FACTORS AFFECTING THE ENVIRONMENTAL ASSISTED CRACKING BEHAVIOR OF 2205 DUPLEX STAINLESS STEEL

被引:0
|
作者
Chasse, Kevin R. [1 ]
Yang, Di [2 ]
Singh, Preet M. [1 ]
Neu, Richard W. [1 ,2 ]
机构
[1] Georgia Inst Technol, Sch Mat Sci & Engn, Atlanta, GA 30332 USA
[2] Georgia Inst Technol, Sch Mech Engn, Atlanta, GA 30332 USA
来源
TMS 2010 139TH ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 3: GENERAL PAPER SELECTIONS | 2010年
关键词
2205; duplex stainless steel; low frequency fatigue; hydrogen embrittlement; STRESS-CORROSION CRACKING; HYDROGEN; FATIGUE; EMBRITTLEMENT; WATER;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The reliable performance of duplex stainless steels (DSSs) in chloride- and sulfide-containing solutions is important to many industrial processes. Previous studies have shown that DSSs are susceptible to environmental assisted cracking (EAC) under certain conditions in these solutions; however, the mechanical and electrochemical conditions under which DSSs may become susceptible are not well understood. To elucidate some of these mechanical and electrochemical conditions, the EAC susceptibilities of a 2205 DSS were evaluated in an acidic-chloride solution and a sulfide-containing caustic solution. Low frequency cyclic tests were performed for a fixed number of cycles, and the crack initiation events were examined after these tests. In the chloride solution, corrosion pits are the preferential sites for crack initiation under cyclic loading. In the sulfide-containing caustic solution, precipitates tend to be the preferential sites for cracks to initiate, especially the ones at or near the interface of the phase boundary and grain boundary. Hydrogen embrittlement (HE) was also found to be a potential form of EAC in this solution at room temperature when a cathodic potential (CP) was applied.
引用
收藏
页码:401 / +
页数:3
相关论文
共 50 条
  • [1] Hydrogen assisted cracking of 2205 duplex stainless steel in synthetic sea water
    Michalska, J.
    Labanowski, J.
    Cwiek, J.
    TECHNOLOGIES AND PROPERTIES OF MODERN UTILISED MATERIALS (TPMUM 2012), 2012, 35
  • [2] EVALUATION OF THE SUSCEPTIBILITY OF DUPLEX STAINLESS STEEL 2205 TO HYDROGEN ASSISTED CRACKING IN REAC SYSTEMS
    He, Mei
    Lippold, John
    Alexandrov, Boian
    Penso, Jorge
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2016, VOL 6B, 2017,
  • [3] Corrosion behavior of 2205 duplex stainless steel
    Platt, JA
    Guzman, A
    Zuccari, A
    Thornburg, DW
    Rhodes, BF
    Oshida, Y
    Moore, BK
    AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS, 1997, 112 (01) : 69 - 79
  • [4] Identification of microstructure factors affecting hydrogen embrittlement of a 2205 duplex stainless steel
    Wu, Weijie
    Liu, Shenguang
    Li, Weiguo
    Li, Jinxu
    CORROSION SCIENCE, 2022, 208
  • [5] Stress corrosion cracking behavior of 2205 duplex stainless steel in concentrated NaCl solution
    Tsai, WT
    Chen, MS
    CORROSION SCIENCE, 2000, 42 (03) : 545 - 559
  • [6] Hydrogen-enhanced cracking of 2205 duplex stainless steel
    Tsay, L. W.
    Young, M. C.
    Shin, C. -S.
    Chan, S. L. I.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2007, 30 (12) : 1228 - 1236
  • [7] Environmental Assisted Cracking Behavior of Sigmatized Super Duplex Stainless Steel in Oilfield Production Brine
    Saithala, J. R.
    Mahajanam, S.
    Ubhi, H. S.
    Atkinson, J.
    CORROSION, 2013, 69 (03) : 276 - 285
  • [8] Hot Deformation Behavior of Duplex Stainless Steel 2205
    Zhang, Yong-jun
    Dong, Yuan
    Hu, Jie-ren
    Zhang, Hui
    Han, Jing-tao
    METAL SCIENCE AND HEAT TREATMENT, 2024, 65 (9-10) : 624 - 628
  • [9] Hot Deformation Behavior of Duplex Stainless Steel 2205
    Zhang Yong-jun
    Dong Yuan
    Hu Jie-ren
    Zhang Hui
    Han Jing-tao
    Metal Science and Heat Treatment, 2024, 65 : 624 - 628
  • [10] HOT DEFORMATION BEHAVIOR OF 2205 DUPLEX STAINLESS STEEL
    Chen Lei
    Wang Longmei
    Du Xiaojian
    Liu Xiao
    ACTA METALLURGICA SINICA, 2010, 46 (01) : 52 - 56