Creep resistance and material degradation of a candidate Ni-Mo-Cr corrosion resistant alloy

被引:22
作者
Shrestha, Sachin L. [1 ]
Bhattacharyya, Dhriti [1 ]
Yuan, Guangzhou [2 ]
Li, Zhijun J. [2 ]
Budzakoska-Testone, Elizabeth [1 ]
De Los Reyes, Massey [1 ]
Drew, Michael [1 ]
Edwards, Lyndon [1 ]
机构
[1] ANSTO, Inst Mat Engn, Locked Bag 2001, Kirrawee Dc, NSW 2232, Australia
[2] Chinese Acad Sci, Shanghai Inst Appl Phys, Ctr Thorium Molten Salts Reactor Syst, Beijing 100864, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2016年 / 674卷
关键词
Nickel based alloy; Creep deformation; Carbide precipitation; Scanning electron microscopy; Electron backscatter diffraction; Transmission electron microscopy; MOLTEN-SALT REACTOR; STRUCTURAL-MATERIALS; RUPTURE PROPERTIES; STRESS RUPTURE; INCONEL; 718; SUPERALLOY; CHALLENGES; STRENGTH; BEHAVIOR; FRACTURE;
D O I
10.1016/j.msea.2016.07.032
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study investigated the creep deformation properties of GH3535, a Ni-Mo-Cr corrosion resistant structural alloy being considered for use in future Gen IV molten salt nuclear reactors (MSR) operating at around 700 degrees C. Creep testing of the alloy was conducted at 650-750 degrees C under applied stresses between 85-380 MPa. From the creep rupture results the long term creep strain and rupture life of the alloy were estimated by applying the Dorn Shepard and Larson Miller time-temperature parameters and the alloy's allowable ASME design stresses at the MSR's operating temperature were evaluated. The material's microstructural degradation at creep rupture was characterised using scanning electron microscopy (SEM), electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). The micro structural study revealed that the material failure was due to wedge cracking at triple grain boundary points and cavitation at coarse secondary grain boundary precipitates, nucleated and grown during high temperature exposure, leading to intergranular crack propagation. EBSD local misorientation maps clearly show that the root cause of cavitation and crack propagation was due to large strain localisation at the grain boundaries and triple points instigated by grain boundary sliding during creep deformation. This caused the grain boundary decohesion and subsequent material failure. Crown Copyright (C) 2016 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:64 / 75
页数:12
相关论文
共 40 条
[1]  
[Anonymous], 1996, P ASTM 0 01 MET MECH
[2]  
Ashby M.F., 2005, ENG MAT, V3rd, DOI DOI 10.1016/C2009-0-64288-4
[3]  
ASME, 2013, BOIL PRESS VESS CO D
[4]  
Boiler A., 2007, PRESSURE VESSEL CO D
[5]  
Booker M., 1979, EVALUATION CREEP REL
[6]   THE EFFECT OF GRAIN-BOUNDARY PRECIPITATES ON THE CREEP-BEHAVIOR OF INCONEL 718 [J].
CHEN, W ;
CHATURVEDI, MC .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 183 (1-2) :81-89
[7]   Dependence of creep fracture of Inconel 718 on grain boundary precipitates [J].
Chen, W ;
Chaturvedi, MC .
ACTA MATERIALIA, 1997, 45 (07) :2735-2746
[8]   Microstructural Evolution of an Ion Irradiated Ni-Mo-Cr-Fe Alloy at Elevated Temperatures [J].
de los Reyes, Massey ;
Edwards, Lyndon ;
Kirk, Marquis A. ;
Bhattacharyya, Dhriti ;
Lu, Kim T. ;
Lumpkin, Gregory R. .
MATERIALS TRANSACTIONS, 2014, 55 (03) :428-433
[9]  
Donachie M J., 2002, Superalloys: a Technical Guide
[10]  
Forsberg C.W., 2004, P ICAPP