Austenitisation kinetics of unalloyed and alloyed ductile iron

被引:11
|
作者
Ahmadabadi, MN [1 ]
Parsa, MH [1 ]
机构
[1] Univ Tehran, Fac Engn, Dept Met & Mat Engn, Tehran, Iran
关键词
D O I
10.1179/026708301101509953
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Specimens with different microstructures of an unalloyed iron and a 0.75 wt-%Mn ductile iron were austenitised at 870 degreesC to study the kinetics of austenitisation. The specimens were austenitised in a salt bath furnace for different periods. The wafer specimens were ground, polished and etched before metallography and hardness tests. The thermodynamic procedure was used to calculate the Ae(3) phase boundary as a function of composition. The results were used to explain the effect of segregation on the kinetics of austenitisation. The results showed that the transformation rate in both the alloyed and the unalloyed pearlitic ductile iron is higher than that of the ferritic iron. As far as the ferritic structure is concerned, at the early stage of transformation the alloyed iron showed a higher austenitisation rate than the unalloyed iron, while after longer transformation the unalloyed iron showed the higher rate. This change in transformation rate is supposedly because of the effect of Mn segregation in the intercellular region. In the case of specimens with a pearlitic microstructure, unalloyed iron has a higher austenitisation rate than alloyed iron because of the effect of Mn on the stability of carbides in the pearlite. It was also shown that in all the specimens the cell boundaries are the most potent sites for nucleation of austenite. The Avrami equation was used to calculate k and n parameters as a function of microstructure. The results obtained indicate that n for specimens with different microstructures varies from 1.5 to 3.5. The results also show that the effect of the initial microstructure on the n and k values is greater than that of the chemical composition of the iron.
引用
收藏
页码:162 / 167
页数:6
相关论文
共 50 条
  • [1] Indentation fracture toughness of boronized unalloyed and alloyed ductile iron
    Toktas, Guelcan
    Korkmaz, Selman
    MATERIALS CHEMISTRY AND PHYSICS, 2023, 296
  • [2] Investigation of Mechanical Properties in Ductile Iron with Alloyed and Unalloyed at Time and Temperature on Austempering
    Rao, T. Lakshmana
    Lakshminarayana, V.
    Rao, Y. B. Shankar
    Suryanarana, B.
    JOURNAL OF POLYMER & COMPOSITES, 2023, 11 : S1 - S9
  • [3] Impact of heat treatment on mechanical and tribological behaviour of unalloyed and alloyed ductile iron
    Akinribide, O. J.
    Olusunle, S. O. O.
    Akinwamide, S. O.
    Babalola, B. J.
    Olubambi, P. A.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 14 : 1809 - 1819
  • [4] Transformation kinetics of unalloyed and high Mn austempered ductile iron
    Ahmadabadi, MN
    Farjami, S
    MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (05) : 645 - 649
  • [5] Austempering study of unalloyed and alloyed ductile irons
    Sidjanin, L.
    Rajnovic, D.
    Eric, O.
    Smallman, R. E.
    MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (05) : 567 - 571
  • [6] Properties of Unalloyed and Low-Alloyed Ductile Cast Iron at Elevated Temperatures.
    Roehrig, K.
    Giessereipraxis, 1985, (3-4): : 29 - 40
  • [7] Phase transformation and fatigue properties of alloyed and unalloyed austempered ductile irons
    Wu, CZ
    Shih, TS
    2002 WORLD CONFERENCE ON ADI: AUSTEMPERED DUCTILE IRON (ADI) FOR CASTING PRODUCERS, SUPPLIERS AND DESIGN ENGINEERS, 2002, : 107 - 109
  • [8] Austempering kinetics of Cu-Ni alloyed austempered Ductile Iron
    Olivera Eric Cekic
    Leposava Sidjanin
    Dragan Rajnovic
    Sebastian Balos
    Metals and Materials International, 2014, 20 : 1131 - 1138
  • [9] Austempering Kinetics of Cu-Ni Alloyed Austempered Ductile Iron
    Cekic, Olivera Eric
    Sidjanin, Leposava
    Rajnovic, Dragan
    Balos, Sebastian
    METALS AND MATERIALS INTERNATIONAL, 2014, 20 (06) : 1131 - 1138
  • [10] Multiphase matrix structure of unalloyed austempered ductile iron
    Yang, Chen
    Cui, Xixi
    Liu, Cheng
    MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (03) : 261 - 267