Surface characterization analysis of failed dental implants using scanning electron microscopy

被引:6
|
作者
Daood, Umer [1 ]
Bandey, Ninette [1 ]
Bin Qasim, Saad [1 ]
Omar, Hanan [1 ]
Khan, Saad A. [1 ]
机构
[1] King Saud Univ, Riyadh, Saudi Arabia
关键词
titanium implants; dental implants; surface morphology; TITANIUM IMPLANTS; OSSEOINTEGRATED IMPLANTS; ORAL IMPLANTS; BONE RESPONSE;
D O I
10.3109/00016357.2011.569507
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. To investigate the failure of 15 dental implants (Paragon/Zimmer) in relation to their surface quality. Materials and methods. The study comprised of 15 dental implants (7 mm D Advent Implant, 3.9 mm D apex design implant), which were followed from surgery to completion of prosthetic restorations. The implants were placed during a 6-year period from 2003-2009 in non-smoking patients (male; 7, females; 5). There were eight upper and seven lower implants. Surface characterization after immersion in SBF of these failed implants was investigated using SEM and EDS compared to that of an unused implant of the same brand. Results. Results revealed that, following immersion in SBF, the implant surfaces showed new components like Ca+, Na+ and Cl-, but in trace quantities. Conclusions. After SEM observation and EDS analysis, it was concluded that the apatite layer formation could not be verified.
引用
收藏
页码:367 / 373
页数:7
相关论文
共 50 条
  • [21] SCANNING ELECTRON-MICROSCOPIC STUDIES OF THE ORAL-TISSUE RESPONSES TO DENTAL IMPLANTS
    STEFLIK, DE
    MCKINNEY, RV
    SISK, AL
    PARR, GR
    KOTH, DL
    SCANNING MICROSCOPY, 1990, 4 (04) : 1021 - 1038
  • [22] Surface analysis algorithms for scanning probe microscopy
    Lindquist, CS
    Urban, FK
    THIN SOLID FILMS, 1995, 270 (1-2) : 399 - 405
  • [23] Influence of Surface Modification Methods on the Topography of Dental Implants by Using Metrological Observation Techniques
    Bulutsuz, A. G.
    Mercan, C. U.
    Karapinar, G.
    Katiboglu, A. B.
    Lewandowska, M.
    ACTA PHYSICA POLONICA A, 2016, 129 (04) : 625 - 627
  • [24] Evaluation of loading conditions on fatigue-failed implants by fracture surface analysis
    Huang, HM
    Tsai, CM
    Chang, CC
    Lin, CT
    Lee, SY
    INTERNATIONAL JOURNAL OF ORAL & MAXILLOFACIAL IMPLANTS, 2005, 20 (06) : 854 - 859
  • [25] Surface Characterization of Dental Implants Coated With Hydroxyapatite by Plasma Spray and Biomimetic Process
    Vidigal, Guaracilei Maciel, Jr.
    Groisman, Mario
    de Sena, Lidia Agata
    Soares, Gloria de Almeida
    IMPLANT DENTISTRY, 2009, 18 (04) : 353 - 361
  • [26] CO2 laser surface treatment of failed dental implants for re-implantation: an animal study
    Kasraei, Shahin
    Torkzaban, Parviz
    Shams, Bahar
    Hosseinipanah, Seyed Mohammad
    Farhadian, Maryam
    LASERS IN MEDICAL SCIENCE, 2016, 31 (05) : 985 - 989
  • [27] Hot isostatic pressing-processed hydroxyapatite-coated titanium implants: Light microscopic and scanning electron microscopy investigations
    Wie, H
    Hero, H
    Solheim, T
    INTERNATIONAL JOURNAL OF ORAL & MAXILLOFACIAL IMPLANTS, 1998, 13 (06) : 837 - 844
  • [28] CO2 laser surface treatment of failed dental implants for re-implantation: an animal study
    Shahin Kasraei
    Parviz Torkzaban
    Bahar Shams
    Seyed Mohammad Hosseinipanah
    Maryam Farhadian
    Lasers in Medical Science, 2016, 31 : 985 - 989
  • [29] Atomic force microscopy and scanning electron microscopy characterization of the controlling of surface morphology of epoxy-amine-cured spin-coated films
    Shenk, Timothy M.
    Benjamin, Kenneth M.
    Winter, Robb M.
    JOURNAL OF APPLIED POLYMER SCIENCE, 2024, 141 (06)
  • [30] Histomorphometric Analysis of Osseointegrated Intraosseous Dental Implants Using Undecalcified Specimens: A Scoping Review
    Peev, Stefan
    Yotsova, Ralitsa
    Parushev, Ivaylo
    BIOMIMETICS, 2024, 9 (11)