Simulations on the thermal decomposition of a poly(dimethylsiloxane) polymer using the ReaxFF reactive force field

被引:406
作者
Chenoweth, K
Cheung, S
van Duin, ACT
Goddard, WA [1 ]
Kober, EM
机构
[1] CALTECH, Div Chem, Mat & Proc Simulat Ctr, Pasadena, CA USA
[2] CALTECH, Div Chem Engn, Mat & Proc Simulat Ctr, Pasadena, CA USA
[3] Los Alamos Natl Lab, Los Alamos, NM 87545 USA
关键词
D O I
10.1021/ja050980t
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
To investigate the failure of the poly(dimethylsiloxane) polymer (PDMS) at high temperatures and pressures and in the presence of various additives, we have expanded the ReaxFF reactive force field to describe carbon-silicon systems. From molecular dynamics (MD) simulations using ReaxFF we find initial thermal decomposition products of PDMS to be CH3 radical and the associated polymer radical, indicating that decomposition and subsequent cross-linking of the polymer is initiated by Si-C bond cleavage, in agreement with experimental observations. Secondary reactions involving these CH3 radicals lead primarily to formation of methane. We studied temperature and pressure dependence of PDMS decomposition by following the rate of production of methane in the ReaxFF MD simulations. We tracked the temperature dependency of the methane production to extract Arrhenius parameters for the failure modes of PDMS. Furthermore, we found that at increased pressures the rate of PDMS decomposition drops considerably, leading to the formation of fewer CH3 radicals and methane molecules. Finally, we studied the influence of various additives on PDMS stability. We found that the addition of water or a SiO2 slab has no direct effect on the short-term stability of PDMS, but addition of reactive species such as ozone leads to significantly lower PDMS decomposition temperature. The addition of nitrogen monoxide does not significantly alter the degradation temperature but does retard the initial production of methane and C-2 hydrocarbons until the nitrogen monoxide is depleted. These results, and their good agreement with available experimental data, demonstrate that ReaxFF provides a useful computational tool for studying the chemical stability of polymers.
引用
收藏
页码:7192 / 7202
页数:11
相关论文
共 37 条
[1]   The conformation of poly(dimethylsiloxane) in the crystalline state [J].
Albouy, PA .
POLYMER, 2000, 41 (08) :3083-3086
[2]   DENSITY-FUNCTIONAL THERMOCHEMISTRY .3. THE ROLE OF EXACT EXCHANGE [J].
BECKE, AD .
JOURNAL OF CHEMICAL PHYSICS, 1993, 98 (07) :5648-5652
[3]   MOLECULAR-DYNAMICS WITH COUPLING TO AN EXTERNAL BATH [J].
BERENDSEN, HJC ;
POSTMA, JPM ;
VANGUNSTEREN, WF ;
DINOLA, A ;
HAAK, JR .
JOURNAL OF CHEMICAL PHYSICS, 1984, 81 (08) :3684-3690
[4]   Thermal destruction of polydimethyl-siloxane on a phosphorus-containing silica surface [J].
Bogatyr'ov, VM ;
Borysenko, MV .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2000, 62 (02) :335-344
[5]   EMPIRICAL POTENTIAL FOR HYDROCARBONS FOR USE IN SIMULATING THE CHEMICAL VAPOR-DEPOSITION OF DIAMOND FILMS [J].
BRENNER, DW .
PHYSICAL REVIEW B, 1990, 42 (15) :9458-9471
[6]  
Butts M, 2003, ENCY POLYM SCI TECHN
[7]   Thermal polydimethylsiloxane degradation. Part 2. The degradation mechanisms [J].
Camino, G ;
Lomakin, SM ;
Lageard, M .
POLYMER, 2002, 43 (07) :2011-2015
[8]   Polydimethylsiloxane thermal degradation - Part 1. Kinetic aspects [J].
Camino, G ;
Lomakin, SM ;
Lazzari, M .
POLYMER, 2001, 42 (06) :2395-2402
[9]   Characterisation and oxidative degradation of a room-temperature vulcanised poly(dimethylsiloxane) rubber [J].
Chaudhry, AN ;
Billingham, NC .
POLYMER DEGRADATION AND STABILITY, 2001, 73 (03) :505-510
[10]   EFFICIENT DIFFUSE FUNCTION-AUGMENTED BASIS SETS FOR ANION CALCULATIONS. III. THE 3-21+G BASIS SET FOR FIRST-ROW ELEMENTS, LI-F [J].
CLARK, T ;
CHANDRASEKHAR, J ;
SPITZNAGEL, GW ;
SCHLEYER, PV .
JOURNAL OF COMPUTATIONAL CHEMISTRY, 1983, 4 (03) :294-301