Fatigue properties of Ti-6Al-4V alloy friction stir welding joint obtained under rapid cooling condition

被引:15
|
作者
Ma, Zhongwei [1 ]
Wang, Yue [1 ,2 ]
Ji, Shude [1 ]
Xiong, Lidong [3 ]
机构
[1] Shenyang Aerosp Univ, Sch Aerosp Engn, Shenyang 110136, Liaoning, Peoples R China
[2] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
[3] Nanchang Inst Sci & Technol, Nanchang 330108, Jiangxi, Peoples R China
关键词
Ti-6Al-4V titanium alloy; Friction stir welding; Fatigue properties; Contamination; MECHANICAL-PROPERTIES; CYCLE FATIGUE; TENSILE PROPERTIES; TEXTURE EVOLUTION; ALUMINUM-ALLOY; MICROSTRUCTURE; PERFORMANCE; PARAMETERS; BEHAVIOR;
D O I
10.1016/j.jmapro.2018.10.006
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Friction stir welding joints of Ti-6Al-4V titanium alloy were obtained under air and rapid cooling conditions. After post welding heat treatment, the low-cycle fatigue properties of the joints were manly investigated. The results show that the application of liquid nitrogen on the joint top surface decreases the peak welding temperature and the temperature gradient along the joint thickness, which results in a finer and more homogeneous microstructure. Consequently, the improved tensile properties and microhardness are obtained. Fatigue tests show that the joints obtained under rapid cooling condition possess an increased fatigue life. The W-Re alloy contaminations resulting from the tool wear play a significant role in the joint fatigue performance. The fatigue specimens fracture in the SZ due to the existence of contaminations and these contaminations with different sizes have different influences on the fatigue crack initiation and propagation.
引用
收藏
页码:238 / 247
页数:10
相关论文
共 50 条
  • [1] Fatigue Properties of Ti-6Al-4V Titanium Alloy Friction Stir Welding Joint
    Liu, Zhenlei
    Wang, Yue
    Ji, Shude
    Yan, Dejun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (08) : 4308 - 4316
  • [2] Fatigue Properties of Ti-6Al-4V Titanium Alloy Friction Stir Welding Joint
    Zhenlei Liu
    Yue Wang
    Shude Ji
    Dejun Yan
    Journal of Materials Engineering and Performance, 2018, 27 : 4308 - 4316
  • [3] Effects of intense cooling on microstructure and properties of friction-stir-welded Ti-6Al-4V alloy
    Liu, Zhenlei
    Wang, Yue
    Ji, Shude
    Li, Zhengwei
    MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (02) : 209 - 219
  • [4] Friction-stir welding and processing of Ti-6Al-4V titanium alloy: A review
    Mironov, S.
    Sato, Y. S.
    Kokawa, H.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (01) : 58 - 72
  • [5] Structure and Properties of a Permanent Joint of Ti-6Al-4V Titanium Alloy Formed by Friction Stir Welding
    Chumaevskii, A., V
    Amirov, A., I
    Moskvichev, E. N.
    Ivanov, A. N.
    Kolubaev, E. A.
    RUSSIAN PHYSICS JOURNAL, 2022, 65 (05) : 765 - 770
  • [6] Friction stir welding of Ti-6Al-4V alloy: Friction tool, microstructure, and mechanical properties
    Li, Junping
    Shen, Yifu
    Hou, Wentao
    Qi, Yiming
    JOURNAL OF MANUFACTURING PROCESSES, 2020, 58 : 344 - 354
  • [7] Friction stir welding of additively manufactured Ti-6Al-4V: Microstructure and mechanical properties
    Singh, Amit Kumar
    Kumar, Bhoopendra
    Jha, Kaushal
    Astarita, Antonello
    Squillace, Antonino
    Franchitti, Stefania
    Arora, Amit
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2020, 277
  • [8] Structure and Properties of a Permanent Joint of Ti-6Al-4V Titanium Alloy Formed by Friction Stir Welding
    A. V. Chumaevskii
    A. I. Amirov
    E. N. Moskvichev
    A. N. Ivanov
    E. A. Kolubaev
    Russian Physics Journal, 2022, 65 : 765 - 770
  • [9] Effect of initial microstructure on Ti-6Al-4V joint by friction stir welding
    Yoon, Sungook
    Ueji, Rintaro
    Fujii, Hidetoshi
    MATERIALS & DESIGN, 2015, 88 : 1269 - 1276
  • [10] Eliminating the tearing defect in Ti-6Al-4V alloy joint by back heating assisted friction stir welding
    Ji, Shude
    Li, Zhengwei
    Zhang, Liguo
    Wang, Yue
    MATERIALS LETTERS, 2017, 188 : 21 - 24