Phase transformation and cycling characteristics of a Ce2Ni7-type single-phase La0.78Mg0.22Ni3.45 metal hydride alloy

被引:39
作者
Zhang, Lu [1 ,2 ]
Li, Yuan [1 ,2 ]
Zhao, Xin [3 ]
Liu, Jingjing [1 ,2 ]
Ke, Dandan [1 ,2 ]
Du, Wenkai [1 ,2 ]
Yang, Shuqin [1 ,2 ]
Han, Shumin [1 ,2 ]
机构
[1] Yanshan Univ, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[2] Yanshan Univ, Sch Environm & Chem Engn, Hebei Key Lab Appl Chem, Qinhuangdao 066004, Peoples R China
[3] Baotou Res Inst Rare Earth, Baotou 014030, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
HYDROGEN STORAGE ALLOYS; ELECTROCHEMICAL PROPERTIES; MG; BEHAVIOR; SYSTEM; ELECTRODES; BATTERIES; LA2MGNI9; (ND; AL;
D O I
10.1039/c5ta02554k
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A Ce2Ni7-type single-phase La0.78Mg0.22Ni3.45 alloy has been prepared by zoning annealing of the as-cast sample. It is found that at temperatures below 890 degrees C, non-super-stacking CaCu5- and MgCu4Sn-type phases disappear and super-stacking Ce5Co19-, Gd2Co7- and Ce2Ni7-type phases remain. The Ce5Co19-type phase can totally transform into the Ce2Ni7-type phase via a peritectic reaction at temperatures of 890-900 degrees C. At temperatures of 900-950 degrees C, the Gd2Co7-type phase melts and decomposes into the Ce5Co19-type phase, and the newly formed Ce5Co19-type phase subsequently reacts to form the Ce2Ni7-type phase. The Ce2Ni7-type single phase remains stable even at higher temperatures of 950-975 degrees C. The single-phase alloy shows a superior discharge capacity, close to 394 mA h g (1), and high electrochemical cycling stability, which can achieve 413 cycles as its discharge capacity reduces to 60% of the maximum value. We found that the capacity attenuation of the single-phase alloy is mainly due to the loss of active material at the alloy surface caused by oxidization of La and Mg, and the pulverization of the alloy is not severe with 100 charge/discharge cycles. The crystal structure of the single-phase alloy can be preserved well. Oxidation of La occurs prior to that of Mg. La hydroxide grows from nano-structured needles to larger-scaled rods then to unformed lamellar hydroxide, whereas the precipitation of Mg forms as irregular lamellae inlaid with hexagonal flakes.
引用
收藏
页码:13679 / 13690
页数:12
相关论文
共 24 条
[1]   Mg substitution effect on the hydrogenation behaviour, thermodynamic and structural properties of the La2Ni7-H(D)2 system [J].
Denys, R. V. ;
Riabov, A. B. ;
Yartys, V. A. ;
Sato, Masashi ;
Delaplane, R. G. .
JOURNAL OF SOLID STATE CHEMISTRY, 2008, 181 (04) :812-821
[2]   Hydrogen storage properties and structure of La1-xMgx(Ni1-yMny)3 intermetallics and their hydrides [J].
Denys, R. V. ;
Riabov, B. ;
Yartys, V. A. ;
Delaplane, R. G. ;
Sato, M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 446 :166-172
[3]  
Deyuan Z., 1991, J LESS-COMMON MET, V169, P45
[4]   Hydrogen atom distribution and hydrogen induced site depopulation for the La2-xMgxNi7-H system [J].
Guzik, Matylda N. ;
Hauback, Bjorn C. ;
Yvon, Klaus .
JOURNAL OF SOLID STATE CHEMISTRY, 2012, 186 :9-16
[5]   Annealing effect on phase composition and electrochemical properties of the Co-free La2MgNi9 anode for Ni-metal hydride batteries [J].
Hu, Wei-Kang ;
Denys, Roman V. ;
Nwakwuo, Christopher C. ;
Holm, Thomas ;
Maehlen, Jan Petter ;
Solberg, Jan Ketil ;
Yartys, Volodymyr A. .
ELECTROCHIMICA ACTA, 2013, 96 :27-33
[6]   Experimental investigation and thermodynamic modeling of the Nd-Ni system [J].
Huang, ML ;
McCallum, RW ;
Lograsso, TA .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 398 (1-2) :127-132
[7]   Hydrogen storage properties of new ternary system alloys:: La2MgNi9, La5Mg2Ni23, La3MgNi14 [J].
Kohno, T ;
Yoshida, H ;
Kawashima, F ;
Inaba, T ;
Sakai, I ;
Yamamoto, M ;
Kanda, M .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 311 (02) :L5-L7
[8]   Effect of crystal transformation on electrochemical characteristics of La-Mg-Ni-based alloys with A2B7-type super-stacking structures [J].
Liu, Jingjing ;
Han, Shumin ;
Li, Yuan ;
Zhang, Junling ;
Zhao, Yumeng ;
Che, Linda .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (34) :14903-14911
[9]   An investigation on phase transformation and electrochemical properties of as-cast and annealed La0.75Mg0.25Nix (x=3.0, 3.3, 3.5, 3.8) alloys [J].
Liu, Jingjing ;
Han, Shumin ;
Li, Yuan ;
Yang, Shuqin ;
Shen, Wenzhuo ;
Zhang, Lu ;
Zhou, Yu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 552 :119-126
[10]   Degradation mechanism of the La-Mg-Ni-based metal hydride electrode La0.7Mg0.3Ni3.4Mn0.1 [J].
Liu, YF ;
Pan, HG ;
Gao, MX ;
Lei, YQ ;
Wang, QD .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (06) :A1089-A1095