Texture evolution and earing in aluminium can sheet

被引:15
|
作者
Hirsch, J [1 ]
机构
[1] Hydro Aluminium Deutschland GMBH, R&D, D-53014 Bonn, Germany
来源
ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2 | 2005年 / 495-497卷
关键词
rolling texture; cube texture; anisotropy; earing; Al-Mg-Mn alloys can body stock;
D O I
10.4028/www.scientific.net/MSF.495-497.1565
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The texture evolution during hot and cold rolling of A1Mg1Mn1 can body sheet is described and the related anisotropy effects during deep drawing are analysed quantitatively. The typical textures of rolled aluminium show the transition between beta-fibre orientations and cube recrystallization texture, depending on rolling temperature and strain. These correlate with transitions between 45 degrees and 0 degrees/90 degrees ear heights in deep drawn cups which are described by a new method of Fourier series expansion. Processing parameters to achieve low anisotropy are discussed.
引用
收藏
页码:1565 / 1572
页数:8
相关论文
共 50 条
  • [21] Effect of the yield surface evolution on the earing defect prediction
    Aksen, Toros A.
    Firat, Mehmet
    REVISTA DE METALURGIA, 2023, 59 (01)
  • [22] Texture-based design of a convoluted cut-edge for earing-free beverage cans
    Engler, Olaf
    Mertens, Norbert
    van Dam, Pim
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2011, 211 (07) : 1278 - 1284
  • [23] Evolution of texture and strain states in AA 3003 sheet during sandwich rolling
    Huh, M. Y.
    Kim, J. K.
    Lee, J. C.
    Suk, H. G.
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES, 2006, 116-117 (320-323): : 320 - 323
  • [24] Influence of hot deformation parameters on texture and earing behaviour of AA5005
    Liu, C
    Zhuang, L
    van der Winden, MR
    Hurd, TJ
    Charot, B
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 2000, 331-3 : 787 - 792
  • [25] Compromising Effect on Development of Recrystallization Texture in Aluminium Sheet - A 2D MC Type Simulation
    Ito, Kunio
    TEXTURES OF MATERIALS, PTS 1 AND 2, 2012, 702-703 : 655 - 658
  • [26] The Effect of Fe Content on Recrystallization Texture Evolution, Microstructures, and Earing of Cold Rolled Continuous Cast AA5052 Alloy Sheets
    Xiyu Wen
    Wei Wen
    Yuanbin Zhang
    Bin Xu
    Qiang Zeng
    Yansheng Liu
    Lirong Tong
    Tongguang Zhai
    Zhong Li
    Metallurgical and Materials Transactions A, 2016, 47 : 1865 - 1880
  • [27] Evolution of orientation hardening in the cold rolling of an AA3003 aluminium alloy sheet
    Lee, WB
    Wen, XY
    FRACTURE AND STRENGTH OF SOLIDS, PTS 1 AND 2: PT 1: FRACTURE MECHANICS OF MATERIALS; PT 2: BEHAVIOR OF MATERIALS AND STRUCTURE, 1998, 145-9 : 1161 - 1166
  • [28] Simulation of earing during deep drawing of bcc steel by use of a texture component crystal plasticity finite element method
    Raabe, D
    Roters, F
    Wang, Y
    ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2, 2005, 495-497 : 1529 - 1534
  • [29] The effect of precipitation on the evolution of recrystallization texture in AA8011 aluminum alloy sheet
    Ryu, JH
    Lee, DN
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 336 (1-2): : 225 - 232
  • [30] Evolution of texture and strain states in AA 3004 sheet during rolling with a dead block
    Huh, MY
    Lee, KR
    Engler, O
    INTERNATIONAL JOURNAL OF PLASTICITY, 2004, 20 (07) : 1183 - 1197