摘要
The object of this paper is to propose a novel method to evaluate the maximum inclusion size in medium strength steel by ultrasonic fatigue testing. The inclusion sizes in the medium strength steel were evaluated by ultrasonic fatigue testing using the fatigue specimen with a large risk volume under water-cooling condition. To ensure fatigue specimens of medium strength steel fracture from the internal inclusion, heat treatment and oxynitrocarburization were conducted to increase the strength of the specimen and to protect the specimen from surface corrosion induced by cooling water. The results show that evaluation of the inclusion size by the proposed method is more accurate than traditional approaches, which are based on inclusion size characterization from arbitrary two dimensional cross sections. Additionally, as the method is based on fatigue testing in the ultrasonic frequency regime, it can be conducted in a reasonable amount of time.
引用
收藏
页码:2817 / 2824
页数:8
相关论文
共 50 条
  • [41] Evaluation of maximum non-metallic inclusion sizes in steel by statistics of extreme values method based on Micro-CT imaging
    Tian, Linan
    Liu, Long
    Ma, Bo
    Zaïri, Fahmi
    Ding, Ning
    Guo, Weimin
    Xu, Na
    Xu, Huixia
    Zhang, Ming
    Metallurgical Research and Technology, 2022, 119 (02):
  • [42] Evaluation of maximum non-metallic inclusion sizes in steel by statistics of extreme values method based on Micro-CT imaging
    Tian, Linan
    Liu, Long
    Ma, Bo
    Zairi, Fahmi
    Ding, Ning
    Guo, Weimin
    Xu, Na
    Xu, Huixia
    Zhang, Ming
    METALLURGICAL RESEARCH & TECHNOLOGY, 2022, 119 (02)
  • [43] Estimation of torsional fatigue strength of medium carbon steel bars with a circumferential crack by the cyclic resistance-curve method
    Yu, HC
    Tanaka, K
    Akiniwa, Y
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1998, 21 (09) : 1067 - 1076
  • [44] Estimation of torsional fatigue strength of medium carbon steel bars with a circumferential crack by the cyclic resistance-curve method
    Yu, H.C.
    Tanaka, K.
    Akiniwa, Y.
    Fatigue and Fracture of Engineering Materials and Structures, 1998, 21 (09): : 1067 - 1076
  • [45] A novel method to define the effective average grain size of the materials with lath-typed microstructure: An example of medium manganese steel
    Zhang, Yu
    Ding, Hua
    Zhu, Haokun
    Zhang, Yutong
    VACUUM, 2021, 191
  • [46] Retained austenite grain size as a strength-plasticity relationship indicator in Al-alloyed medium-Mn steel processed by intercritical annealing
    Skowronek, Adam
    Grajcar, Adam
    Sozanska-Jedrasik, Liwia
    Radwanski, Krzysztof
    Matus, Krzysztof
    Opara, Jaroslaw
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 3201 - 3213
  • [47] Influence of content and maximum size of light expanded clay aggregate on the fresh, strength, and durability properties of self-compacting lightweight concrete reinforced with micro steel fibers
    Nahhab, Ali H.
    Ketab, Ali K.
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 233
  • [48] Coronal multiplanar reconstruction view from isotropic voxel data sets by multidetector-row CT: Can this method correctly detect enlarged mediastinal and hilar lymph nodes and accurately evaluate their size?
    Kozuka, T
    Tomiyama, N
    Johkoh, T
    Honda, O
    Koyama, M
    Nakamura, H
    RADIOLOGY, 2001, 221 : 536 - 536
  • [49] RISING LOAD TEST METHOD TO EVALUATE HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF CR-MO STEEL .2. EFFECT OF TENSILE-STRENGTH ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY
    NOMURA, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1984, 70 (13): : 1486 - 1486
  • [50] On a New Two-Step Air Cooling Method Following Thermomechanically Controlled Rolling: Microstructural Evolution and Mechanical Properties of a High-Strength Multiphase Medium Carbon Microalloyed Steel
    Magham, Hari Srinivasa Rao
    Maheswari, Nandakumar
    Dinesh, Kumar
    Vijayaraghavan, Lakshmanan
    Sankaran, Shanmugam
    Padmanabhan, Kuppuswamy Anantha
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (05)