Fatigue assessment of cracked pipes with weld misalignment by using stress intensity factors

被引:15
|
作者
Zhao, Hai-Sheng [1 ]
Lie, Seng-Tjhen [1 ]
Zhang, Yao [1 ]
机构
[1] Nanyang Technol Univ, Sch Civil & Environm Engn, 50 Nanyang Ave, Singapore 639798, Singapore
关键词
Fatigue assessment; Finite element analysis; Stress intensity magnification factor; Surface crack; Weld misalignment; TOE MAGNIFICATION FACTORS; CIRCUMFERENTIAL SURFACE CRACKS; COUPLED FRACTURE MODE; PLATE BUTT WELDS; SEMIELLIPTIC CRACKS; ELEMENT-ANALYSIS; JOINTS; THICKNESS; PRESSURE; STRENGTH;
D O I
10.1016/j.ijfatigue.2018.06.030
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, fatigue assessment of cracked pipes with weld misalignment is carried out by using fracture mechanics approach. Two types of weld misalignment, viz., centreline offset weld misalignment with equal thickness but unequal diameters, and centreline offset weld misalignment with unequal thickness but aligned inside surface, are considered. A finite element (FE) mesh generator for cracked plain pipes is developed first, and then it is used for the misaligned pipes by incorporating a coordinate transformation method. A small-scale experimental test on the stress concentration curve along the longitudinal direction of misaligned pipes is conducted to ascertain the accuracy of the transformation method. Then, extensive FE analyses are performed to determine the stress intensity magnification factor (M-k) at the crack deepest point and the crack ends of a surface crack in misaligned pipes. A new set of M-k equations for the misaligned pipes are built up using multiple regression analysis, and statistical analyses are carried out to validate the goodness of fit of these equations. The proposed equations can be employed in the fatigue strength calculation and fatigue life prediction based on the fatigue assessment procedure provided by BS 7910:2013.
引用
收藏
页码:192 / 209
页数:18
相关论文
共 50 条
  • [1] Stress intensity factors for circumferential cracked pipes
    Fushun Shiyou Xueyuan Xuebao, 2 (25-29):
  • [2] ON ESTIMATES OF STRESS INTENSITY FACTORS FOR CRACKED BEAMS AND PIPES
    GAO, HJ
    HERRMANN, G
    ENGINEERING FRACTURE MECHANICS, 1992, 41 (05) : 695 - 706
  • [3] Study on stress intensity factors for circumferential cracked elliptical pipes under tension
    Wang, W.
    Cai, Y. M.
    Xie, Y. J.
    MATERIALS AND MANUFACTURING, PTS 1 AND 2, 2011, 299-300 : 912 - +
  • [4] Critical stress intensity factors for cracked hollow pipes under transient thermal loads
    Jayadevan, KR
    JOURNAL OF THERMAL STRESSES, 2002, 25 (10) : 951 - 968
  • [5] Evaluation of stress intensity factors due to welding residual stresses for circumferential cracked pipes
    Oh, Chang-Young
    Kim, Yun-Jae
    Oh, Young-Jin
    Kim, Jong-Sung
    Song, Tae-Kwang
    Kim, Yong-Beum
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2013, 105 : 36 - 48
  • [6] ESTIMATION OF STRESS INTENSITY FACTORS DUE TO WELDING RESIDUAL STRESSES FOR CIRCUMFERENTIALLY CRACKED PIPES
    Oh, Chang-Young
    Kim, Ji-Soo
    Kim, Yun-Jae
    Oh, Young-Jin
    Lee, Kyoungsoo
    Lee, Sung-Ho
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, PVP 2012, VOL 6, PTS A AND B, 2012, : 63 - 72
  • [7] Stress Intensity Factors for Fatigue Cracks at the Toe of a Transverse Weld.
    Skorupa, Malgorzata
    Archiwum Budowy Maszyn, 1984, 31 (3-4): : 247 - 266
  • [8] STRESS INTENSITY FACTORS FOR CRACKED WEDGES
    STONE, SF
    WESTMANN, RA
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1981, 17 (03) : 345 - 358
  • [9] STRESS INTENSITY FACTORS FOR COMPLEX-CRACKED PIPES BASED ON ELASTIC FINITE ELEMENT ANALYSES
    Jeong, Jae-Uk
    Choi, Jae-Boong
    Huh, Nam-Su
    Kim, Yun-Jae
    ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2015, VOL 6A, 2015,
  • [10] STRESS INTENSITY FACTORS FOR A CRACKED STIFFENED SHEET WITH CRACKED STIFFENERS
    NISHIMURA, T
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1991, 113 (01): : 119 - 124