摘要
The effect of superficial CeO2 coating on the oxidation behavior of Ti-6Al-4V has been studied under isothermal and cyclic heating conditions in the temperature range of 923-1223 K in dry air. During the early periods of exposure, the oxide scale grows obeying near linear followed by near parabolic kinetics and consists of alternate layers of alpha-Al2O3 and TiO2. The mass gain of the uncoated alloys is found to be two times higher than that of the coated one in the temperature range of 923-1123 K up to 36 h of exposure. The scale composition on the bare or coated alloy is found to depend both on the temperature and on the time of exposure. During cyclic exposure, the scale suffers spallation for both the bare and the coated alloy, which has been attributed to insufficient plasticity of the scale. (C) 2012 Elsevier B. V. All rights reserved.
引用
收藏
页码:106 / 111
页数:6
相关论文
共 50 条
  • [31] INFLUENCE OF SUPERFICIAL COATING OF CEO2 ON THE OXIDATION BEHAVIOR OF AISI-304 STAINLESS-STEEL
    MITRA, SK
    ROY, SK
    BOSE, SK
    OXIDATION OF METALS, 1993, 39 (3-4): : 221 - 229
  • [32] The formation of hydride and its influence on Ti-6Al-4V alloy fracture behavior
    Zhang, Hongbo
    Leygraf, Christofer
    Wen, Lei
    Huang, Feifei
    Chang, Hai
    Jin, Ying
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2023, 48 (92) : 36169 - 36184
  • [33] An organic silicone composite coating for protection of Ti-6Al-4V alloy: Oxidation behavior at 600 C in dry air
    Lu, Yiliang
    Xin, Li
    Li, Xiaonan
    Zhao, Qingqing
    Zhang, Kai
    Du, Yao
    Chen, Zheng
    Wang, Cheng
    Zhu, Shenglong
    Wang, Fuhui
    CORROSION SCIENCE, 2023, 211
  • [34] High-temperature corrosion of Ti and Ti-6Al-4V alloy
    Du, HL
    Datta, PK
    Lewis, DB
    BurnellGray, JS
    OXIDATION OF METALS, 1996, 45 (5-6): : 507 - 527
  • [35] INFLUENCE OF CEO2 ADDITION AND SCANNING SPEED ON MICROSTRUCTURE AND TRIBOLOGICAL BEHAVIOR OF LASER-CLAD Ti-Co REINFORCED COATINGS ON Ti-6Al-4V ALLOY
    Adesina, O. S.
    Farotade, G. A.
    Popoola, A. P., I
    Oloruntoba, D. T.
    SURFACE REVIEW AND LETTERS, 2020, 27 (04)
  • [36] The Effect of Widmanstatten and Equiaxed Microstructures of Ti-6Al-4V on the Oxidation Rate and Creep Behavior
    Sugahara, T.
    Reis, D. A. P.
    Moura Neto, C.
    Barboza, M. J. R.
    Perez, E. A. C.
    Piorino Neto, F.
    Hirschmann, A. C. O.
    ADVANCED MATERIALS FORUM V, PT 1 AND 2, 2010, 636-637 : 657 - +
  • [37] Comparison of molybdenizing and NiCrAlY coating on Ti and Ti-6Al-4V
    Peng Xiaomin
    Xia Changqing
    Liu Yingying
    Zhang Zhigao
    RARE METALS, 2009, 28 (01) : 49 - 56
  • [38] Study of high temperature mechanical behavior of the thermally oxidized Ti-6Al-4V alloy
    Severino, B. P.
    Couto, A. A.
    Reis, D. A. P.
    Aguiar, C. L.
    Castagnet, M.
    Moura Neto, C.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2014, 45 (04) : 269 - 280
  • [39] Gas nitriding and subsequent oxidation of Ti-6Al-4V alloys
    Lee, Dong Bok
    Pohrelyuk, Iryna
    Yaskiv, Oleh
    Lee, Jae Chun
    NANOSCALE RESEARCH LETTERS, 2012, 7 : 1 - 5
  • [40] The effect of oxidation on the subsurface microstructure of a Ti-6Al-4V alloy
    Bagot, P. A. J.
    Radecka, A.
    Magyar, A. P.
    Gong, Y.
    Bell, D. C.
    Smith, G. D. W.
    Moody, M. P.
    Dye, D.
    Rugg, D.
    SCRIPTA MATERIALIA, 2018, 148 : 24 - 28