Effect of Cold Rolling and Annealing on Texture Evolution and Mechanical Properties of IF Steel Sheet

被引:0
作者
Shen, Yongfeng [1 ]
Xue, Wenying [2 ]
Guo, Yanhui [3 ]
机构
[1] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Minist Educ, Shenyang 110004, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110004, Peoples R China
[3] Shanghai Inst Technol, Shanghai 200235, Peoples R China
关键词
IF steel; Texture; Cold rolling rate; Annealing; Strength; LOW-CARBON STEELS; LARGE STRAINS; STRENGTH; MICROSTRUCTURE; DEFORMATION; ORIENTATION; ALUMINUM; ARB;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The dependence of textural evolution, deformation microstructure and flow stress on cold-rolling reductions of an interstitial-free (IF) steel sheet has been investigated using the X-ray diffraction and the transmission electron microscopy techniques as well as tensile tests. The development of both alpha-and gamma-fiber orientations is observed during cold-rolling to reductions of 13% to 75%. It is also noted that deformation microstructures consist of geometrically necessary boundaries and incidental dislocation boundaries. Dislocation and grain boundary hardening leads to increase in flow stress with the rolling reduction. A fall in ductility seen between rolling reductions of 13% to 46% is attributed to the onset of localized shearing. The re-gaining ductility is concerned with the more uniform size of cell blocks in two dimensions with an increase of rolling reduction to 57%. Further annealing tests were carried out for the sample with 75% of rolling reduction to obtain an improved ductility. However, the sample exhibited a very small increment in ductility (similar to 3%) and an obvious decrease in strength under an annealed temperature of 500 degrees C. With an increase in annealing temperature to 750 degrees C, the ductility impressively increased to 29% at the expense of strength, decreasing from 710 MPa to 210 MPa due to the process of recovery and recrystallization. These results clearly demonstrate that, without geometrically necessary boundaries and incidental dislocation boundaries, the lack of strain hardening at room temperature is related to dynamic recovery.
引用
收藏
页码:146 / 149
页数:4
相关论文
共 20 条
[1]   ORIENTATION DISTRIBUTION, ELASTIC AND PLASTIC ANISOTROPY IN STABILIZED STEEL SHEET [J].
BUNGE, HJ ;
ROBERTS, WT .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 1969, 2 :116-&
[2]   Evaluation of stored energy in cold-rolled steels from EBSD data [J].
Choi, SH ;
Jin, YS .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 371 (1-2) :149-159
[3]  
EMREN F, 1986, ACTA METALL, V34, P1205
[4]   THEORY OF TENSILE TEST [J].
HART, EW .
ACTA METALLURGICA, 1967, 15 (02) :351-&
[5]   Microstructure and strength of nickel at large strains [J].
Hughes, DA ;
Hansen, N .
ACTA MATERIALIA, 2000, 48 (11) :2985-3004
[6]   Shear rolling and recrystallization textures of interstitial-free steel sheet [J].
Lee, SH ;
Lee, DN .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 249 (1-2) :84-90
[7]   Study of metadynamic recrystallization behaviors in a low alloy steel [J].
Lin, Y. C. ;
Chen, Ming-Song ;
Zhong, Jue .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (05) :2477-2482
[8]   Microstructure and strength of commercial purity aluminium (AA 1200) cold-rolled to large strains [J].
Liu, Q ;
Huang, X ;
Lloyd, DJ ;
Hansen, N .
ACTA MATERIALIA, 2002, 50 (15) :3789-3802
[9]   Work-hardening/softening behaviour of BCC polycrystals during changing strain paths: II. TEM observations of dislocation sheets in an if steel during two-stage strain paths and their representation in terms of dislocation densities [J].
Peeters, B ;
Bacroix, B ;
Teodosiu, C ;
Van Houtte, P ;
Aernoudt, E .
ACTA MATERIALIA, 2001, 49 (09) :1621-1632
[10]   ANNEALING TEXTURES OF BCC METALS [J].
RAABE, D ;
LUCKE, K .
SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (11) :1533-1538