Wear Resistance of Aluminum Matrix Composites' Coatings Added on AA6082 Aluminum Alloy by Laser Cladding

被引:9
|
作者
Riquelme, Ainhoa [1 ]
Rodrigo, Pilar [1 ]
Escalera-Rodriguez, Maria Dolores [1 ]
Rams, Joaquin [1 ]
机构
[1] Univ Rey Juan Carlos, Escuela Super Ciencias Expt & Tecnol, Ciencia & Ingn Mat, Madrid 28933, Spain
关键词
laser cladding; coatings; AA6082; wear; CORROSION BEHAVIOR; MICROSTRUCTURE;
D O I
10.3390/coatings12010041
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ceramic-reinforced metal matrix composites are known for their high wear resistance. A coating based on these materials would be helpful to improve the wear behavior of aluminum alloys. Laser cladding has been used to deposit a coating consisting of an aluminum alloy reinforced with SiC particles on an AA6082 aluminum alloy. Laser cladding is a very energetic technique that causes the SiC particles to react with the molten aluminum to form Al4C3, which degrades the particles and reduces the properties of the coating. The formation of this detrimental compound was successfully achieved with the addition of Silicon and Titanium to the composite matrix. The microstructures of the newly developed material were characterized and the wear behavior was studied under dry sliding conditions on a pin-on-disc tribometer. The relationship between the microstructure and wear behavior was identified. The absence of Al4C3 in the Al40Si/SiC and Al12Si20Ti/SiC coatings' microstructures resulted in an abrasion mechanism instead of a delamination mechanism. The wear behavior changed along the sliding distances. During the first 200 m of sliding distances, the wear rate of all coatings was lower than the uncoated one due to their higher microhardness. For longer sliding distances, the wear resistance of the uncoated AA6082 was higher than the coated ones due to the formation of a lubricant oxide layer on the AA6082 worn surface. For 1000 m of wear distances, the wear behavior was different for each coating. The wear rate of the Al12Si/SiC coating continued growing due to the delamination mechanism and the presence of Al4C3 that acted as starting crack points. The wear rate of the Al40Si/SiC coating decreased due to the formation of a thin, superficial oxide layer. The wear rate of the Al12SiTi/SiC progressively decreased along the sliding distance to below the substrate wear rate.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Corrosion Resistance of Al/SiC Laser Cladding Coatings on AA6082
    Riquelme, Ainhoa
    Rodrigo, Pilar
    Dolores Escalera-Rodriguez, Maria
    Rams, Joaquin
    COATINGS, 2020, 10 (07)
  • [2] Dry Sliding Tribological Properties of a Hard Anodized AA6082 Aluminum Alloy
    Santecchia, Eleonora
    Cabibbo, Marcello
    Hamouda, Abdel Magid Salem
    Musharavati, Farayi
    Popelka, Anton
    Spigarelli, Stefano
    METALS, 2020, 10 (02)
  • [3] Development of empirical relationships for prediction of mechanical and wear properties of AA6082 aluminum matrix composites produced using friction stir processing
    Dinaharan, I.
    Murugan, N.
    Thangarasu, A.
    ENGINEERING SCIENCE AND TECHNOLOGY-AN INTERNATIONAL JOURNAL-JESTECH, 2016, 19 (03): : 1132 - 1144
  • [4] Microhardness, wear resistance, and corrosion resistance of AlxCrFeCoNiCu high-entropy alloy coatings on aluminum by laser cladding
    Li, Yanzhou
    Shi, Yan
    OPTICS AND LASER TECHNOLOGY, 2021, 134 (134):
  • [5] Optimal conditions for the deposition of novel anticorrosive coatings by RF magnetron sputtering for aluminum alloy AA6082
    Brachetti-Sibaja, S. B.
    Dominguez-Crespo, M. A.
    Rodil, S. E.
    Torres-Huerta, A. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 : S437 - S443
  • [6] Effect of different grain sizes and textures on the corrosion behaviour of aluminum alloy AA6082
    Haendel, M.
    Nickel, D.
    Lampke, T.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2011, 42 (07) : 606 - 611
  • [7] Effect of laser cladding Al3Ti-based coatings on the wear and corrosion resistances of AA6063 aluminum alloy
    He, Huan
    Guo, Weihua
    Xiao, Min
    Pang, Xingzhi
    Shen, Xiaoming
    Fu, Yuechun
    Zeng, Jianmin
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING, PTS 1-3, 2013, 652-654 : 1897 - 1903
  • [8] Corrosion and wear of 6082 aluminum alloy
    Panagopoulos, C. N.
    Georgiou, E. P.
    Gavras, A. G.
    TRIBOLOGY INTERNATIONAL, 2009, 42 (06) : 886 - 889
  • [9] Predicting the wear rate of AA6082 aluminum surface composites produced by friction stir processing via artificial neural network
    Dinaharan, Isaac
    Palanivel, Ramaswamy
    Murugan, Natarajan
    Laubscher, Rudolf Frans
    MULTIDISCIPLINE MODELING IN MATERIALS AND STRUCTURES, 2020, 16 (02) : 409 - 423
  • [10] Microstructure and wear properties of laser cladding Ti-Al-Fe-B coatings on AA2024 aluminum alloy
    Xu, J
    Liu, WJ
    Kan, YD
    Zhong, ML
    MATERIALS & DESIGN, 2006, 27 (05) : 405 - 410