Erosion behavior of EEDS cermet coatings

被引:11
作者
Guo, Jin [1 ,2 ]
Xu Bin-shi [3 ]
Wang Hai-dou [3 ]
Liang, Yin [1 ]
Li Qing-fen [2 ]
Wei Shi-cheng [3 ]
Cui Xiufang [4 ]
机构
[1] Tsinghua Univ, State Key Lab Tribol, Beijing 100084, Peoples R China
[2] Harbin Engn Univ, Ctr Biomed Mat & Engn, Harbin 150001, Peoples R China
[3] Armores Forces Engn Inst, Natl Key Lab Remfg, Beijing 100072, Peoples R China
[4] Harbin Engn Univ, Sch Mat Sci & Chem Engn, Harbin 150001, Peoples R China
关键词
erosion; structure; TEM; EEDS; cermet coating;
D O I
10.1016/j.apsusc.2008.02.098
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper investigates the erosion performance of electro-thermal explosion directional spraying (EEDS) cermet WC/Co coatings using an air solid particle erosion rig. The influences of the different parameters such as impact angle, impingement velocity, environment temperature, particle diameter, on the erosion property of the coatings were studied. The eroded surfaces were examined by scanning electron microscopy (SEM) equipped with energy dispersive spectrometry (EDS) and the erosion mechanisms were discussed. The structure and bond characters of the coatings were also determined by transmission electron microscopy (TEM), X-ray diffraction (XRD) and SEM. The results indicate that the EEDS WC/Co coatings are characterized by. ne grain structure, good metallurgical bond and brittle erosion character. The erosion rates of the coatings decrease with temperature increasing and increase with impact angle and impingement velocity increasing. At elevated temperature, the oxidation happens on the coatings surface, which affects the erosion behavior. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:5470 / 5474
页数:5
相关论文
共 23 条
[1]   Erosion-corrosion properties of different WC-Co-Cr coatings deposited by the HVOF process - influence of metallic matrix composition and spray powder size distribution [J].
Berget, J. ;
Rogne, T. ;
Bardal, E. .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (18) :7619-7625
[2]  
Cullity B., 1978, ELEMENTS XRAY DIFFRA
[3]   The effect of impact angle on the erosion rate of polycrystalline α-Al2O3 [J].
Franco, A ;
Roberts, SG .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (03) :269-274
[4]   Erosion rate correlations of a pipe protruded in an abrupt pipe contraction [J].
Habib, M. A. ;
Badr, H. M. ;
Ben-Mansour, R. ;
Kabir, M. E. .
INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2007, 34 (08) :1350-1369
[5]   Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings [J].
Hawthorne, HM ;
Arsenault, B ;
Immarigeon, JP ;
Legoux, JG ;
Parameswaran, VR .
WEAR, 1999, 225 :825-834
[6]  
Hocking M.G., 1989, Metallic and Ceramic Coatings: Production, High Temperature Properties and Applications
[7]   Erosion-oxidation behaviour of pack-aluminized 9% chromium steel under fluidized-bed conditions at elevated temperature [J].
Huttunen-Saarivirta, E. ;
Stott, F. H. ;
Rohr, V. ;
Schuetze, M. .
CORROSION SCIENCE, 2007, 49 (07) :2844-2865
[8]   Investigation on the formation and wear resistance of TiC coatings [J].
Jin Guo ;
Xu Bin-shi ;
Wang Hai-dou ;
Li Qing-fen ;
Wei Shi-cheng .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 435 :355-359
[9]   Solid particle erosion of thermal sprayed coatings [J].
Kulu, P ;
Hussainova, I ;
Veinthal, R .
WEAR, 2005, 258 (1-4) :488-496
[10]   Ultra-fine powder by wire explosion method [J].
Kwon, YS ;
Jung, YH ;
Yavorovsky, NA ;
Illyn, AP ;
Kim, JS .
SCRIPTA MATERIALIA, 2001, 44 (8-9) :2247-2251