Effect of the Supplementary Aging Process on the Microstructure and Mechanical Properties of Mg-5Sn and Mg-5Sn-0.5Zn Alloys

被引:1
|
作者
Yousefi, Masoud [1 ]
Mofrad, Nadia Sadat Bahrololoumi [1 ]
Kerahroodi, Mohamad Sadegh Amiri [1 ]
Barikbin, Hanieh Sadat [2 ]
Moudi, Mehdi [3 ]
机构
[1] Shahid Beheshti Univ, Abbaspour Power & Water Coll Engn, Dept Energy & Mech Engn, Tehran, Iran
[2] Islamic Azad Univ, Sci & Res Branch, Fac Food & Sci & Engn, Tehran, Iran
[3] Inst Appl Mat Reliabil Components & Syst IAM ZBS, Karlsruhe, Germany
关键词
Novel aging process; Mg-5Sn; Mg-5Sn-0.5Zn; Nanostructure; Mechanical properties; Supplementary aging; AGE-HARDENING RESPONSE; CORROSION BEHAVIOR; CREEP RESISTANCE; MAGNESIUM ALLOY; ZN; CAST; ADDITIONS; AL; EVOLUTION; AZ91;
D O I
10.1007/s12666-018-1489-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper presents a novel aging process consisting of two stages: an aging at 250 A degrees C for 12 h and a supplementary aging at 70 A degrees C for 18 h. The ingots of Mg-5Sn and Mg-5Sn-0.5Zn alloys were solution heat-treated for 24 h at 480 A degrees C and then quenched in water. Afterward, aging treatments were performed. To compare the effects of this process on age hardening response of both alloys, other aging treatments were performed at 200 A degrees C for 60 h and at 280 A degrees C for 12 h. The age hardening responses were measured by the Vickers hardness test. The structure of specimens was investigated by XRF, DSC, XRD, and FE-SEM. Also, mechanical properties were determined by tensile test and Charpy impact test. Although by using supplementary aging process, maximum hardness of these alloys is not very different in comparison with single- as well as double-aging processes, the necessary times of aging processes are significantly lower than those at around 90%, 85%, and 50%. After the aging process, the microstructure of Mg-5Sn and Mg-5Sn-0.5Zn alloys consists of alpha-Mg, nano-metric particles of Mg2Sn, and GP-zones. In Mg-5Sn alloy, after supplementary aging process, the yield strength, ultimate tensile strength, and elongation increase to 151.2 MPa, 221.2 MPa, and 8% sequentially. In Mg-5Sn-0.5Zn alloy, the YS, UTS, and elongation increase to 154 MPa, 224 MPa, and 7%, respectively. The impact energy in both alloys is 6.63 J and 7.05 J, respectively.
引用
收藏
页码:383 / 399
页数:17
相关论文
共 50 条
  • [31] The microstructure, creep resistance, and high-temperature mechanical properties of Mg-5Sn alloy with Ca and Sb additions, and aging treatment
    Nayyeri, G.
    Mahmudi, R.
    Salehi, F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (21-22): : 5353 - 5359
  • [32] Effect of Zn Content on the Microstructure and Mechanical Properties of Mg-Al-Sn-Mn Alloys
    Zhao, Tianshuo
    Hu, Yaobo
    Pan, Fusheng
    He, Bing
    Guan, Maosheng
    Yuan, Yuan
    Tang, Aitao
    MATERIALS, 2019, 12 (19)
  • [33] Effect of Ag and Cu trace additions on the microstructural evolution and mechanical properties of Mg-5Sn alloy
    Jayalakshmi, S.
    Sankaranarayanan, S.
    Koh, S. P. X.
    Gupta, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 565 : 56 - 65
  • [34] Microstructure evolution of as-cast Mg-5Sn alloy with Ba addition
    Chen, Yu'An (chenyuan@cqu.edu.cn), 1600, Elsevier Ltd (657):
  • [35] Enhanced creep properties of a cast Mg-5Sn alloy subjected to aging-treatment
    Nayyeri, G.
    Mahmudi, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (18-19): : 4613 - 4618
  • [36] Microstructure evolution of as-cast Mg-5Sn alloy with Ba addition
    Jiang, Yan
    Chen, Yu'an
    Liu, Hao
    Jin, Li
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 657 : 68 - 72
  • [37] Electrical and thermal conductivity in Mg-5Sn Alloy at different aging status
    Wang, Chunming
    Cui, Zhiming
    Liu, Hongmei
    Chen, Yungui
    Ding, Wucheng
    Xiao, Sufen
    MATERIALS & DESIGN, 2015, 84 : 48 - 52
  • [38] Effect of Er-Adding on Microstructure and Lattice Parameter for Mg-5Sn as Cast Alloy
    Zhang Dingfei
    Ma Chunhua
    Zhang Hongju
    Chai Sensen
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (12) : 2481 - 2485
  • [39] Effect of Sn Content on the Microstructure, Mechanical Properties and Corrosion Behavior of Biodegradable Mg-x ( 1, 3 and 5 wt.%) Sn-1Zn-0.5Ca Alloys
    Zhao, Zheng-Xue
    Hua, Zhen-Ming
    Li, Da-Wei
    Wei, Dong-Song
    Liu, Yan
    Wang, Jin-Guo
    Luo, Dan
    Wang, Hui-Yuan
    MATERIALS, 2018, 11 (12)
  • [40] Effects of Zn/Sn mass ratio on microstructure and mechanical properties of Mg-Zn-Sn-Al-Ca alloys
    Pan, X. Q.
    Chen, J. H.
    Yan, H. G.
    Su, B.
    Wei, J. Y.
    Fan, C.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (02) : 169 - 176