Autonomous crack healing ability of SiC dispersed Yb2Si2O7 by oxidations in air and water vapor

被引:11
作者
Okawa, A. [1 ]
Nguyen, S. T. [2 ]
Wiff, J. P. [1 ]
Son, H-W [1 ]
Nakayama, T. [1 ]
Do, T. M. D. [1 ,3 ]
Suematsu, H. [1 ]
Suzuki, T. [3 ]
Goto, T. [1 ]
Niihara, K. [1 ]
机构
[1] Nagaoka Univ Technol, Extreme Energy Dens Res Inst, Nagaoka, Niigata 9402188, Japan
[2] Kushiro Coll, Natl Inst Technol, Dept Creat Engn, Kushiro 0840916, Japan
[3] Nagaoka Univ Technol, Dept Nucl Syst Safety Engn, Nagaoka, Niigata 9402188, Japan
关键词
Ceramic matrix composites; Environmental barrier coatings; Crack healing; Ytterbium disilicate; Silicon carbide; Water vapor oxidation; ENVIRONMENTAL BARRIER COATINGS; MECHANICAL-PROPERTIES; SILICON-CARBIDE; CERAMICS; KINETICS; BEHAVIOR; CRYSTALLIZATION; CORROSION; ALUMINA; AL2O3;
D O I
10.1016/j.ceramint.2021.09.020
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Yb2Si2O7 is a popular environmental barrier coating; however, it decomposes into Yb2SiO5 in high-temperature steam environments. The thermal mismatch between Yb2Si2O7 and Yb2SiO5 leads to the cracking and failure of the disilicate coating via oxidation. Dispersing SiC nanofillers into the Yb2Si2O7 matrix is suggested to maintain the Yb2Si2O7 matrix and promote crack self-healing. This study is aimed at clarifying the effect of water vapor on the self-healing ability of such composites. X-ray diffraction analysis and scanning electron microscopy were used to monitor the surface composition and the crack formation, respectively, in 10 vol% SiC-dispersed Yb2Si2O7 composites. Annealing at temperatures higher than 750 degrees C in air or in a water vapor rich atmosphere led to strength recovery and the self-healing of indentation-induced surface cracks owing to volume expansion during the oxidation of SiC. The self-healing effect was influenced by the oxidation time and temperature. Rapid diffusion of H2O as an oxidizer into the SiO2 layer promoted self-healing in a water vapor rich atmosphere. However, accelerated oxidation at temperatures higher than 1150 degrees C formed bubbles on the surface. Fabricating composites with a small amount of Yb2SiO5 will be a solution to these problems.
引用
收藏
页码:34802 / 34809
页数:8
相关论文
共 55 条
[11]   Self-Healing Engineering Ceramics with Oxidation-Induced Crack Repair [J].
Greil, Peter .
ADVANCED ENGINEERING MATERIALS, 2020, 22 (09)
[12]   Blowing of silica microforms on silicon carbide [J].
Guinel, MJF ;
Norton, MG .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2005, 351 (03) :251-257
[13]   Thermodynamic Assessment of the Si-Ta and Si-W Systems [J].
Guo, Zhongnan ;
Yuan, Wenxia ;
Sun, Yu ;
Cai, Zhoufei ;
Qiao, Zhiyu .
JOURNAL OF PHASE EQUILIBRIA AND DIFFUSION, 2009, 30 (05) :564-570
[14]   GENERALIZED ISOTROPIC YIELD CRITERION [J].
HOSFORD, WF .
JOURNAL OF APPLIED MECHANICS, 1972, 39 (02) :607-&
[15]   Crack -healing behaviour of zirconia/SiC composite ceramics [J].
Dept. of Mech. Eng., Oyama Nat. College of Tech., Nakakuki, Oyama, 323-0806, Japan ;
不详 .
Zairyo, 2009, 6 (510-515) :510-515
[16]   Oxidation and corrosion of ceramics and ceramic matrix composites [J].
Jacobson, NS ;
Opila, EJ ;
Lee, KN .
CURRENT OPINION IN SOLID STATE & MATERIALS SCIENCE, 2001, 5 (04) :301-309
[17]  
Jiangtao Gao, 2018, Journal of Physics: Conference Series, V1074, DOI 10.1088/1742-6596/1074/1/012074
[18]   Silicon Nitride for High-Temperature Applications [J].
Klemm, Hagen .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (06) :1501-1522
[19]   Crack-healing in ytterbium silicate filled with silicon carbide particles [J].
Kunz, Willy ;
Klemm, Hagen ;
Michaelis, Alexander .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (15) :5740-5748
[20]   Thermodynamic optimization of the Nb-Si-W ternary system [J].
Li, Yan ;
Li, Changrong ;
Du, Zhenmin ;
Guo, Cuiping .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2013, 43 :112-123