Kinetic study of austenite formation during continuous heating of unalloyed ductile iron

被引:12
作者
Vazquez-Gomez, Octavio [1 ]
Antonio Barrera-Godinez, Jose [1 ]
Javier Vergara-Hernandez, Hector [2 ]
机构
[1] Univ Nacl Autonoma Mexico, Dept Met Engn, Fac Chem, Mexico City 04510, DF, Mexico
[2] Morelia Inst Technol, Met Sci Postgrad Programme, Morelia 58820, Michoacan, Mexico
关键词
ductile iron; austenite; continuous heating; heating rate; kinetics; dilatometry; CARBON MICROALLOYED STEEL; TRANSFORMATION; PEARLITE;
D O I
10.1007/s12613-015-1039-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The austenite formation kinetics in unalloyed cast ductile iron was studied on the basis of dilatometry measurements, and Avrami's equation was used to estimate the material's kinetic parameters. A continuous heating transformation diagram was constructed using heating rates in the range of 0.06 to 0.83A degrees C center dot s(-1). As the heating rate was augmented, the critical temperatures, A (c1) and A (alpha), as well as the intercritical range, which was evaluated as the difference between the critical temperatures, Delta T = A (alpha) - A (c1), increased. At a low heating rate, the kinetics of austenite formation was slow as a consequence of the iron's silicon content. The effect of heating rate on k and n, the kinetic parameters of Avrami's equation, was also determined. Parameter n, which is associated with nucleation sites and growth geometry, decreased with an increase in heating rate. In addition, parameter k increased with the increase of heating rate, suggesting that the nucleation and growth rates are carbon- and silicon-diffusion controlled during austenite formation under continuous heating.
引用
收藏
页码:27 / 31
页数:5
相关论文
共 15 条
[1]   Formation kinetics of austenite in pearlitic ductile iron [J].
Abdollahi, Payam ;
Amirsadeghi, Alborz ;
Kheirandish, Shahram ;
Mirdamadi, Shamsoddin .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2012, 19 (06) :506-510
[2]   THEORY FOR REAUSTENITIZATION FROM FERRITE/CEMENTITE MIXTURES IN FE-C-X STEELS [J].
ATKINSON, C ;
AKBAY, T ;
REED, RC .
ACTA METALLURGICA ET MATERIALIA, 1995, 43 (05) :2013-2031
[3]  
Avrami M., 1940, J CHEM PHYS, V8, P212, DOI [10.1063/1.1750631, DOI 10.1063/1.1750631]
[4]   Mathematical model for austenitization kinetics of ductile iron [J].
Batra, U ;
Ray, S ;
Prabhakar, S .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2005, 14 (05) :574-581
[5]   Kinetics of bainite-to-austenite transformation during continuous reheating in low carbon microalloyed steel [J].
Chang, Ming ;
Yu, Hao .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2013, 20 (05) :427-432
[6]   Application of dilatometric analysis to the study of solid-solid phase transformations in steels [J].
de Andrés, CG ;
Caballero, FG ;
Capdevila, C ;
Alvarez, LF .
MATERIALS CHARACTERIZATION, 2002, 48 (01) :101-111
[7]  
Hernandez-Morale B., 2014, Materials Science Forum, V783-786, P771, DOI 10.4028/www.scientific.net/MSF.783-786.771
[8]   The pearlite reaction in steels: Mechanisms and crystallography part I. From HC Sorby to RF Mehl [J].
Howell, PR .
MATERIALS CHARACTERIZATION, 1998, 40 (4-5) :227-260
[9]   A computational study of austenite formation kinetics in rapidly heated steels [J].
Katsamas, A. I. .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (14) :6414-6422
[10]   Modelling of the eutectoid reaction in spheroidal graphite Fe-C-Si alloys [J].
Lacaze, J ;
Gerval, V .
ISIJ INTERNATIONAL, 1998, 38 (07) :714-722