Structural, microstructure and electrical properties of La2O3-doped Bi0.5(Na0.68K0.22Li0.01)0.5TiO3 lead-free piezoelectric ceramics synthesized by the combustion technique

被引:27
|
作者
Bhupaijit, Pamornnarumol [1 ]
Kornphom, Chittakorn [1 ,2 ]
Vittayakorn, Naratip [3 ]
Bongkarn, Theerachai [1 ,2 ,4 ]
机构
[1] Naresuan Univ, Fac Sci, Dept Phys, Phitsanulok 65000, Thailand
[2] Naresuan Univ, Fac Sci, Res Ctr Acad Excellence Appl Phys, Phitsanulok 65000, Thailand
[3] King Mongkuts Inst Technol Ladkrabang, Fac Sci, Dept Chem, Bangkok 10520, Thailand
[4] Naresuan Univ, Res Ctr Acad Excellence Petr Petrochem & Adv Mat, Phitsanulok 65000, Thailand
关键词
Combustion technique; Perovskite structure; Dielectric; Piezoelectric; Ferroelectric; FERROELECTRIC PROPERTIES;
D O I
10.1016/j.ceramint.2015.03.226
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of firing temperatures on phase formation, microstructure and physical properties of [Bi-0.5(Na0.68K0.22Li0.1)(0.5)TiO3] doped with La2O3 at 0.1 wt% (BNKLLT) ceramics prepared by the combustion method was studied. Glycine was used as fuel and the ratio of raw material (corresponding oxidant metal nitrate) with fuel was about 1:0.56. The samples were calcined at 600-900 degrees C for 2 h and sintered at 1075-1150 degrees C for 2 h. The single rhombohedral peroveskite phase of BNKLLT powders was observed from the sample calcined at 750 degrees C for 2 h. The BNKLLT ceramics exhibited a pure peroveskite phase in all samples. The microstructures of the BNKLLT powders exhibited an agglomerated form while the grain ceramics exhibited a square shape. The average particle size and average grain size increased with increasing firing temperatures. The density, dielectric constant (epsilon(r) and epsilon(m)), P-r and d(33) tended to increase with increasing sintering temperatures up to 1100 degrees C and then decreased. The maximum density (5.73 g/cm(2)), maximum dielectric constant (epsilon(r)similar to 2572 and epsilon(m)similar to 5536), good ferroelectic properties (P-r similar to 35.78 mu C/cm(2) and E-c similar to 22.42 kV/cm) and highest d(33) (210 pC/N) were obtained by the sample sintered at 1100 degrees C for 2 h. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:S81 / S86
页数:6
相关论文
共 50 条
  • [41] The Research on the Piezoelectric and Dielectric Properties of Bi0.5(Nak)0.5-BaTiO3 Lead-free Ceramics
    Guo, Jian-yong
    Zhou, Tao-sheng
    Liao, Ji-hong
    PROCEEDINGS OF 2014 INTERNATIONAL CONFERENCE ON MATERIAL SCIENCE AND ENGINEERING, 2014, 1035 : 422 - +
  • [42] Influence of lead titanate additive on the structural and electrical properties of Na0.5Bi0.5TiO3-SrTiO3 piezoelectric ceramics
    Perumal, Rajesh Narayana
    Athikesavan, Venkatraj
    Nair, Prita
    CERAMICS INTERNATIONAL, 2018, 44 (11) : 13259 - 13266
  • [43] Optimum Sintering Temperature for Fabrication of 0.8Bi0.5Na0.5TiO3-0.2Bi0.5K0.5TiO3 Lead-Free Ceramics by Combustion Technique
    Thongtha, Atthakorn
    Bongkarn, Theerachai
    ADVANCED MATERIALS AND COMPUTER SCIENCE, PTS 1-3, 2011, 474-476 : 1754 - 1759
  • [44] Lead-free Bi0.5(Na1-xKx)0.5TiO3 relaxor ferroelectric ceramics for a wearable energy harvester
    Cho, Sam Yeon
    Kim, Eun-Young
    Kim, Hyunseung
    Jeong, Chang Kyu
    Bu, Sang Don
    CERAMICS INTERNATIONAL, 2022, 48 (05) : 6917 - 6922
  • [45] Structure, ferroelectric properties, and electric field-induced large strain in lead-free Bi0.5(Na,K)0.5TiO3-(Bi0.5La0.5)AlO3 piezoelectric ceramics
    Ullah, Aman
    Ahn, Chang Won
    Lee, Sun Young
    Kim, Jin Soo
    Kim, Ill Won
    CERAMICS INTERNATIONAL, 2012, 38 : S363 - S368
  • [46] Bipolar and unipolar fatigue property in Bi0.5Na0.5TiO3-Bi0.5K0.5TiO3-SrTiO3 lead-free piezoelectric ceramics
    Zhu, Yinyin
    Zhou, Helezi
    Sun, Dazhi
    PHYSICA B-CONDENSED MATTER, 2019, 575
  • [47] Effect of Li2O addition on the phase formation, microstructure and electrical properties of 0.79Bi0.5Na0.5TiO3-0.18Bi0.5K0.5TiO3-0.03BiFeO3 ceramics
    Chootin, Suphornphun
    Bhupaijit, Pamornnarumol
    Bongkarn, Theerachai
    FERROELECTRICS, 2022, 601 (01) : 49 - 58
  • [48] Effect of La2O3-Enriched Bi0.5(Na0.68K0.22Li0.1)0.5TiO3 on Properties of (K0.44Na0.52Li0.04)(Nb0.84Ta0.10Sb0.06)O3 Ceramics Prepared by Solid State Combustion
    Chittakorn Kornphom
    Jaru Jutimoosik
    Theerachai Bongkarn
    Journal of Electronic Materials, 2019, 48 : 3919 - 3930
  • [49] Structural and electromechanical properties of lead-free Na0.5Bi0.5TiO3-BaZrO3 ceramics
    Hussain, Ali
    Rahman, Jamil Ur
    Maqbool, Adnan
    Kim, Min Su
    Song, Tae Kwon
    Kim, Won Jeong
    Kim, Myong Ho
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2014, 211 (08): : 1704 - 1708
  • [50] Relaxor behavior and ferroelectric properties of Na0.5Bi0.5TiO3-K0.5Bi0.5TiO3-KNbO3 lead-free ceramics
    Yueming Li
    Wen Chen
    Qing Xu
    Jing Zhou
    Journal of Materials Science, 2005, 40 : 3625 - 3628