Ochiai, S [1 ]
Ueda, T
Sato, K
Hojo, M
Waku, Y
Nakagawa, N
Sakata, S
Mitani, A
Takahashi, T
机构
[1] Kyoto Univ, Grad Sch Engn, Mesoscop Mat Res Ctr, Sakyo Ku, Kyoto 6068501, Japan
[2] JUTEMI, Ube, Yamaguchi 7550001, Japan
[3] UBE Ind Ltd, Corp Res & Dev, Ube Res Lab, Ube, Yamaguchi 7558633, Japan
关键词
fracture toughness; strength; deformation; Al2O3/YAG composite; ultra high temperature;
D O I
10.1016/S0266-3538(01)00159-2
中图分类号
TB33 [复合材料];
学科分类号
摘要
The deformation and fracture behavior of a newly developed Al2O3/YAG composite, fabricated by the unidirectional solidification of a eutectic composition, was investigated by means of bending tests between room temperature and 2023 K, on specimens whose longitudinal directions were parallel (L specimen) and perpendicular (T specimen) to the direction of solidification. At low temperatures, the composite fractured in a brittle manner at all displacement speeds. At high temperatures, it fractured in a brittle manner at high displacement speed, but in a ductile manner with accompanying plastic deformation at low speed for both L and T specimens. The brittle-ductile transition temperature became higher at higher displacement speeds in both L and T specimens, while it was slightly higher in the latter specimen. The crack propagated dominantly through YAG with lower ductility than Al2O3, as a consequence of which the fraction of YAG in the fracture surface was higher than the structural value estimated from a polished surface. The strength at room temperature of both L and T specimens was maintained up to 2023 K at high displacement speeds. At low displacement speeds, the strength decreased beyond 1900 K as a result of the enhanced plastic deformation. The stress exponent for plastic deformation at high temperatures (1823-2023 K) was 5-6, suggesting that the plastic deformation is controlled by a dislocation mechanism during bending as well as in compressive and tensile loading. The fracture toughness tended to increase with increasing temperature and with decreasing displacement speed, especially in L specimens. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2117 / 2128
页数:12
相关论文
共 14 条
[1]  
CANNON WR, 1983, J MATER SCI, V18, P1, DOI 10.1007/BF00543808
[2]   CREEP OF YTTRIUM-ALUMINUM-GARNET SINGLE-CRYSTALS [J].
CORMAN, GS .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1993, 12 (06) :379-382
[3]  
Davidge R.W., 1979, MECH BEHAV CERAMICS, P64
[4]  
*JAP SOC IND, 1994, R1617 JIS
[5]   BRITTLE-DUCTILE TRANSITION AND DISLOCATION MOBILITY IN SAPPHIRE [J].
KIM, HS ;
ROBERTS, S .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (12) :3099-3104
[6]   FRACTURE-TOUGHNESS OF SINGLE-CRYSTAL YAG [J].
MAH, T ;
PARTHASARATHY, TA .
SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (11) :1383-1385
[7]  
OCHIAI S, 1993, MECH PROPERTIES META, P473
[8]   DEFORMATION-BEHAVIOR OF AN AL2O3-Y3AL5O12 EUTECTIC COMPOSITE IN COMPARISON WITH SAPPHIRE AND YAG [J].
PARTHASARATHY, TA ;
MAH, TL ;
MATSON, LE .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (01) :29-32
[9]   HIGH-TEMPERATURE PROPERTIES OF UNIDIRECTIONALLY SOLIDIFIED AL2O3/YAG COMPOSITES [J].
WAKU, Y ;
NAKAGAWA, N ;
OHTSUBO, H ;
OHSORA, Y ;
KOHTOKU, Y .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1995, 59 (01) :71-78
[10]   Sapphire matrix composites reinforced with single crystal YAG phases [J].
Waku, Y ;
Ohtsubo, H ;
Nakagawa, N ;
Kohtoku, Y .
JOURNAL OF MATERIALS SCIENCE, 1996, 31 (17) :4663-4670