Investigation of interface characteristics of Al2O3/Si under various O2 plasma exposure times during the deposition of Al2O3 by PA-ALD

被引:12
|
作者
Min, Kwan Hong [1 ,2 ]
Choi, Sungjin [1 ,3 ]
Jeong, Myeong Sang [1 ,2 ]
Kang, Min Gu [1 ]
Park, Sungeun [1 ]
Song, Hee-Eun [1 ]
Lee, Jeong In [1 ]
Kim, Donghwan [2 ]
机构
[1] Korea Inst Energy Res, Photovolta Lab, Daejeon 34129, South Korea
[2] Korea Univ, Dept Mat Sci & Engn, Seoul 02841, South Korea
[3] Korea Univ, Grad Sch Korea Energy & Environm, Green Sch, Dept Energy Environm Policy & Technol, Seoul 02841, South Korea
关键词
Plasma-assisted atomic layer deposition; Passivation; Al2O3; Plasma damage; Silicon solar cell; ATOMIC LAYER DEPOSITION; SURFACE PASSIVATION; FILMS; ALUMINA; GROWTH; OZONE; OXIDE; TMA;
D O I
10.1016/j.cap.2018.09.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Plasma-assisted atomic layer deposition (PA-ALD) is more suitable than thermal atomic layer deposition (ALD) for mass production because of its faster growth rate. However, controlling surface damage caused by plasma during the PA-ALD process is a key issue. In this study, the passivation characteristics of Al2O3 layers deposited by PA-ALD were investigated with various O-2 plasma exposure times. The growth per cycle (GPC) during Al2O3 deposition was saturated at approximately 1.4 angstrom/cycle after an O-2 plasma exposure time of 1.5 s, and a refractive index of Al2O3 in the range of 1.65-1.67 was obtained. As the O-2 plasma exposure time increased in the Al2O3 deposition process, the passivation properties tended to deteriorate, and as the radio frequency (RF) power increased, the passivation uniformity and the thermal stability of the Al2O3 layer deteriorated. To study the Al2O3 /Si interface characteristics, the capacitance-voltage (C-V) and the conductance-voltage (G-V) were measured using a mercury probe, and the fixed charge density (Q(f)) and the interface trap density (D-it) were then extracted. The Q(f) of the Al2O3 layer deposited on a Si wafer by PA-ALD was almost unaffected, but the D-it , increased with O-2 plasma exposure time. In conclusion, as the O-2 plasma exposure time increased during Al2O3 layer deposition by PA-ALD, the Al2O3/Si interface characteristics deteriorated because of plasma surface damage.
引用
收藏
页码:155 / 161
页数:7
相关论文
共 50 条
  • [41] Kinetic study of glycerol hydrodeoxygenation on Al2O3 and NiMo2C/Al2O3 catalysts
    Duarte, Rafael Belo
    Corazza, Marcos Lucio
    Pimenta, Joao Lourenco Castagnari Willimann
    Jorge, Luiz Mario de Matos
    FUEL, 2023, 354
  • [42] Hydrogen induced passivation of Si interfaces by Al2O3 films and SiO2/Al2O3 stacks
    Dingemans, G.
    Beyer, W.
    van de Sanden, M. C. M.
    Kessels, W. M. M.
    APPLIED PHYSICS LETTERS, 2010, 97 (15)
  • [43] Silicon Surface Passivation by Al2O3: Effect of ALD Reactants
    Repo, Paivikki
    Talvitie, Heli
    Li, Shuo
    Skarp, Jarmo
    Savin, Hele
    PROCEEDINGS OF THE SILICONPV 2011 CONFERENCE (1ST INTERNATIONAL CONFERENCE ON CRYSTALLINE SILICON PHOTOVOLTAICS), 2011, 8 : 681 - 687
  • [44] ALD Al2O3 based Nanolaminates for Solar Cell Applications
    Simon, Daniel K.
    Jordan, Paul M.
    Knaut, Martin
    Chohan, Talha
    Mikolajick, Thomas
    Dirnstorfer, Ingo
    2015 IEEE 42ND PHOTOVOLTAIC SPECIALIST CONFERENCE (PVSC), 2015,
  • [45] MANOS performance dependence on ALD Al2O3 oxidation source
    Nikolaou, Nikolaos
    Dimitrakis, Panagiotis
    Normand, Pascal
    Speliotis, Thanassis
    Kukli, Kaupo
    Niinisto, Jaakko
    Mizohata, Kenichiro
    Ritala, Mikko
    Leskela, Markku
    Ioannou-Sougleridis, Vassilios
    MICROELECTRONIC ENGINEERING, 2016, 159 : 127 - 131
  • [46] Spatial ALD of Al2O3 and ZnO using heavy water
    Kinnunen, Sami
    Sajavaara, Timo
    SURFACE & COATINGS TECHNOLOGY, 2022, 441
  • [47] Adsorption of NO and O2 on MnO2 and (MnO2)3/Al2O3
    Li, Hui
    Wang, Denghui
    Hui, Shien
    APPLIED SURFACE SCIENCE, 2021, 569
  • [48] Microstructural Changes of the Al2O3 Ceramics during the Exposure to Fluorine Plasma
    Kim, Dae Min
    Lee, Sung-Min
    Kim, Seong Won
    Kim, Hyung Tae
    Oh, Yoon-Suk
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2008, 45 (07) : 405 - 410
  • [49] Room-temperature synthesis of χ-Al2O3 and ruby (α-Cr:Al2O3)
    Cortes-Vega, Fernando D.
    Yang, Wenli
    Zarate-Medina, J.
    Brankovic, Stanko R.
    Herrera Ramirez, Jose M.
    Hernandez, Francisco C. Robles
    CRYSTENGCOMM, 2018, 20 (25): : 3505 - 3511
  • [50] Characterization of Al2O3 thin films prepared by thermal ALD
    Barbos, Corina
    Blanc-Pelissier, Daniele
    Fave, Alain
    Blanquet, Elisabeth
    Crisci, Alexandre
    Fourmond, Erwann
    Albertini, David
    Sabac, Andrei
    Ayadi, Khaled
    Girard, Philippe
    Lemiti, Mustapha
    5TH INTERNATIONAL CONFERENCE ON SILICON PHOTOVOLTAICS, SILICONPV 2015, 2015, 77 : 558 - 564